    Hi,

    I picked up a Buffalo Forge Post Drill the other day.

    I'm wondering if I should leave it as is and use it for a decorative piece for outside or strip it back and paint it up for a decorative piece inside?

    If I strip it back what would be the best way of de-rusting it? Molasses? Or a chemical alternative?

    Ben.
    Buffalo 3.jpgBuffalo 2.jpgBuffalo 1.jpg

  2. #2
    Join Date
    Oct 2015
    Location
    melbourne
    Posts
    294

    Default

    Or, restore and use..... 🙂

    I've had success with molasses, although smelly, and electrolysis. (quicker), and evaporust ($$$).

    If you don't want to use it, then id at least derust and paint to preserve it for the next owner.

    (a wire brush to start would reduce the load on whatever you use to clean up the rest)

  3. #3
    Join Date
    Nov 2017
    Location
    Geelong, Australia
    Age
    53
    Posts
    755

    Default

    Iím a fan of using Penetrol on bits and pieces that I want to protect but not lose the all over old steel look. A quick rub with a hand wire brush to take off any loose stuff then a couple of coats of Penetrol.
    It gives a finish that looks similar to a lightly oiled surface rust, but dries completely and you can paint over it later if you want.



    Itís about $30 at Bunnings for that 950ml tin. Thereís a smaller one, but that size is better value and lasts me a couple of years with no issues of hardening in the tin etc.

    Steve

  4. #4
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,028

    Default

    If you are going to put outside the current trend is to leave as it is

  5. #5
    Join Date
    Aug 2008
    Location
    Tennant Creek, Aust
    Age
    57
    Posts
    449

    Default

    I am a recent convert to citric acid.

    https://metalworkforums.com/f65/t204...trolysis-lathe

    I would clean it up and restore it.

    Ratty 05/2004 -05/07/2010 COOPER 01/08/1998-31/01/2012

  6. #6
    Join Date
    Oct 2011
    Location
    Sydney, NSW
    Posts
    1,176

    Default

    Hi,

    I think I'll break it down and put it into individual tubs of citric acid and see how it goes.

    I'll paint it up eventually.

    Ben.

Similar Threads

  1. Old forge photo
    By Lxe in forum THE SMITHY
    Replies: 3
    Last Post: 30th Mar 2016, 09:10 PM
  2. Old forge
    By Lxe in forum THE SMITHY
    Replies: 0
    Last Post: 21st Mar 2016, 01:52 PM
  3. forge questions
    By steamjunkprops in forum THE SMITHY
    Replies: 16
    Last Post: 23rd May 2014, 06:29 PM
  4. New old forge
    By Andy Mac in forum THE SMITHY
    Replies: 8
    Last Post: 17th Apr 2009, 12:08 AM
  5. Forge
    By JB in forum THE SMITHY
    Replies: 28
    Last Post: 21st May 2005, 07:55 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •