    Default Induction heater/furnace. Are they useless?

    I am not a blacksmith - have only swung a hammer against hot metal a few times


    I have a customer job to create many small steel buttons, rustic door studs. Was planning to bash mild steel rod slugs - 12mm round, about 18mm long - into a die. Some of the buttons need a pattern, so the die will have machined and the slugs will have to be quite hot.

    Probably yellow hot, maybe closer to white?
    Butane or propane won't do it. Maybe MAP or Oxy Acetylene?



    I was thinking about building one of those little induction heating gizmos with the water-cooled coils, that they claim can heat steel to red hot in seconds, can melt small amounts of Gold in a crucible, et c.

    From what I understand of the physics, it is a magnetic effect that causes the heating. Which would stop at red hot (Curie point)?


    Has anyone used one of these with steel?

  2. #2
    Join Date
    Mar 2011
    Location
    Adelaide
    Posts
    876

    Default

    I did a similar job about 3 years ago, just under 200 fake rivets, with patina. I used Oxy Acetylene because thats what I have on hand. One of the single most frustrating paid jobs Ive done, ever. How are you intending to create the patina?

  3. #3
    Join Date
    Aug 2019
    Location
    Revesby - Sydney Australia
    Age
    54
    Posts
    452

    Default

    Patina?

    I was contemplating acid, but have a bucket of cast iron filings ready to soak them in with other reagents.


    Better suggestions?

  4. #4
    Join Date
    Mar 2011
    Location
    Adelaide
    Posts
    876

    Default

    Sorry, I meant make them look old and knocked about physically, not so much stained. Kind of like a golf ball. If its not part of your brief please return to regular programming

  5. #5
    Join Date
    Aug 2019
    Location
    Revesby - Sydney Australia
    Age
    54
    Posts
    452

    Default

    The samples he gave me were actually cast.

    Inside surface typical iron sand casting,
    but outside surface was mostly smooth. Some looked lacquered.


    I did think about reheating the slugs, and hammering them into iron shavings for some texture. It will depend on how efficient I am in making them. If I go the electric induction "furnace" route, that will take extra time to build/setup, but should be faster to heat the slugs and churn them out.

  6. #6
    Join Date
    Nov 2017
    Location
    Geelong, Australia
    Age
    55
    Posts
    1,754

    Default

    Id be looking at something to heat them in quantity, and bribe a suitable helper to grab the next one with tongs and hand it to you for forming.
    Small pot of charcoal and hair drier sort of setup??

    Steve

  7. #7
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    6,412

    Default

    I used an induction furnace at work in the US to melt small amounts (grams) mixture of rock powders and flux in a platinum crucible. It got to about 1500C in very quick time (<minute) and gave off all sorts of RF noise so had to be done inside a Faraday cage. Very spectacular. The resulting "glass bead" was then easily dissolved in strong acids and analysed in a mass spectrometer or a spectrophotometer. Once we tried it outside the Faraday cage and succeeded in damaging a bunch of sensitive electronic instruments in the lab next door which cost a couple of grand to fix

  8. #8
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    6,412

    Default

    Here's one on Banggood
    Claim is 1200C in 5 minutes

    Capacity claims is 3kg gold, or 150 cc - not much really,
    Screen Shot 2021-09-22 at 5.03.02 pm.png

    https://www.banggood.com/MM-TC-3000-...N&rmmds=search

  9. #9
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    2,831

    Default

    Quote Originally Posted by BobL View Post
    Capacity claims is 3kg gold, or 150 cc - not much really,
    $235,800 in fact!
    Chris

  10. #10
    Join Date
    Aug 2019
    Location
    Revesby - Sydney Australia
    Age
    54
    Posts
    452

    Default

    Bob, thanks for that link, 5000W is a decent amount of power/heat,
    though at nearly $2000US is out of my price range for one small job



    1200C would certainly be hot enough for soft working of steel,

    but I suspect getting that hot requires the graphite crucible;
    graphite gets super hot, metal sitting on the graphite heats up,
    and a lot of heat radiates out of the top of the crucible.

    (which is why they have a quartz thing to hold the graphite thing)



    Also, 1200C in 5 minutes? Sounds like nicely made up round numbers, doesn't it?

  11. #11
    Join Date
    Aug 2019
    Location
    Revesby - Sydney Australia
    Age
    54
    Posts
    452

    Default Finally found some useful info

    https://spaco.org/Blacksmithing/ZVSI...eaterNotes.htm

    Basically, his conclusion is that they are no good for forging steel.




    Also found some good forums that talk about melting alloys for casting, and annealing bullet casings:

    https://highvoltageforum.net/index.php?topic=530.80

    https://forum.accurateshooter.com/th...3908353/page-2

  12. #12
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,358

    Default

    For many times less than those sort of prices you could build a simple gas forge.

Similar Threads

  1. Nitinol,,,,,,Something interesting but probably useless to most.
    By shedhappens in forum METALWORK GENERAL
    Replies: 6
    Last Post: 22nd Apr 2019, 07:04 PM
  2. factory workshop heater wildcat 410 lp gas heater
    By dodge at4 in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 0
    Last Post: 19th May 2017, 11:38 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •