Search:
Type: Posts; User: RustyArc
Search: Search took 0.02 seconds.
-
15th Mar 2024, 08:44 AM
Thread: Specialty Steel Supply
by RustyArc- Replies
- 21
- Views
- 1,473
A Bare-co sales rep told me. Perhaps he mixed up...
A Bare-co sales rep told me. Perhaps he mixed up his numbers? Their web site says 1040 is their minimum spec, implying they may use “better” alloys in some cases.
-
12th Mar 2024, 09:43 AM
Thread: Specialty Steel Supply
by RustyArc- Replies
- 21
- Views
- 1,473
Bit late to this, but it’s worth mentioning that...
Bit late to this, but it’s worth mentioning that Bare-Co pins - sold in various sizes for tractor linkages - are 4140. Most tractor places stock a range of their pins. In Canberra, Tractor...
-
12th Dec 2023, 10:06 PM
Thread: Neat Little Welder
by RustyArc- Replies
- 3
- Views
- 750
When I first got a MIG machine I ran fluxcore,...
When I first got a MIG machine I ran fluxcore, and coming from stick, saw the smoke, spatter and slag as no big deal. I've been running gas for years since, but going back to fluxcore yesterday and...
-
12th Dec 2023, 04:08 PM
Thread: Neat Little Welder
by RustyArc- Replies
- 3
- Views
- 750
Neat Little Welder
I was helping out a neighbour yesterday sort out a little Toro diesel mower when we discovered a bit of flat bar across the deck had cracked off. He ran off and came back with a little gasless...
-
10th Oct 2023, 07:20 PM
Thread: Suggestions for theif proof gate lock
by RustyArc- Replies
- 61
- Views
- 3,945
This thread has ended up hitting on a number of...
This thread has ended up hitting on a number of issues - I'll add my 2 cents:
Crims hate sensor lights, so you can never have too many.
Never deal with an insurer directly. Use a broker, and... -
4th Oct 2023, 02:57 PM
Thread: Suggestions for theif proof gate lock
by RustyArc- Replies
- 61
- Views
- 3,945
I’ve got one of them Dingos that I bought...
I’ve got one of them Dingos that I bought primarily for trenching. I believe it’s a K9 4 - it has a 27hp diesel. It has a keyed latch that locks the flow divider such that there’s no flow to the...
-
16th May 2023, 09:49 PM
Thread: Fix for Shaft Pitting?
by RustyArc- Replies
- 12
- Views
- 1,435
Went with the speedi sleeve option - the one in...
Went with the speedi sleeve option - the one in stock was a few mm to wide, so after pressing on with some Loctite 515 as suggested, I put it back on the lathe, trimmed it back and then cleaned it up...
-
16th May 2023, 09:39 PM
Thread: Fix for Shaft Pitting?
by RustyArc- Replies
- 12
- Views
- 1,435
That would be a great upgrade, although I'm not...
That would be a great upgrade, although I'm not seeing the built-in sleeve? That said, some of the seal would be bearing on areas that aren't pitted, so wouldn't require any extra work.
I ended up... -
13th May 2023, 07:54 PM
Thread: Fix for Shaft Pitting?
by RustyArc- Replies
- 12
- Views
- 1,435
Well there's something I'd never heard of - I'm...
Well there's something I'd never heard of - I'm glad I asked :)
Looks like the ideal solution. The seal is 80x110x16, so a nominal 80mm one should do the job.
Thanks for the tip regarding... -
13th May 2023, 06:15 PM
Thread: Fix for Shaft Pitting?
by RustyArc- Replies
- 12
- Views
- 1,435
Fix for Shaft Pitting?
Had a leaky seal on a tractor wheel shaft. Where the seal makes cotact there's pitting. I've cleaned it up as best I can with emery paper, but am concerned the pitting will cause premature failure of...
-
12th May 2023, 01:24 PM
Thread: Metal cutting circular saw
by RustyArc- Replies
- 32
- Views
- 2,728
The GMC saw I have must be 10-15 years old....
The GMC saw I have must be 10-15 years old. They're as safe as any circular saw, which is to say, they need to be used with care.
While I rarely use the GMC freehand saw, I do use this almost... -
4th May 2023, 09:31 PM
Thread: Metal cutting circular saw
by RustyArc- Replies
- 32
- Views
- 2,728
I have a fairly old GMC carbide metal saw. On one...
I have a fairly old GMC carbide metal saw. On one occasion many years ago I needed to bring a length of 65x20 flat bar down to 60mm - I went through the options available and concluded that using the...
-
30th Mar 2023, 08:26 PM
- Replies
- 7
- Views
- 908
+1 for the Chicago Hush compressors. I had a...
+1 for the Chicago Hush compressors.
I had a Cut40 for a few years - I think it cost me $200 or something. It was good for up to 6mm or so, and it gave me the experience to determine if it'd be... -
9th Jan 2023, 01:47 PM
- Replies
- 4
- Views
- 670
I mill PCBs with the same carbide engraving bits...
I mill PCBs with the same carbide engraving bits - spindle runs at 24,000 RPM and does a very clean cut in copper.
-
8th Jan 2023, 01:38 PM
- Replies
- 4
- Views
- 670
Many years back I made up a bunch of signs using...
Many years back I made up a bunch of signs using Gravoply on my CNC router. From memory I used a common 10 degree carbide engraving bit - I might be able to dig up the job file and confirm that.
I... -
22nd Nov 2022, 09:06 PM
- Replies
- 28
- Views
- 3,942
If you're thinking about a MIG that does TIG,...
If you're thinking about a MIG that does TIG, this unit might be worth looking at:
https://www.bunnings.com.au/bossweld-mst185-plus-180a-mig-stick-and-tig-inverter-welder_p0274491
It comes with... -
31st Oct 2022, 01:40 PM
Thread: Shopping for a new air compressor
by RustyArc- Replies
- 50
- Views
- 6,362
Had to replace a compressor where I work - it...
Had to replace a compressor where I work - it was an angry little direct-drive unit that made a hell of a row, and often vibrated across the floor until it unplugged itself. I've been waiting more...
-
8th Sep 2022, 09:04 PM
Thread: 6 x 4 trailer crane
by RustyArc- Replies
- 40
- Views
- 8,903
I mounted one of these to my F150 cab chassis ute...
I mounted one of these to my F150 cab chassis ute many moons ago. The crane was positioned in the the front left corner of the tray with a removable setup that had the base plate welded to a length...
-
9th Aug 2022, 11:23 PM
Thread: Hand operated trailer mover
by RustyArc- Replies
- 46
- Views
- 9,015
That's a pretty impressive unit, particularly...
That's a pretty impressive unit, particularly with the steering feature. While it's a bit rowdy, I wonder if you're going to be able to make something much quieter, given the torque and gearing...
-
9th Aug 2022, 11:19 PM
Thread: Enclosed Trailer Fitout
by RustyArc- Replies
- 25
- Views
- 5,609
I'd been wondering where I could take this...
I'd been wondering where I could take this trailer to get a weighbridge reading on its weight, as I wasn't 100% confident that my approach of weighing one wheel and the jockey wheel while levelling...
-
6th Aug 2022, 03:37 PM
Thread: Enclosed Trailer Fitout
by RustyArc- Replies
- 25
- Views
- 5,609
I'm still totally confused about the weight...
I'm still totally confused about the weight rating of this trailer. I looked up the rego, and it is indeed rated at 2t ATM, and a tare of 440kg, which must have been before it was modified.
... -
4th Aug 2022, 07:00 PM
Thread: Enclosed Trailer Fitout
by RustyArc- Replies
- 25
- Views
- 5,609
I didn't describe my issue properly - the tank...
I didn't describe my issue properly - the tank will be sitting 50mm behind the axle - I'm just wondering if there's a risk the axle will move backwards as the springs flatten, and possibly hit the...
-
4th Aug 2022, 04:09 PM
Thread: Enclosed Trailer Fitout
by RustyArc- Replies
- 25
- Views
- 5,609
Another question for the brains trust. I'm...
Another question for the brains trust. I'm installing 2 small water tanks under the floor, ideally either side of the axle so the balance doesn't change much as one tank empties (although it'll be...
-
3rd Aug 2022, 01:53 PM
- Replies
- 18
- Views
- 2,796
A few years back I rang the local fastener shop...
A few years back I rang the local fastener shop as they'd recently taken over the stock of one of the bearing shops. I was put through to the "bearing guy". I was after a taper lock bush with a 25mm...
-
28th Jul 2022, 01:50 PM
Thread: M&G D1-4 Collet Chuck
by RustyArc- Replies
- 5
- Views
- 916
I purchased the same chuck and had the same...
I purchased the same chuck and had the same problem. I did post here regarding how to rectify it, but can't find it now. In the end I sent it back to M&G and they told me it fit their lathe fine,...
-
26th Jul 2022, 08:00 PM
Thread: Enclosed Trailer Fitout
by RustyArc- Replies
- 25
- Views
- 5,609
With the floor removed, along with the front and...
With the floor removed, along with the front and back panels of the trailer, I decided to weigh it again, as it's going to be the lightest it'll ever be. It came out at 580kg, which is close to half...
-
26th Jul 2022, 07:44 PM
Thread: Enclosed Trailer Fitout
by RustyArc- Replies
- 25
- Views
- 5,609
Yep, I'm currently going through grinding down...
Yep, I'm currently going through grinding down the welds that I plasma cut and wire wheeling rusty bits, then spraying with cold gal. Once I'm done, I'll probably add a coat of something, not sure...
-
25th Jul 2022, 09:12 PM
Thread: Enclosed Trailer Fitout
by RustyArc- Replies
- 25
- Views
- 5,609
There was a random bit of chequer plate on the...
There was a random bit of chequer plate on the drawbar that I was keen to remove, but revealed some worrying sings of rust:
399273
That and the odd, undulating floor lead me to decide to pull up... -
25th Jul 2022, 08:52 PM
Thread: Enclosed Trailer Fitout
by RustyArc- Replies
- 25
- Views
- 5,609
Double-sided tape is something I hadn't though of...
Double-sided tape is something I hadn't though of - it seems a lot more practical than using Sikaflex in terms of getting a consistent adhesive thickness - i.e. making sure everything ends up flat.
-
25th Jul 2022, 08:49 PM
Thread: Enclosed Trailer Fitout
by RustyArc- Replies
- 25
- Views
- 5,609
Bunnings flog polystyrene foam Foilboard in 10,15...
Bunnings flog polystyrene foam Foilboard in 10,15 & 20mm thicknesses. They may end up sponsoring this project, so that's definitely an option.
-
23rd Jul 2022, 11:35 AM
Thread: Trailer lights and wires
by RustyArc- Replies
- 21
- Views
- 4,179
I'd agree if the connection is flapping around in...
I'd agree if the connection is flapping around in the breeze, but if the connections are bundled together and secured with tape, I wouldn't be too concerned about brittle joints failing.
That... -
22nd Jul 2022, 08:55 PM
Thread: Trailer lights and wires
by RustyArc- Replies
- 21
- Views
- 4,179
I redid the trailer wiring on the enclosed...
I redid the trailer wiring on the enclosed trailer I'm fitting out in another thread - the long history of the trailer meant there were multiple generations of mods to the wiring, with lots of wads...
-
22nd Jul 2022, 11:34 AM
Thread: Enclosed Trailer Fitout
by RustyArc- Replies
- 25
- Views
- 5,609
I'm tempted to add insulation, but there's only a...
I'm tempted to add insulation, but there's only a 30mm gap in the walls, and 20mm in the roof, and there's a lot of random blocks of MDF that have been glued there, which I'm not sure how to remove...
-
21st Jul 2022, 06:16 PM
Thread: Enclosed Trailer Fitout
by RustyArc- Replies
- 25
- Views
- 5,609
Thanks for the comments - the axle is 40mm with 7...
Thanks for the comments - the axle is 40mm with 7 leaves on the spring, so I'm not sure what's going on there.
Since I don't do this kind of thing often, I went and modelled the trailer so I can... -
26th Jun 2022, 09:57 AM
Thread: drilling holes in star pickets
by RustyArc- Replies
- 17
- Views
- 4,419
I’ve used the plain steel ones extensively where...
I’ve used the plain steel ones extensively where I’ve cut them down, cut a new point, banged them in and then drilled holes to line up with sleepers to take batten screws. Drilled 6mm holes no...
-
25th Jun 2022, 02:13 PM
Thread: Enclosed Trailer Fitout
by RustyArc- Replies
- 25
- Views
- 5,609
I think I might have to take it over a...
I think I might have to take it over a weighbridge, as I can't quite accept that it weighs a tonne as it is.
I'm in the process of stripping out the lining, which looks to be 4mm ply, so that... -
24th Jun 2022, 09:43 PM
Thread: Enclosed Trailer Fitout
by RustyArc- Replies
- 25
- Views
- 5,609
Enclosed Trailer Fitout
I've volunteered to fit out an enclosed trailer to act as a mobile clinic. They've purchased this:
399022399021
Which it seems was originally for carrying motorbikes, hence the rear ramp, and... -
24th Jun 2022, 11:06 AM
Thread: New Lathe - AL-346V ?
by RustyArc- Replies
- 83
- Views
- 25,678
It'll get worse once you buy more tool holders -...
It'll get worse once you buy more tool holders - mine have all different Allen key sizes, to the point where I've taken to marking the top with a paint pen. From memory they're a mix of 3/16" and...
-
19th Jun 2022, 07:14 PM
Thread: Makita tool less AG locking flange
by RustyArc- Replies
- 17
- Views
- 2,680
My Metabo 5" has that nut, but I've never been...
My Metabo 5" has that nut, but I've never been brave enough to try the grinder lock trick, as I can't see how it's not going to damage the lock mechanism over time. My other corded 5" is a Flex...
-
6th Jun 2022, 04:45 PM
- Replies
- 10
- Views
- 2,036
I find Duragal welds reasonably well with no prep...
I find Duragal welds reasonably well with no prep and MIG gas, although it is nicer using CO2 gas. The much thicker hot-dipped gal is another matter.
-
3rd Jun 2022, 06:59 PM
- Replies
- 78
- Views
- 9,545
I purchased the 5C collet setup when I got my...
I purchased the 5C collet setup when I got my lathe. What I didn't realise is that the collets have a very limited clamping range, so, for example, the set you are getting can't clamp 1" stock with...
-
31st May 2022, 05:23 PM
- Replies
- 78
- Views
- 9,545
That's the live centre set I got, but in the MT3...
That's the live centre set I got, but in the MT3 version. Didn't come in no fancy box tho.
-
29th May 2022, 07:57 PM
- Replies
- 78
- Views
- 9,545
I probably should re-visit the Eccentric...
I probably should re-visit the Eccentric Engineering tooling I bought, see if I can identify an application for it that isn't covered by my collection of carbide insert and HSS tooling, and if not,...
-
28th May 2022, 07:48 PM
- Replies
- 78
- Views
- 9,545
When I got my lathe, being generally clueless...
When I got my lathe, being generally clueless about tooling, I got everything from H&F. Their stuff maybe overpriced compared to Aliexpress or Banggood, but the quality seems to be pretty decent. For...
-
28th May 2022, 02:51 PM
Thread: 8x5 Tipper Trailer
by RustyArc- Replies
- 28
- Views
- 6,452
I use Edcon Steel's online pricing to get an idea...
I use Edcon Steel's online pricing to get an idea of what a decent price is - my local supplier usually comes in pretty close to their pricing. That said, I haven't bought steel for 3-4 months, so I...
-
3rd May 2022, 08:24 PM
Thread: Shopping for a new air compressor
by RustyArc- Replies
- 50
- Views
- 6,362
I bought one of those Stanley units from...
I bought one of those Stanley units from Supercheap. I have no idea what the comparison must be to call these things “silent”, but it must be something like a jet engine, as it’s not term I’d use to...
-
2nd May 2022, 08:27 PM
Thread: Shopping for a new air compressor
by RustyArc- Replies
- 50
- Views
- 6,362
While I haven't bought one, I've always liked the...
While I haven't bought one, I've always liked the specs and quality of the P17.
-
30th Mar 2022, 10:33 AM
Thread: Compressed air line leaks.
by RustyArc- Replies
- 7
- Views
- 1,147
My Bunnings Pex-based air system for my shed has...
My Bunnings Pex-based air system for my shed has the "silent" air compressor going off about every4-5 days when not being used, which means it could be a tiny leak, so struggling to get motivated to...
-
19th Feb 2022, 08:48 PM
Thread: DIY sandblasting cabinet
by RustyArc- Replies
- 63
- Views
- 12,435
Getting 3 phase can be a variable experience. At...
Getting 3 phase can be a variable experience. At a property I work at, there was HV running along the edge of the property. but no transformers any where near. where we needed power. From memory it...
-
11th Feb 2022, 09:59 PM
Thread: 3.5T Flat deck trailer build
by RustyArc- Replies
- 102
- Views
- 23,312
Spotted this one in the wild the other day:...
Spotted this one in the wild the other day:
396857
Brand new 3.7 x 2.4 tipper with removable sides. Tare is 1.2t.
Detail of the tie-down rail, wiring & lights.
396856
Pivot point of...