    My bro picket a 1980's BMW for $300.

    He reckons it had been sitting stationary for at least 10 years and the remaining fuel in the tanks smells like turps.
    It has also turned some of the rubber parts inside the tank (not the hoses) into black goo and would like to know if it is decomposed fuel or turps or something else has been accidentally put in the tank

    He has a vid about it on his Youtube channel (FangitJoe) https://youtu.be/lO57w_a3Pq0 skip to about 9:30 if you just want to look at the goo.

    Thanks

  2. #2
    Join Date
    Feb 2014
    Location
    Melbourne
    Posts
    36

    Default

    Bob, I would say just decomposed fuel. Modern fuel does not store well and way worse if it has any ethanol - something I found out about the hard way.
    I had a fuel pump assembly in one of my Buells completely toasted after sitting for for 3 years.

    The fuel smelt really bad and had formed a layer of black sludge towards the bottom nicely covering the fuel pump assembly - here is what looked like it came off the Titanic.

    IMG_2177.jpg

    One interesting side effect was that all of the wiring had the exposed copper wiring dissolved well into the wires with just the plastic outer remaining.

Similar Threads

  1. Fuel Tank Strainer
    By Goggomobile in forum AUTO RESTORATION
    Replies: 2
    Last Post: 15th Jul 2016, 10:45 PM
  2. Fuel Tanks
    By Goggomobile in forum AUTO RESTORATION
    Replies: 9
    Last Post: 7th Jul 2016, 08:06 AM
  3. Just brazed up fuel tank-safely
    By Mathuranatha in forum WELDING
    Replies: 3
    Last Post: 8th Jun 2009, 09:43 PM
  4. brazing fuel tank?
    By Mathuranatha in forum WELDING
    Replies: 36
    Last Post: 26th Apr 2009, 12:14 PM
  5. Motorbike fuel tank repairer
    By Outsider in forum METALWORK GENERAL
    Replies: 6
    Last Post: 19th May 2008, 10:49 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •