  1. This just came up on my fb feed from 11 year's...

    This just came up on my fb feed from 11 year's ago my very second day of tig welding and i ran these beads, it was out in the wind and i had the machines fan blowing across the welds i did'nt know...
  2. Replies
    5
    Views
    344

    Yeah i may paint on the cold gal thank's for that...

    Yeah i may paint on the cold gal thank's for that tip

    Nah was'nt offended just been doing other thing's lately getting back into gardening veggies

    Had a lot on my mind, leading up to my mum's...
  3. Yeah still messing with outboards, current...

    Yeah still messing with outboards, current outboard was a bit of a steal tho, Yamaha 80hp 4 stroke 2003 cost $1500, another $300 to weld and machine the head and purchase gaskets, $50 for a control...
  4. Replies
    5
    Views
    344

    To buy a friend's trailer..

    A friend has offered me a Sea Link boat trailer the cross members and rear quarter of the main chassis has galvanize coating flaking off in big chunk's, it's a 3mm steel trailer just wondering how...
  5. A job from 9 year's ago, Outboard every bolt snapped

    This came up on my facebook from 9 year's ago i think it was one of the first tig job's i done, i used a Repco 140A arc welder converted to tig, No HF so was only scratch start and no anti stick on...
  6. Replies
    30
    Views
    1,394

    I started to build this homemade boat fuel tank...

    I started to build this homemade boat fuel tank it was only around 500mm wide the material was bendable 2.5mm aluminium, if you were to make a 1800mm wide similar bender you can run a series of holes...
  7. Replies
    11
    Views
    861

    Problem with that is it's a morse taper shaft so...

    Problem with that is it's a morse taper shaft so any side movement it will just fall out
  8. I'm not to sure they are just RCD...

    I'm not to sure they are just RCD switches/breakers which are resettable, one for stove and another for the big A/C
  9. Still getting the hang of welding in awkward...

    Still getting the hang of welding in awkward position's, today i tacked on a piece of 5mm flat bar to possibly 1.6mm round tubing, at first i had set the EWM to 30amp i was sure i was going to blow...
  10. Replies
    11
    Views
    861

    Looking around the internet u can get a 3/4"...

    Looking around the internet u can get a 3/4" weldon shank to fit the mag drill with a 1/2" 20 UNF threaded section to fit a er16 collet
  11. I had something like this a couple day's ago i...

    I had something like this a couple day's ago i had the main dinning room/lounge room 5kw air con going and turned the stove on and it shut the air con off even tho there are two RCD's thinking the...
  12. Replies
    11
    Views
    861

    Karl in the video he removes the magnet and...

    Karl in the video he removes the magnet and bolt's the mag drill to the frame using the magnet mounting hole's
  13. Replies
    11
    Views
    861

    Nifty little homemade mag drill mill

    I have been seeing mill's and lathe, drill, mill machines come up for sale just missed a lathe, mill, drill machine for $100 just did'nt think i would be able to carry it or move it, another one was...
  14. Replies
    28
    Views
    4,326

    Actually i just checked on the Edcon Steel...

    Actually i just checked on the Edcon Steel website i estimated 6 meters of 50x50x3mm shs it's showing 25.5kg that's just over $100 to galvanize at $4 per kilo to galvanize

    I will go this option...
  15. Replies
    28
    Views
    4,326

    Yeah it's Duragal i have been told HDG only comes...

    Yeah it's Duragal i have been told HDG only comes in heavier steel length's, i can go upto 75x75x3mm that's if i can find it in HDG, main chassis is 100x50mm so it should'nt look to awkward, at $4 a...
  16. Yeah i will likely be peddling up hill's that's...

    Yeah i will likely be peddling up hill's that's ok with assistance, i have read these MY1016 250w motor's arenot rated for continous duty cycle so i will have to go easy on it especilly if i need to...
  17. Replies
    28
    Views
    4,326

    Hey guys what are my option's for cross member's...

    Hey guys what are my option's for cross member's

    All i can find in 50x50x3mm is pre galvanised but it's not hot dipped galvanized, i really need to keep my GVM under 749kgs, old trailer rego paper...
  18. Who want's to peddle tho lol

    Who want's to peddle tho lol
  19. Just lost my reply lost internet connection,...

    Just lost my reply lost internet connection, sprocket's range about 54T-92T 92 is the biggest i have found so i will be ordering that, according to the link's above in there calculator's the speed...
  20. It would be the same thing tho Droog diameter of...

    It would be the same thing tho Droog diameter of x and x sprocket be it teeth or diameter both will work on a ratio
  21. Thank's for the link that website is awesome ...

    Thank's for the link that website is awesome

    According to the calculation my new 250watt motor will take 4.6mins to ride 1km up my street which is 3% grade at 13kph, 30 meter's rise over 1km,...
  22. I'm doing some circumference and ratio...

    I'm doing some circumference and ratio calculation's using a calculator so i'm probably all wrong

    25mm diameter main drive sprocket
    500mm wheel spocket
    Equils 20:1 ratio
    0.9n.m at 20:1 = 18n.m...
  23. That link trying to figure out the ratio to put...

    That link trying to figure out the ratio to put in the ratio is 1:6.33 when i add that number the calculatir reset's to 1, when i add a ratio of 6 i get 5.4N.M
  24. I ordered a new kit which includes one of these...

    I ordered a new kit which includes one of these MY1016 motor's, any idea how to calculate the torque output
    ...
  25. Just ran the test again it settles down to 21amp,...

    Just ran the test again it settles down to 21amp, for me to get any power out of this starter i'm not sure if it will be practicle, legal limit is 200watts for a Ebike this little motor pump's out...
  26. Just spun up the motor using the watt meter...

    Just spun up the motor using the watt meter battery was reading 11volt watt meter read 24amp 239watts only tested it for 3-4 second's, i will charge battery soon and get some stable number's
  27. Took 10min to remove the front wheel and fit a...

    Took 10min to remove the front wheel and fit a rear wheel to the front fork

    https://ibb.co/qr3PVDK
  28. NSW Sorry Kryn i just seen your post, I sold the chop...

    Sorry Kryn i just seen your post, I sold the chop saw 2 day's ago, bugger
  29. I thought about a clamp meter after i had...

    I thought about a clamp meter after i had purchased the watt meter bugger

    Anyway i just picked up a bike just a BMX shagged old thing from market place for $30 tried to buy a rear wheel to place...
  30. Thank's guy's, If i rewire it i will unwind the...

    Thank's guy's, If i rewire it i will unwind the armature and measure the total length of wire x the thickness and look up the Ohms spec's and pick a new wire and x diameter

    The starter is for a...
  31. Thank's :2tsup:, i pulled the motor apart again...

    Thank's :2tsup:, i pulled the motor apart again and measured the wire diameter it measured 0.40mm x 5T, wound around every 1 and 4 poles, there are 16 poles, i done a little reaserch looking for...
  32. As soon as i receieved the starter last week i...

    As soon as i receieved the starter last week i opened it up to check the winding's, i have no problem rewinding the armature i just don',t know how many turn's and what thickness wire to use

    It...
  33. It's a brush motor so i need to keep it at 12...

    It's a brush motor so i need to keep it at 12 volt's it's rated 50amp but i won't need that huge amount of power, 10-15amp possibly up to 20amp should be sufficient

    Thought about rewinding the...
  34. How to regulate current on a 12volt circuit

    Hey guy's how do i regulate current on a 12volt circuit to lower the speed of a electric motor?

    It's a starter motor i was going to rewind but hooked up a multimeter to test current and noticed it...
  35. NSW Mini 6in Chop Saw, Pipe/Bar Vice, Canley Heights

    Mini 6 inch chop saw look's rough as it sat out in the garden shed for 7 year's, got a workout once or twice a year, very easy to carry, takes a 150x2.5x22mm cutting disc available from bunnings, has...
  36. Replies
    13
    Views
    1,384

    Thank's for that link my local welding shop...

    Thank's for that link my local welding shop sell's them by the stick or kg :2tsup: will give those a try
  37. Replies
    13
    Views
    1,384

    Droog those cold gal paint's never work on...

    Droog those cold gal paint's never work on saltwater boat trailers a plan was to use tefgel but i may still use tefgel along with soldering the hole to seal the steel

    Trying to avoid adding extra...
  38. Replies
    13
    Views
    1,384

    Thank's China, i was'nt sure if solder would...

    Thank's China, i was'nt sure if solder would stick to steel :2tsup:
  39. Replies
    13
    Views
    1,384

    Soldering Hole in Steel?

    Hey Guy's, Can i drill a 13mm hole in steel than solder around the rim of the hole using a blow torch without burning off the galvanize? Hole will be redrilled to 12mm-12.5mm just need to keep the...
  40. Replies
    6
    Views
    505

    If weld need's to be tidy can u just key the bar...

    If weld need's to be tidy can u just key the bar and slot the flat bar into the round bar? I have seen lot's of people cut key slot's on the lathe
  41. Replies
    28
    Views
    4,326

    Video guy's...

    Video guy's https://youtu.be/lfUdtorsT3Q?si=bfPRxJRICR0jWQm8
  42. Replies
    28
    Views
    4,326

    Video Guy's, Not a professional video but giving...

    Video Guy's, Not a professional video but giving it a go

    https://youtu.be/lfUdtorsT3Q?si=bfPRxJRICR0jWQm8
  43. Replies
    28
    Views
    4,326

    I need 1370mm on the outsides of the main chassis...

    I need 1370mm on the outsides of the main chassis to fit my old trailer axle and spring hanger's with that i need a 90mm wide drawbar it's just the sweet spot the steel beam's rested at, i don't...
  44. Replies
    28
    Views
    4,326

    Was tempted to use left over PFC 100x50mm C...

    Was tempted to use left over PFC 100x50mm C channel for the drawbar but i will get a length of 100x100x3mm gal tubing for the drawbar so there's no twisting when i turn corner's
  45. Replies
    28
    Views
    4,326

    Main frame is bent and cut to size, one side is...

    Main frame is bent and cut to size, one side is sitting lower on the grass and the otherside is sitting on the concrete so it appear's one side is twisted but they are both bent straight
  46. Replies
    28
    Views
    4,326

    Hey guy's i got my 4x bend's made, the two bend's...

    Hey guy's i got my 4x bend's made, the two bend's bending away from the flange turned out perfect, the two bend's bending towards the flange not so great 1 set of flanges bent out the other piece...
  47. Replies
    28
    Views
    4,326

    I put a little more bend into the first bend on...

    I put a little more bend into the first bend on the length than proceeded to make the second bend it was late about 6:30-7pm dropped a few pieces of steel and only cracked it once and said "" out...
  48. Replies
    1
    Views
    598

    Upload Speed?

    Has admin reduced my upload speed it's taking 1min per 1mb to upload, happy to stop posting if that's the case

    Over 20min's to upload 3 picture's
  49. Replies
    28
    Views
    4,326

    Some pic's of the bend's, no galvanize cracking...

    Some pic's of the bend's, no galvanize cracking yet
  50. Replies
    44
    Views
    3,139

    I just checked my vernier caliper is off by...

    I just checked my vernier caliper is off by 00.20mm