After much consideration and searching from, the good the bad and the ugly of AC tigs, I bought the Token Tools Elite 215A combo with plasma cutter.

Took just 7 days from order to arrival here in SW WA.

Packed extremely well and very impressed with the total package, I also bough some ally rods , tungsten's and a small torch.

Not fired up in anger as I need some argon first (have argon mix from my mig) so need to swop out at the big green shed, but it all lights up and seems fairly easy to understand the menus.

More to follow.

Oh and it's bloody heavy ! so I'm assuming a good sign of a quality unit.