    Default Aluminium Castings - Flux and melt Gas release alternatives

    Hi guys,
    i was watching myfordboy on youtube casting aluminium.

    i note that he uses salt and washing soda for flux and removing gases from the molten aluminium.

    Has anyone tried this, does it work as successfully as it seems to for myfordboy.

  2. #2
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,112

    Default

    Most casters I know use borax

  3. #3
    Join Date
    Dec 2007
    Location
    Sydney
    Posts
    152

    Default

    Bluey purple coloured tablets, probably borax.
    Ive possibly got the TAFE notes in the stash somewhere.
    H.
    Jimcracks for the rich and/or wealthy. (aka GKB '88)

  4. #4
    Join Date
    Apr 2018
    Location
    Drouin Vic
    Posts
    226

    Default

    I have used them and they seem to work just fine- although I am far from an authority. Lite salt is the stuff to use for flux- it is a blend of sodium chloride and potassium chloride. I wrap about a tablespoon of it in some alfoil, drop it into the pot and stir it in. Sodium carbonate- laundry soda- wrapped the same way and plunged into the bottom of the pot certainly brings a lot of bubbles to the surface. I bought some commercial stuff a few years ago but I have to travel half a day to any foundry supply so use DIY solutions.

Similar Threads

  1. Is lathe bed grinding available in Brisbane? Any alternatives?
    By j3dprints in forum METALWORK GENERAL
    Replies: 11
    Last Post: 12th May 2018, 06:18 PM
  2. Alternatives to stainless acid pickles
    By Michael G in forum WELDING
    Replies: 24
    Last Post: 18th Jun 2017, 10:44 AM
  3. Welding Alternatives.
    By soundman in forum WELDING
    Replies: 0
    Last Post: 8th Oct 2014, 10:35 AM
  4. how can you melt aluminum without a furnace
    By welder in forum THE FOUNDRY
    Replies: 10
    Last Post: 2nd Oct 2012, 07:34 PM
  5. Anodising or alternatives in the shed
    By Michael G in forum METALWORK GENERAL
    Replies: 7
    Last Post: 3rd Jun 2012, 03:13 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •