    Default Stop Corrosion

    About a year ago we had a volcanic eruption.
    Our rainwater catchment tank is 15 years old and has had no problems until now.
    It has begun a relatively small but difficult corrosion problem.
    Sulphur gasses are probably the cause of its starting.
    I am getting ready to fix all the problems, then repaint it.

    The tank is about 18-1/2' dia X 5' high.
    The sides are painted galvanized corrugated steel, bolted together with the top layer overlapping the lower layer.
    I'm guessing, but I believe the overlap is no more than 6" or less.

    RIMG0274_sm.jpg
    I need to stop and seal the corrosion between the sheets before painting.
    An automotive anti-rust spray has been suggested.
    I'm still worried about corrosion above the sealant growing and breaking the seal with time.
    I do not want to drain the tank, then disassemble its walls to treat it, if possible.
    if I have to go that far I may just as well replce the tank.
    it don't needs replacing.

    Thoughts and suggestions on stopping and sealing the corrosion?

  2. #2
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    4,875

    Default

    Post was moved to General Engineering
    Grahame

  3. #3
    Join Date
    Aug 2008
    Location
    near Rockhampton
    Posts
    5,854

    Default

    I am not sure what you can do. Corrugated iron tanks here went out of favour once concrete tanks became commonplace, and now plastic tanks are replacing the concrete.

    However what was done to lengthen the life of the corrugated iron tanks once they started leaking was they were plastered with a concrete mortar which can last a surprisingly long time, I have also seen them fibreglassed which leaked like a sieve afterwards, then took up. Modern corrugated iron tanks are lined with a plastic liner, but I still think they have a poor life expectancy.
    Gold, the colour of choice for the discerning person.

Similar Threads

  1. How corrosion inhibitors protect metal
    By Driftabout in forum METALWORK GENERAL
    Replies: 0
    Last Post: 16th Jun 2019, 02:42 PM
  2. Corrosion on Stainless Steel
    By Karsty in forum METALWORK GENERAL
    Replies: 6
    Last Post: 3rd Nov 2016, 11:28 AM
  3. More on lube and anti corrosion /reclaimation
    By Grahame Collins in forum METALWORK GENERAL
    Replies: 3
    Last Post: 16th Apr 2012, 12:07 AM
  4. Aluminium on Steel corrosion problem?
    By JillB in forum METALWORK GENERAL
    Replies: 11
    Last Post: 16th Nov 2009, 08:30 PM
  5. Ironbark and Bolt corrosion
    By Don51 in forum METALWORK GENERAL
    Replies: 11
    Last Post: 9th Nov 2005, 02:40 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •