Search:

Type: Posts; User: qwertyu

Search: Search took 0.00 seconds.

  1. Replies
    8
    Views
    1,782

    Any tips on lining up drill bits in the drill...

    Any tips on lining up drill bits in the drill doctor that have a split point? I have major issues lining up my P&N set. its a 135deg with splint point
  2. Replies
    3
    Views
    649

    This: Dulux ZINCSHIELD 2 9907036M ...

    This: Dulux ZINCSHIELD 2 9907036M

    https://duluxpowders.com.au/products/zincshield/

    this is the top coat https://duluxpowders.com.au/products/duralloy/

    it says that its good indoors and even...
  3. Replies
    3
    Views
    649

    Powder coating - zinc undercoat vs none

    For something that is being kept indoors, is zinc undercoating required for something made of mild steel and has been sand blastered? I get mixed responses from people - some say it looks the same...
  4. Aluminium pot modifications for induction cooktop

    This is a bit of a weird one. Planning to switch to induction cooktop and have a giant aluminium steamer which will not work on it. Im thinking it would be good to bond some stainless to the...
  5. Ordered Adflo with versaflo shield. will get...

    Ordered Adflo with versaflo shield.

    will get welding helmet in the future if I can justify it/do more welding

    the earmuffs designed for the versaflo (and I think speedglas too) (3M H31P3) ...
  6. Thanks everyone. I think I will stick with 3M, an...

    Thanks everyone. I think I will stick with 3M, an extra $500 for safety on an item that will last years is probably worth it. Also makes buying spare parts easier too. So even though I will be doing...
  7. Tecmen powered faceshield vs 3M adflo vs 3M versaflo

    I posted this in the WWF but figured its worth posting here too. I am after a PARP mainly for woodworking and the occasional welding too. It would be nice if there are filters for spray painting too...
  8. Replies
    7
    Views
    1,142

    Thanks all for your replies. The item would be...

    Thanks all for your replies. The item would be indoors and not in a 'salty' area.

    Im inquiring with a few places regarding powder coating - what is the sandblasting step for? Is that worth doing? ...
  9. Replies
    7
    Views
    1,142

    Blackening metal vs powder coating

    Curious what is a more durable finish - powder coating vs blackening by heating and rubbing on oil like in this video:
    https://www.youtube.com/watch?v=hz6wdvraC-g

    That blackening process is like...
  10. Replies
    22
    Views
    7,508

    Hi thanks for the response. Yes that is the exact...

    Hi thanks for the response. Yes that is the exact welder I have.

    The voltage for all those beads was 24v (max) and the wirespeed is what I wrote in green. Wire stick out is about 10mm and they...
  11. Replies
    22
    Views
    7,508

    Would be much appreciated to get an opinion on my...

    Would be much appreciated to get an opinion on my question. I know this is a forum of people who enjoy working with metal and discussion is great but would love to hear what you guys think about...
  12. Replies
    22
    Views
    7,508

    I tried running the welder on max voltage at...

    I tried running the welder on max voltage at different wire speeds - 14/13/12/11/10 on some 10mm flat bar which removed the mill scale from

    394875394876

    Looking at these, are any better than...
  13. Replies
    22
    Views
    7,508

    Thanks for the responses! If I wanted to also...

    Thanks for the responses!

    If I wanted to also weld the 10mm to 2.5mm steel, would a stick welder be a good bet too? My machine came with a stick welder too
  14. Replies
    22
    Views
    7,508

    10mm settings on unimig viper 185

    I recently purchased a unimig viper 185 and I want to weld some 10mm flat bar. I am using gas and the 0.9mm wire that came with the machine. The table inside the side panel only shows settings for up...
  15. Replies
    16
    Views
    2,477

    Is this the best thing to use to remove it? 3M...

    Is this the best thing to use to remove it? 3M clean and strip?

    https://www.blackwoods.com.au/abrasives/non-woven-abrasives/clean-strip/disc-s-brite-3m-cleanandstrip-prp-dc-125mm/p/05342529

    I...
  16. Replies
    16
    Views
    2,477

    Newby painting/preping steel

    I bought some mild steel from Surdex over the weekend. Its not painted or anything and just coated in oil.

    I cleaned the oil off and I notice that the surface is really dark. Do I need to remove...
  17. Replies
    22
    Views
    9,537

    I still havent bought the welder yet - will...

    I still havent bought the welder yet - will probably do so next week. On the shopping list is:


    Unimig Razorweld 200A (I decided to get a 200A since why not and decided against second hand cause...
  18. Replies
    22
    Views
    9,537

    Great - is there much difference between various...

    Great - is there much difference between various brands of wire? Seems to be a pretty big price range:

    https://www.totaltools.com.au/111582-michigan-mild-steel-wire-0-9mm-15kg-mer70s60915...
  19. Replies
    22
    Views
    9,537

    Another question - welding 2.5 or 3mm mild steel...

    Another question - welding 2.5 or 3mm mild steel together or to 10mm mild steel - what size mig wire should I be getting? I saw a chart which says 1mm but I can only find 0.9 or 1.2mm
  20. Replies
    22
    Views
    9,537

    Where is the best place to look for second hand...

    Where is the best place to look for second hand units? I looked on machines4u and there was one for $400 but that was it.

    Just wondering - what sort of situations do people use a tig welder when...
  21. Replies
    22
    Views
    9,537

    I dont know whats going on it seems like my posts...

    I dont know whats going on it seems like my posts arent getting submitted :S

    Anyway - I should mention that I hope to weld up to 10mm flat bar to 2.5mm box section - are these migs up to the task?...
  22. Replies
    22
    Views
    9,537

    I should also probably add - Would like to weld...

    I should also probably add - Would like to weld the 10mm flat bar to the box section occasionally - hope MIG is best for that.

    In regards to TIG functionality, would be nice to be able to weld up...
  23. Replies
    22
    Views
    9,537

    Buying first mig welder

    I posted this and just before and it seems to have disappeared

    I want to buy my first mig welder, I have only ever used a stick welder once. I want to weld mild steel 2.5mm and occasionally 10mm...
  24. Replies
    1
    Views
    2,051

    Buying first mig welder

    I would like to buy a MIG welder - but I have no idea what is suitable. I have 15amp and 3 phase power and would like to weld 2.5mm mild steel mostly and maybe sometimes 10mm flat bar.

    I have...
Results 1 to 24 of 24