Thanks: 0
Needs Pictures: 0
Results 1 to 3 of 3
Thread: Single pointing long threads
-
26th Sep 2024, 09:17 AM #1Most Valued Member
- Join Date
- Sep 2011
- Location
- Ballarat
- Age
- 66
- Posts
- 3,172
Single pointing long threads
Hi all,
I got asked if I could thread a whole heap of 12 mm bars (and I mean a heap of them) for some long 'J' bolts he needed. Each one needed 350mm of M12 x 1.75 thread. I had previously made a tailstock die holder so decided to use that. Dies just aren't what they used to be and the finish on the threads was atrocious. Single pointing is the only choice I had left. This required the use of the travelling steady. What worried me is that when I cut the square thread for the Douglas shaper I found the threads would cut in to the supports of the steady and I was constantly adjusting the arms.
I made up a different type of travelling steady and it worked a treat.
Phil
https://youtube.com/shorts/aR0Goh7802o
-
26th Sep 2024, 11:00 AM #2Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 72
- Posts
- 6,290
Fantastic thinking outside the square.
I was thinking it would be a travelling steady with a bearing on the end of the support.
KrynTo grow old is mandatory, growing up is optional.
-
26th Sep 2024, 11:39 PM #3Most Valued Member
- Join Date
- Sep 2011
- Location
- Ballarat
- Age
- 66
- Posts
- 3,172
Thanks Kryn. I had thought of that but for some reason I have very little travel in the support arms of the supplied travelling steady. It may have been a design flaw.
The guides for the one I made are removable so I can make new blocks, mount them and drill and ream in position if I need to do quantities of a different size.
They are case hardened as well which adds to the longevity.
Phil
Similar Threads
-
Single pointing 40 TPI in aluminium
By bob ward in forum METALWORK GENERALReplies: 3Last Post: 12th Oct 2015, 03:08 PM -
Thread wobble - single point cutitng of small diameter threads
By variant22 in forum METALWORK GENERALReplies: 9Last Post: 18th Jun 2014, 02:23 PM -
reconditioning a windmill (long long story here)
By .RC. in forum METALWORK GENERALReplies: 35Last Post: 29th Sep 2012, 07:14 PM -
Looking for long threads
By Big Shed in forum METALWORK GENERALReplies: 11Last Post: 17th Jan 2011, 03:56 PM -
Why do some people persist in putting up new threads with enormously long headings ?
By Gumby in forum FORUMS INFO, HELP, DISCUSSION & FEEDBACKReplies: 15Last Post: 20th Apr 2006, 12:38 AM