    Default Restoring a vise and making the stand for it

    I found quality vise from scrapyard.
    Condition wasn't what it could be, so i restored it.


  2. #2
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    5,205

    Default

    G day Tuomas,
    That's an awesome looking vice. The welding on it looked to be steel so can I assume that part was cast steel?

    I am also curious about the bead of material you squeezed under the floor base plate.

    Was it something to help preserve the life of the tile ?

    Thanks for posting

    Grahame

  3. #3
    Join Date
    Apr 2019
    Location
    Finland
    Age
    42
    Posts
    65

    Default

    Quote Originally Posted by Grahame Collins View Post
    G day Tuomas,
    That's an awesome looking vice. The welding on it looked to be steel so can I assume that part was cast steel?

    I am also curious about the bead of material you squeezed under the floor base plate.

    Was it something to help preserve the life of the tile ?

    Thanks for posting

    Grahame
    Yep. Those are cast steel. Also compressed during the cast. Those Ridgid vises are really hard, but still strong ones.


    Weld plates are hardly ever absolutely straight.
    I used silicone between the stand and flooring, that gives better contact between plate and floor.
    Then it doesn't "lean" to any corner and connection is stronger when forces are "shared" equally.

    For concrete floor i would have used mortar or plaster.
    So, it was for straightening surfaces between the bottom plate and floor.

Similar Threads

  1. Is this lathe worth getting / restoring
    By Viperx85 in forum METALWORK GENERAL
    Replies: 33
    Last Post: 22nd Jul 2018, 08:03 PM
  2. Restoring an old mill
    By Alf Scotting in forum METALWORK GENERAL
    Replies: 17
    Last Post: 1st Feb 2017, 12:16 PM
  3. Machine Tool Restoring
    By cba_melbourne in forum METALWORK GENERAL
    Replies: 8
    Last Post: 9th Aug 2014, 01:28 PM
  4. Restoring-ish a Mars Thor
    By Gammaboy in forum METALWORK GENERAL
    Replies: 4
    Last Post: 8th Jan 2014, 01:20 PM
  5. Restoring chrome parts
    By mcchaddy in forum METALWORK GENERAL
    Replies: 2
    Last Post: 30th Jan 2008, 09:03 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •