    Default How to tightly hold a bundle of small steel rods

    Im making another pair of these hand carders for SQMBO.
    These ones are made from 2mm regular steel TIG welding rods
    IMG_4685.jpg

    This time I'm using 3mm TSS rods.
    Cutting 48 equal length rods is pretty monotonous. They don't need to be a specific length but they should all be the same, so I rough cut them on my thin kerf abrasive table saw and was looking for a way to hold a bundle together to hold them all even at one end so's I could sanded the other end all to the same length.
    Tried zip ties - SS was too slippery, Then I tried using a collet in a collect chuck/block.
    Get the all levelled up like this

    colletEnd.JPG

    And grind the other end on a disc sander like this.
    You'll notice one is still short - that's just a spare to help the others sit tight in the collet - its not going to be used in the final pieces.
    groundend.JPG

    Now have to sharpen one end, bend the sharpened tips, and make up some handles.
    Attached Images Attached Images

Similar Threads

  1. Tig brazing rods v's Oxy rods. Any difference?
    By Zumanity in forum WELDING
    Replies: 8
    Last Post: 13th Mar 2020, 09:21 AM
  2. which steel for small jeweller roller?
    By Alex_Campili in forum JEWELLERY
    Replies: 2
    Last Post: 12th Nov 2017, 12:44 AM
  3. GP arc mild steel welding rods for teaching
    By Paul M D in forum WELDING
    Replies: 9
    Last Post: 18th Jun 2016, 12:49 AM
  4. Small steel Engineering job please
    By seriph1 in forum METALWORK GENERAL
    Replies: 19
    Last Post: 25th Feb 2016, 09:47 PM
  5. Question On Welding Rods and RHS Steel
    By mattwolf in forum WELDING
    Replies: 1
    Last Post: 29th Jul 2009, 10:11 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •