    Default dent-removal-brass

    Quote Originally Posted by BaronJ View Post
    Hi Wooly,

    Can you solder a pair of small brass washers to the inside of the lever ?
    Hi Baron. Yes I could solder these washers but why would I? The gap between the lever and the posts was meant to accomodate the spring. Unless I use a spring which mounts somewhere else. Actually I prefer that solution in which case you are right about using washers. Presumably to prevent the key from wobbling? Actually soldering is a bit of a risk because the cap on the end of the lever is soft soldered and I'd have to use a wet cloth to prevent it falling off. But the washers could be done using solder although I'm finding epoxy resin is much easier.
    Looking at the download of my previous post I see the photos of the trombone before and after the dents were removed didn't get sent. I'll try again, Right this is my problem in sending trombone photos. They arrived by e mail and I can't find a way to link them to this post on the forum. They have a reference number img1688.jpg in the e mail section but how do I refer to it in the forum attachments?
    Last edited by woolyhead; 26th Nov 2020 at 01:01 AM. Reason: omission

  2. #32
    Join Date
    Sep 2012
    Location
    North Yorkshire UK
    Posts
    4,195

    Default

    Hi Wooly,

    I don't think that a pair of washers would impact the spring at all, indeed if you didn't want to solder them a dab of super glue would do the same and could be removed if needed with a little heat.

    I've just been looking at the drawing you posted. Is the key solid or folded ? Is the 2 mm you called out a gap or is it a solid piece. Good pictures would make understanding what you can see a lot easier.

    I was looking at a cornet and the spring on the little lever was quite small looking like a pair of chopsticks with a loop of wire at the end. Your drawing seems to show a much more complicated spring, probably to reduce the side twisting of a hairpin spring.

    As far as pictures in an Email simply copy them to the desktop or somewhere you can find them, then go to "Manage Attachments" below the post, click on "Add Files" then click on "Browse" which will open a window on your machine, navigate to the pictures you want to post and click on it. Then click on "Upload", Insert, then "Done".

    HTH.
    Best Regards:
    Baron J.

  3. #33
    Join Date
    Nov 2020
    Location
    Cambridge, uk
    Posts
    16

    Default dent removal in brass

    Quote Originally Posted by BaronJ View Post
    Hi Wooly,

    I don't think that a pair of washers would impact the spring at all, indeed if you didn't want to solder them a dab of super glue would do the same and could be removed if needed with a little heat.

    I've just been looking at the drawing you posted. Is the key solid or folded ? Is the 2 mm you called out a gap or is it a solid piece. Good pictures would make understanding what you can see a lot easier.

    I was looking at a cornet and the spring on the little lever was quite small looking like a pair of chopsticks with a loop of wire at the end. Your drawing seems to show a much more complicated spring, probably to reduce the side twisting of a hairpin spring.

    As far as pictures in an Email simply copy them to the desktop or somewhere you can find them, then go to "Manage Attachments" below the post, click on "Add Files" then click on "Browse" which will open a window on your machine, navigate to the pictures you want to post and click on it. Then click on "Upload", Insert, then "Done".

    HTH.
    Much obliged BaronJ. I'll give it a go soon. Meanwhile the key is solid and the 2mmis also solid. If the washers don't impact on the spring they would have to be smaller in diameter than the coils of the spring. But what would be the purpose of using these washers? With the original maker's springs there was barely enough room to get them in. I'll send the trombone pictures soon. Sorry about the quality of my hand drawn sketches but this object is difficult to draw right. I have moved the photo to documents where it is called scan0008 but I can't seem to pick it up for adding to my forum post. Still working on it.
    Last edited by woolyhead; 27th Nov 2020 at 07:30 AM. Reason: omissions

  4. #34
    Join Date
    Sep 2012
    Location
    North Yorkshire UK
    Posts
    4,195

    Default

    Hi Wooly,

    Thanks for the extra bit of info, I originally got the impression that the key was a folded part, that was why I suggested small washers.

    I look forward to the pictures.
    Best Regards:
    Baron J.

Page 3 of 3 FirstFirst 123

Similar Threads

  1. what rods for thin brass to brass ??
    By Mathuranatha in forum WELDING
    Replies: 7
    Last Post: 23rd Nov 2020, 08:17 PM
  2. What's the best way to dent this back?
    By qwe7410 in forum METALWORK GENERAL
    Replies: 6
    Last Post: 26th Jun 2017, 09:40 PM
  3. VICTORIA Brass Flat Bar Assorted Sizes & 1/4" SWB Threaded Rod & 260 Carbide Brass Sheet
    By thumbsucker in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 7
    Last Post: 18th Mar 2013, 03:36 PM
  4. Key Removal
    By tongleh in forum METALWORK GENERAL
    Replies: 17
    Last Post: 15th Nov 2012, 01:48 PM
  5. Spindle removal
    By Buncha in forum THE HERCUS AREA
    Replies: 6
    Last Post: 14th Jan 2009, 10:33 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •