    Hi all,
    I got asked if I could thread a whole heap of 12 mm bars (and I mean a heap of them) for some long 'J' bolts he needed. Each one needed 350mm of M12 x 1.75 thread. I had previously made a tailstock die holder so decided to use that. Dies just aren't what they used to be and the finish on the threads was atrocious. Single pointing is the only choice I had left. This required the use of the travelling steady. What worried me is that when I cut the square thread for the Douglas shaper I found the threads would cut in to the supports of the steady and I was constantly adjusting the arms.
    I made up a different type of travelling steady and it worked a treat.

    Phil
    https://youtube.com/shorts/aR0Goh7802o
    Attached Images Attached Images

  2. #2
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    72
    Posts
    6,294

    Default

    Fantastic thinking outside the square.
    I was thinking it would be a travelling steady with a bearing on the end of the support.
    Kryn
    To grow old is mandatory, growing up is optional.

  3. #3
    Join Date
    Sep 2011
    Location
    Ballarat
    Age
    66
    Posts
    3,172

    Default

    Quote Originally Posted by KBs PensNmore View Post
    Fantastic thinking outside the square.
    I was thinking it would be a travelling steady with a bearing on the end of the support.
    Kryn
    Thanks Kryn. I had thought of that but for some reason I have very little travel in the support arms of the supplied travelling steady. It may have been a design flaw.
    The guides for the one I made are removable so I can make new blocks, mount them and drill and ream in position if I need to do quantities of a different size.
    They are case hardened as well which adds to the longevity.

    Phil

Similar Threads

  1. Single pointing 40 TPI in aluminium
    By bob ward in forum METALWORK GENERAL
    Replies: 3
    Last Post: 12th Oct 2015, 03:08 PM
  2. Thread wobble - single point cutitng of small diameter threads
    By variant22 in forum METALWORK GENERAL
    Replies: 9
    Last Post: 18th Jun 2014, 02:23 PM
  3. reconditioning a windmill (long long story here)
    By .RC. in forum METALWORK GENERAL
    Replies: 35
    Last Post: 29th Sep 2012, 07:14 PM
  4. Looking for long threads
    By Big Shed in forum METALWORK GENERAL
    Replies: 11
    Last Post: 17th Jan 2011, 03:56 PM
  5. Why do some people persist in putting up new threads with enormously long headings ?
    By Gumby in forum FORUMS INFO, HELP, DISCUSSION & FEEDBACK
    Replies: 15
    Last Post: 20th Apr 2006, 12:38 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •