    Default Enlarging a plain wedding ring

    So, I had to get an x-ray of my hand, and had to remove my wedding ring. Took a few minutes of pulling over my swollen knuckle, turning, pushing the skin under the flat inside surface, et c.
    IMG_3665.jpg

    All you guys – safety conscious metalworkers – probably take it off every day???,
    but I don't, and over the years the calluss has gotten thicker, the fingers have gotten thicker, and removal just got too hard, so I leave it on there.

    Need to resize this thing.


    Jeweller? No way. It is just metal. I can work metal, right???


    Plumbing pipe expander is a little too big:
    IMG_3666.jpg




    but my finger/ring is about the size of an MT2 taper:
    IMG_3667.jpg


    I don't want to scratch too much GOld off, so I use the newest/cleanest taper I have.
    Tap the ring down to the big end with that steel spacer, and we should be happy?
    IMG_3668.jpg


    It wasn't big enough on my finger. So, I try to gently peen the ring all the way around, hoping it will get a little bigger with each tap:
    IMG_3669.jpg
    (photo just for graphical communication - I actually tapped on a block of timber)


    Sadly, they didn't make much difference - ring still too tight - so I found a longer taper and forced the ring further along:
    IMG_3670.jpg


    That did the trick. Ring clears the knuckle now!

  2. #2
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,947

    Default

    Hi Nigel, That is exactly how a jeweller would have done it.
    Best Regards:
    Baron J.

  3. #3
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,693

    Default

    Jeweller would have done very similar depending on how much larger it needed to be, and of course have ring stretchers to do the job, you need to be careful as you can break the ring especially if it has been soldered.
    good to see it all worked out.

  4. #4
    Join Date
    Feb 2024
    Location
    France
    Age
    31
    Posts
    1

    Default

    Hi
    Wowww! I didn't know this kind of process was possible! Thanks for sharing!

  5. #5
    Join Date
    Aug 2019
    Location
    Revesby - Sydney Australia
    Age
    57
    Posts
    1,285

    Default

    I didn't know this kind of process was possible!
    We can do many things with a hammer.


    Real jewellers might even join (weld) a new link of metal in if the size difference was large.



    Welcome to the forum, Roxi !
    Nigel, from a cave FULL of unfinished projects and lost tools.

  6. #6
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,947

    Default

    Hi Nigel,

    https://www.youtube.com/watch?v=g72LxZVu_eg

    I meant to post this at the time but forgot ! Sorry.
    Best Regards:
    Baron J.

Similar Threads

  1. Quality of cheap titanium/tungsten wedding bands?
    By icu222much in forum JEWELLERY
    Replies: 7
    Last Post: 2nd Jan 2020, 10:26 AM
  2. plain bearing material.
    By onanonanon in forum METALWORK GENERAL
    Replies: 34
    Last Post: 27th Jul 2018, 09:00 PM
  3. Just finished my Brother In-law wedding ring
    By Jerms in forum METALWORK GENERAL
    Replies: 6
    Last Post: 3rd Oct 2012, 09:19 AM
  4. Enlarging the axle hole on Fork Leg
    By Sterob in forum METALWORK GENERAL
    Replies: 5
    Last Post: 7th Mar 2011, 05:07 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •