Search:
Type: Posts; User: Superbunny
Search: Search took 0.02 seconds.
-
6th Jan 2021, 07:39 PM
Thread: Mig 0.6mm gassless wire
by Superbunny- Replies
- 7
- Views
- 2,470
Thanks guys, I have now solved my problems with...
Thanks guys, I have now solved my problems with welding thin steel based on your advice and now I am welding much better with success. I practice nearly every day to gain the skill needed to become...
-
23rd Dec 2020, 10:38 AM
Thread: Mig 0.6mm gassless wire
by Superbunny- Replies
- 7
- Views
- 2,470
So I gather that this stuff is not common then. I...
So I gather that this stuff is not common then. I want to use it for thinner mild steel as I have reduced the current and still getting some blow through on my welds. I'm happy to admit that it could...
-
22nd Dec 2020, 09:04 PM
Thread: Mig 0.6mm gassless wire
by Superbunny- Replies
- 7
- Views
- 2,470
Mig 0.6mm gassless wire
I'm having trouble finding 0.6 gassless mig welding wire, got any ideas where I might source some in 1kg please. I tried eBay and no show, I'm guessing maybe 0.6 is not a gassless product, I don’t...
-
27th Feb 2013, 09:44 PM
Thread: Forum Runner app on iPad problems?
by Superbunny- Replies
- 12
- Views
- 6,683
Is this the same problem as I'm having with my...
Is this the same problem as I'm having with my latest IPad in that I just use the normal safari web browser and when I try to post a reply I find my screen freezes and I have to do a complete reboot...
-
25th Jun 2010, 03:29 PM
Thread: Pictures in an album
by Superbunny- Replies
- 1
- Views
- 4,039
Pictures in an album
Here is one for the moderators. I've gone to all the effort to put together some albums of my work so others can enjoy but I can't specify the order that pictures in the album are placed in to show a...
-
24th Feb 2010, 09:15 PM
Thread: logging on
by Superbunny- Replies
- 3
- Views
- 4,621
Yes, that must be the problem and I didn't notice...
Yes, that must be the problem and I didn't notice this was the cause, thanks.:D:D
SB -
23rd Feb 2010, 10:13 PM
Thread: logging on
by Superbunny- Replies
- 3
- Views
- 4,621
logging on
In recent times I log on to the forum and it always asks for my user name and password even though I checked the remember me. Do you know why this is happening please.:D:D
SB -
6th Jan 2010, 09:45 PM
Thread: sharft and bushes help needed.
by Superbunny- Replies
- 6
- Views
- 5,353
Thanks for help guys, I got the bushes from an...
Thanks for help guys, I got the bushes from an auto electrcian, and the shaft from a local engineering coy. It took me half a day to locate going from recommendation to recommendation.:D:D
SB -
4th Jan 2010, 10:24 PM
Thread: sharft and bushes help needed.
by Superbunny- Replies
- 6
- Views
- 5,353
sharft and bushes help needed.