Whilst not a machining project, I thought I'd show you my recent metalwork project.
Made from flat templates outlined onto sheet metal, cut, scored, bent and welded, and left outside to rust. Many hours of trial and error.
They stand about 300mm high and 450mm long.
Not hard to see my welding leaves a lot to be desired.
-
9th May 2020, 11:48 AM #2
Diamond Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 33
- Posts
- 1,455
They look great, good enough to keep other birds away even.
-
9th May 2020, 12:17 PM #3
Senior Member
- Join Date
- Sep 2019
- Location
- Newcastle, AU
- Posts
- 238
They look great!
-
9th May 2020, 02:58 PM #4
Senior Member
- Join Date
- Feb 2012
- Location
- Tamworth, NSW
- Posts
- 160
Fantastic!
-
9th May 2020, 03:21 PM #5
Hi Vicval01
Definitely something to crow about!
Well done!
What was the process you used to weld them up.? Oxy ,Mig, Tig or Stick?
Grahame
-
9th May 2020, 04:27 PM #6
Member
- Join Date
- Apr 2020
- Location
- Ettalong Beach NSW
- Age
- 60
- Posts
- 72
[QUOTE=Grahame Collins;1967984]
Definitely something to crow about!
Ha, thanks. Using a mig.
-
9th May 2020, 09:23 PM #7
Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 70
- Posts
- 5,129
How long does it take to make one? My partner wants to know are you taking orders, as she loves them, as you've really captured the shaping of it.
KrynTo grow old is mandatory, growing up is optional.
-
9th May 2020, 09:54 PM #8
Member
- Join Date
- Apr 2020
- Location
- Ettalong Beach NSW
- Age
- 60
- Posts
- 72
It's hard to estimate, I didn't keep track of the timing. But the one I cut pieces by hand, and the other two I had laser cut which were about $200 each just for supply and cut. I would think the one I cut would have taken me somewhere around 100 hours all up. I would take orders, but in order for it to be worth my while, your partner might not want to pay what I'd like to get for them.
I am planning to do some other animals in the future, probably focusing on Australian natives. If you're interested, PM me with your phone number and I'll contact you. Thanks for the positive feedback.
-
10th May 2020, 06:24 AM #9
Member
- Join Date
- Apr 2020
- Location
- Ettalong Beach NSW
- Age
- 60
- Posts
- 72
Video links
Here's a couple of quick videos I made of how I made the Ravens.
Part 1. https://youtu.be/mD2hBu25Qe0
Part 2. https://youtu.be/MdcW5aEvGVs
-
10th May 2020, 12:25 PM #10
Golden Member
- Join Date
- Sep 2006
- Location
- Mallacoota,VIC,Australia
- Age
- 51
- Posts
- 956
They look really good, well done.
All The Beststeran50 Stewart
The shortest way to do many things is to do only one thing at once.
-
10th May 2020, 11:52 PM #11
You have done a good job capturing them.
Ravens are such smart birds.
I have some photos of a flock of them on Vancouver Island feeding outside a house in a native village. I would have stayed there all day watching them but my wife was nervous about our surroundings.
Bill Reid has done some amazing sculptures which often include Ravens.
The bronze cast ‘Black Canoe’ is in the Vancouver Airport.
Below is a pic of ‘The Raven Discovering Mankind’.
H.Jimcracks for the rich and/or wealthy. (aka GKB '88)
-
11th May 2020, 12:35 PM #12
Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,763
Those ravens are fantastic. You really have captured their true character extremely well. That's not easy to do!
I wish I had that ability!
Simon
Sent from my SM-G970F using TapatalkGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
11th May 2020, 12:54 PM #13
Member
- Join Date
- Apr 2020
- Location
- Ettalong Beach NSW
- Age
- 60
- Posts
- 72
Thanks Simon, patience is a major contributing factor. And skill is just an action repeated. Just got to start at the beginning.
Similar Threads
-
Looking for a steel rod
By juaniv37 in forum METALWORK GENERALReplies: 3Last Post: 22nd Jul 2019, 06:42 PM -
Loan of a Steel hoop or piece of steel with a hole about 350 mm in diameter
By BobL in forum METALWORK GENERALReplies: 13Last Post: 17th May 2018, 08:04 PM -
mild steel to stainless steel
By cava in forum WELDINGReplies: 8Last Post: 27th Nov 2014, 06:48 AM -
Supplier of high speed steel and tool steel bar and spring steel in melbourne?
By fudo133 in forum METALWORK GENERALReplies: 3Last Post: 25th Jun 2014, 12:44 PM -
best steel
By eskimo in forum METALWORK GENERALReplies: 15Last Post: 7th Jun 2012, 10:33 PM