    Not really jewellery but I have a old table lamp that is my fathers. It was made many years ago by soldering a copper pipe for the lamp support onto the back of a silver figurine.
    I want to remove the pipe and try to restore the silver figurine so am wondering how would be the best way. I was thinking of using my weller iron and a solder sucker to remove the majority but Im sure that will leave traces on the silver.


    .20220603_085715.jpg20220603_085637.jpg

  2. #2
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,028

    Default

    I think solder has a greater affinity for raw copper than sliver so maybe try some of that solder wicking copper braid stuff?

  3. #3
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,550

    Default

    Paint around the edge of the solder line with yellow ochre apply fairly heavy or Liquid paper, this will stop the solder flowing further onto the Silver, then as above try solder wick, I do not think this will remove all the solder you will be left with a film that you will need to be removed mechanically. I would use a torch but I have been working with Silver for many years, you may struggle with the weller, if you go with a torch be aware that Silver has low melting point.

  4. #4
    Join Date
    Apr 2018
    Location
    Perth
    Posts
    134

    Default

    Thanks Bob and China,
    Thinking silver should be harder than solder so could I possibly buff away the solder ?

  5. #5
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,550

    Default

    If you go carefully yes.

Similar Threads

  1. SIlver Solder -Suppliers - High silver content
    By steamingbill in forum METALWORK GENERAL
    Replies: 25
    Last Post: 15th Mar 2019, 05:15 PM
  2. WTB ADL Silver solder rod
    By GWH74 in forum WANTED TO BUY
    Replies: 0
    Last Post: 28th Apr 2016, 08:19 AM
  3. 245 Silver solder
    By fxst in forum METALWORK GENERAL
    Replies: 2
    Last Post: 16th Oct 2012, 12:22 AM
  4. source of silver solder other than BOC?
    By desbromilow in forum METALWORK GENERAL
    Replies: 6
    Last Post: 30th Aug 2012, 11:30 AM
  5. Silver Solder Pt 2 How to
    By Grahame Collins in forum METALWORK GENERAL
    Replies: 0
    Last Post: 11th Jan 2007, 10:51 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •