Thanks Kryn, just tried cutting through,...
Thanks Kryn, just tried cutting through, penetration looks good. I'v managed a couple of decent welds this afternoon, but inconsistent. I guess that means it's more me than the settings. I'll try...
-
30th Jun 2019, 01:39 PM
Thread: Welding aluminium- weld building up...
by silkwood- Replies
- 3
- Views
- 2,354
Welding aluminium- weld building up...
I'm practicing welding aluminium (I did a search but couldn't find a specific answer, sorry) and sometimes I get it, sometimes I don't- hence the need to practice! I am using a spool gun with argon...
-
18th Feb 2019, 10:30 AM
- Replies
- 12
- Views
- 6,156
Thanks for all the feedback, people. As stated, I...
Thanks for all the feedback, people. As stated, I appreciate the advice as I do not know the first thing about MIG or TIG (well, I know the basics I have read up on).
Well aware I will need to... -
13th Feb 2019, 01:14 PM
- Replies
- 12
- Views
- 6,156
Budget welder for occasional aluminium welding..