    I was exposed to bismuth as a part of melting it to make shot.i feel very sick now and I feel like I'm out of it. I have shivers and I can't stop shaking. My breathing feels shallow and my stomach hurts. Should I be worried or will this subside.

  2. #2
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    4,989

    Default

    Go to hospital emergency.

  3. #3
    Join Date
    Aug 2010
    Location
    Near Bendigo, Victoria, AUS
    Age
    68
    Posts
    2,696

    Default

    Bisnmujth is considered very safe. It is used as lead replacement in solder for food production utensils, as well as in large quantities in cosmetics and medicines (e.g. for diarrhoea).
    So it is unlikely that the bismuth is the culprit in your case What else was in the melt? Zinc, lead? You need to tell the emergency department as much as you can about the exposure, particularly any other metals, so they can test your blood levels of those. If it was just bismuth, you may well have other isues....
    What you so briefly describe sounds like zinc 'flue' or zinc poisoning. Not good.....
    Cheers, Joe
    again completely retired - more time to contemplate projects and spend more shed time....

Similar Threads

  1. Bismuth dangers
    By Jacarver18 in forum SAFETY FORUM
    Replies: 7
    Last Post: 20th May 2019, 08:07 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •