I would try Boiled Linseed oil. It dries but...
I would try Boiled Linseed oil. It dries but stays sort of rubbery I think . I did a test patch on a mild steel gate over the rust that was already on it years ago and every time I checked for the...
-
12th Oct 2023, 03:37 PM
Thread: Lathe Gears Question.
by auscab- Replies
- 15
- Views
- 1,780
Thanks Kafie that is an amazing thing to see! I...
Thanks Kafie that is an amazing thing to see!
I may have to try to use that gear calculator to figure out gears I may need if they are not already with the machine for what I want to produce .
I... -
11th Oct 2023, 10:45 PM
Thread: Lathe Gears Question.
by auscab- Replies
- 15
- Views
- 1,780
Good idea . That's how I like to cut my mouldings...
Good idea . That's how I like to cut my mouldings with the router. It gives the best finish.
-
11th Oct 2023, 08:41 PM
Thread: Lathe Gears Question.
by auscab- Replies
- 15
- Views
- 1,780
That's good. Thanks Elan. I don't think there is...
That's good. Thanks Elan.
I don't think there is a problem with the direction as the reverse is only reversing the spindle. The tool carriage does its job starting the cutting from right to left.... -
11th Oct 2023, 07:53 PM
Thread: Lathe Gears Question.
by auscab- Replies
- 15
- Views
- 1,780
Thanks for all the reply's . Right or wrong. I...
Thanks for all the reply's . Right or wrong. I like the sound of it not changing the surface speed of the spindle . So I'm crossing my fingers that is correct.
I'm not making a machine but am... -
10th Oct 2023, 10:31 PM
Thread: Lathe Gears Question.
by auscab- Replies
- 15
- Views
- 1,780
Lathe Gears Question.
I"m trying to understand the gears on a wood lathe that has a lead screw and a tool carriage with a spinning cutter that cuts something similar to a screw in the wood . It cuts a Barley Twist...
-
11th Sep 2023, 11:06 PM
Thread: Hercus 9" lathe milling attachment.
by auscab- Replies
- 18
- Views
- 2,350
Hi Bob. That looks good thanks. Ive seen those...
Hi Bob.
That looks good thanks. Ive seen those Myford Milling attachment Copys. Good to see an Original Myford one.
This is the ebay one looks the same as Your amazon one I think.... -
9th Sep 2023, 11:47 PM
Thread: Hercus 9" lathe milling attachment.
by auscab- Replies
- 18
- Views
- 2,350
Thanks Tinkerer77. The Hercus attachment is a...
Thanks Tinkerer77.
The Hercus attachment is a bit different to the south Bend.
I thought they would have been a much closer design . Doesn't matter though.
Hercus picture I found left... -
9th Sep 2023, 09:18 AM
Thread: Hercus 9" lathe milling attachment.
by auscab- Replies
- 18
- Views
- 2,350
Does any one have or know of decent pictures of...
Does any one have or know of decent pictures of the Hercus Milling attachment.
There is probably some on forum here somewhere ?
Id like to see and compare at least to the South Bend ones Im... -
9th Sep 2023, 09:10 AM
Thread: Hercus 9" lathe milling attachment.
by auscab- Replies
- 18
- Views
- 2,350
Hi Baron J, It is just a small thing I'd like...
Hi Baron J,
It is just a small thing I'd like to try out doing. Just playing around though.
Pretty sure Ive seen milling attachments In AU for sale over the years but let them pass. You have to... -
9th Sep 2023, 08:50 AM
Thread: Hercus 9" lathe milling attachment.
by auscab- Replies
- 18
- Views
- 2,350
No it doesn't have to be genuine Hercus . Be nice...
No it doesn't have to be genuine Hercus . Be nice if it was.
Ill keep looking at the cheap imported ones. The South Bend ones I see look good but don't seem to be the exact same as what Hercus did. -
8th Sep 2023, 11:49 PM
Thread: Hercus 9" lathe milling attachment.
by auscab- Replies
- 18
- Views
- 2,350
Hercus 9" lathe milling attachment.
Is the Hercus 9" Lathe milling attachment available anywhere in Australia?
Anyone know of one for sale?
The Southbend ones show up on US ebay . Is that the only option?
Or what options are... -
30th Aug 2023, 09:57 AM
Thread: Making a tap for brass or bronze from 4140
by auscab- Replies
- 9
- Views
- 701
Yeah ? Just HT bolts from where? Do you anneal...
Yeah ? Just HT bolts from where? Do you anneal them first . Machine then harden and temper or just harden?
-
30th Aug 2023, 09:43 AM
Thread: Making a tap for brass or bronze from 4140
by auscab- Replies
- 9
- Views
- 701
I'm copying an antique hand plane for wood and...
I'm copying an antique hand plane for wood and just want to stick to the style that was used so it looks right. And the feel. And my lathe (Hercus) is imperial.
I could use these Acme taps.... -
30th Aug 2023, 12:38 AM
Thread: Making a tap for brass or bronze from 4140
by auscab- Replies
- 9
- Views
- 701
I do have some 01 steel but its only 12mm so not...
I do have some 01 steel but its only 12mm so not large enough for the 1/2" tap I need. 12mm was the largest the supplier had . I need it for another project.
If 01 is more suitable to make a tap... -
30th Aug 2023, 12:13 AM
Thread: Making a tap for brass or bronze from 4140
by auscab- Replies
- 9
- Views
- 701
Making a tap for brass or bronze from 4140
If I want to make a tap to tap a 3/8 or 1/2 inch hole in brass or bronze out of 4140 that'll work wont it ?
It'll cut those materials being harder? Would it cut mild steel as well ?
I want to do... -
16th Aug 2023, 09:22 PM
- Replies
- 26
- Views
- 2,185
Yeah that's about it . You can go more than 2/3...
Yeah that's about it . You can go more than 2/3 of thickness. What ever it takes to bend it easy will do . Maybe leave .5 mm and just hand bend it or use a shifter. .
This is a little bend I did... -
16th Aug 2023, 01:08 AM
- Replies
- 26
- Views
- 2,185
I learned a great way of fabricating parts like...
I learned a great way of fabricating parts like this off a mate who spent some time helping a pro metal worker installing a steel staircase handrail around corners in a building. Once I found out...
-
1st Sep 2022, 11:23 PM
Thread: Turning 4140 and HSS
by auscab- Replies
- 22
- Views
- 2,282
I'm fixing a pair of Wadkin PK twin mitre fences...
I'm fixing a pair of Wadkin PK twin mitre fences Tony. Ive got two old pins . They both don't fit properly which is fine, I'll make one that does. The annoying thing about those originals is they...
-
30th Aug 2022, 11:09 PM
Thread: Turning 4140 and HSS
by auscab- Replies
- 22
- Views
- 2,282
So is EN 25 machined then hardened after...
So is EN 25 machined then hardened after machining ?
Ive got an old Hercus lathe . I did the Knurl on the end of that old knob above . With a push knurl . Lots of passes with oil. I try and keep... -
30th Aug 2022, 10:17 PM
Thread: Turning 4140 and HSS
by auscab- Replies
- 22
- Views
- 2,282
I rang the local engineering place that I buy...
I rang the local engineering place that I buy steel from . No 1030 or 1045 . They just have 4140 or a type called EN25 which I looked up and doesn't sound like it would do . Not sure but it sounds...
-
30th Aug 2022, 10:58 AM
Thread: Turning 4140 and HSS
by auscab- Replies
- 22
- Views
- 2,282
Thanks for the help. I went and did some...
Thanks for the help.
I went and did some YouTube viewing of cut knurling last night . looks interesting and nice but I don't want to go buying more tools and learning that atm .
Ill ask about... -
29th Aug 2022, 11:35 PM
Thread: Turning 4140 and HSS
by auscab- Replies
- 22
- Views
- 2,282
What would be better to make them from then ? Ive...
What would be better to make them from then ? Ive only turned Mild steel 4140 and brass so far.
Something that's common to buy . I want a good knurl but have only done the push type . Its just that... -
29th Aug 2022, 10:40 PM
Thread: Turning 4140 and HSS
by auscab- Replies
- 22
- Views
- 2,282
Turning 4140 and HSS
I forget if I have asked part of this before. Apologies if I have .
I want to make some fittings out of 4140 soon.
I was also turning some simple 4140 stub axles for a machine trolley out of it... -
25th Aug 2022, 09:00 AM
Thread: Heating and cooling cast iron .
by auscab- Replies
- 3
- Views
- 714
Thanks Grahame. Rob
Thanks Grahame.
Rob -
25th Aug 2022, 01:34 AM
Thread: Heating and cooling cast iron .
by auscab- Replies
- 3
- Views
- 714
Heating and cooling cast iron .
If I heat this cast iron clamp to red hot where needed to bend the casting back straight, is it best to just let it air cool on the floor?
Would quenching in cold water make the cast iron brittle... -
23rd Jul 2022, 08:28 PM
Thread: Trailer lights and wires
by auscab- Replies
- 21
- Views
- 4,172
Yes Chris that would be nice . Backing the HF up...
Yes Chris that would be nice . Backing the HF up a lane and around a corner cost me $600 when I hit a car a while back . :((
Melbourne roads and lane ways are a nightmare with trailer or HF .... -
23rd Jul 2022, 07:56 PM
Thread: Trailer lights and wires
by auscab- Replies
- 21
- Views
- 4,172
Crimping sounds like its worth a look . Do you...
Crimping sounds like its worth a look . Do you not heat shrink it though ? Do the plastic covers that come with them do the job ?
I was looking at the bad wiring today on the horse float. Two are... -
22nd Jul 2022, 08:52 PM
Thread: Trailer lights and wires
by auscab- Replies
- 21
- Views
- 4,172
That's the box under my dashboard ? 7...
That's the box under my dashboard ?
7 pin Flat. Think I may have a new one already -
22nd Jul 2022, 11:44 AM
Thread: Trailer lights and wires
by auscab- Replies
- 21
- Views
- 4,172
Thanks Kryn . I'm just starting to Youtube all...
Thanks Kryn .
I'm just starting to Youtube all I can to get prepared to do this. Electrical and me = things can go wrong so I want to get prepared. Ive seen 12V things smoking before. In the days... -
22nd Jul 2022, 12:51 AM
Thread: Trailer lights and wires
by auscab- Replies
- 21
- Views
- 4,172
Trailer lights and wires
Whats a good way to buy new lights plugs and wires to re do a horse float with electric brakes?
It needs a total re wire.
Im in country Vic . Sth Gippsland .
Should I buy the parts through... -
21st Jul 2022, 09:36 PM
Thread: Drilling HSS
by auscab- Replies
- 15
- Views
- 1,530
Tungsten is not ground on CBN though is it ?
Tungsten is not ground on CBN though is it ?
-
21st Jul 2022, 11:54 AM
Thread: Drilling HSS
by auscab- Replies
- 15
- Views
- 1,530
Thanks Snapey. That is a nice neat hole. ...
Thanks Snapey.
That is a nice neat hole.
When I want to show video I load it onto my instagram then put a link to that instagram post in the thread.
Old masonary bit is something I tried on... -
20th Jul 2022, 10:04 PM
Thread: Drilling HSS
by auscab- Replies
- 15
- Views
- 1,530
Ive got a standard cheap Asian drill press. An...
Ive got a standard cheap Asian drill press. An old flat belt driven camel back not running atm but I could get it going. And also a belt driven wood mill with a collet chuck that runs at something...
-
20th Jul 2022, 08:53 PM
Thread: Drilling HSS
by auscab- Replies
- 15
- Views
- 1,530
Drilling HSS
What drill bits do you go looking for to buy for drilling holes in HSS ?
Are they TCT? or solid Tungsten ? Is it done with Milling bits ?
I would possibly be drilling 6 to 10 mm thick HSS . Or... -
22nd Sep 2021, 02:23 AM
Thread: Desktop water jet.
by auscab- Replies
- 9
- Views
- 1,319
I checked that out on the H&F website . Read...
I checked that out on the H&F website . Read through the materials and speeds . Wood is not listed as one . Plastics and soft metals are listed so it would be capable of cutting say 12.5 mm wood...
-
17th May 2021, 09:14 PM
- Replies
- 17
- Views
- 2,518
Thanks . Ive had a look there before and just...
Thanks .
Ive had a look there before and just went back for another . I notice since their new website has been up the range of HSS either hasn't been fully loaded on yet or the range has been... -
16th May 2021, 12:26 PM
- Replies
- 17
- Views
- 2,518
Great . Something I may try out thanks . I...
Great . Something I may try out thanks .
I used my Mig welder with the standard welding wire. After a fail I tried one weld by heating to red hot then welding and leaving to cool slowly buried in... -
16th May 2021, 08:51 AM
- Replies
- 17
- Views
- 2,518
I did think of that but welding HSS doesn't work...
I did think of that but welding HSS doesn't work . Ive done it a number of times and it did stay on one piece once but mostly it just falls off with the slightest pressure.
So in another... -
15th May 2021, 10:37 PM
- Replies
- 17
- Views
- 2,518
Thanks Kryn. We both went and did the same...
Thanks Kryn.
We both went and did the same thing after I posted :).
I think Ive searched at least 6 times on Ebay for such sizes over the last year. A few times in the US .
I want to make... -
15th May 2021, 10:18 PM
- Replies
- 17
- Views
- 2,518
Hopefully its OK stuff . Anyone seen or used it...
Hopefully its OK stuff . Anyone seen or used it before ?
Should be good if it is US stuff.
https://www.ebay.com.au/itm/383391255990?hash=item5943e64db6:g:GYoAAOSwBsleLZFP -
15th May 2021, 10:14 PM
- Replies
- 17
- Views
- 2,518
I just found some on Ebay in the USA . I have...
I just found some on Ebay in the USA .
I have looked there before ( A number of times) but found nothing that size.
Rob -
15th May 2021, 09:42 PM
- Replies
- 17
- Views
- 2,518
Is there a place where 1/2" x 1" HSS tool blanks can be bought ?
1/2" x 1" x 4" long or 8 " long would be good .
Rob -
9th May 2021, 11:22 AM
Thread: Metric threading on Imperial 9"AR Hercus
by auscab- Replies
- 9
- Views
- 2,645
Thank you Tony . I will store that info you...
Thank you Tony .
I will store that info you sent and do a print out for the workshop.
Rob -
9th May 2021, 11:16 AM
Thread: Metric threading on Imperial 9"AR Hercus
by auscab- Replies
- 9
- Views
- 2,645
Thanks Steve . Tony sent me the same, ...
Thanks Steve . Tony sent me the same, explanations from a couple of angles is a great help.
Rob -
8th May 2021, 08:15 PM
Thread: Metric threading on Imperial 9"AR Hercus
by auscab- Replies
- 9
- Views
- 2,645
Thanks Tony I will send a PM . Ill print it out ....
Thanks Tony I will send a PM . Ill print it out .
That left chart, whats the lever positions , they go up to 80 ?
Rob -
8th May 2021, 07:18 PM
Thread: Metric threading on Imperial 9"AR Hercus
by auscab- Replies
- 9
- Views
- 2,645
I found these for the 260 lathe in my TBOT. ...
I found these for the 260 lathe in my TBOT.
Is using these for my AR lathe with same 8TPI lead screw OK ?
391999 392000
I don't understand the gear lever positions either from the chart... -
8th May 2021, 05:43 PM
Thread: Metric threading on Imperial 9"AR Hercus
by auscab- Replies
- 9
- Views
- 2,645
Metric threading on Imperial 9"AR Hercus
I have a imperial 9" Hercus AR.
And a gear set for metric and maybe other stuff I bought through AMH a few years ago.
The transition gears (Right Name ?) are not the 100 to 127 bushed pair but... -
4th May 2021, 11:12 PM
Thread: Text Book Of Turning . Hercus
by auscab- Replies
- 4
- Views
- 2,153
Hi Steve . That looks great Thanks. I replied...
Hi Steve .
That looks great Thanks. I replied to the PM and sent my phone number. No need for more pics .
Just Price and bank details .
Rob -
4th May 2021, 08:38 PM
Thread: Text Book Of Turning . Hercus
by auscab- Replies
- 4
- Views
- 2,153
Thanks Steve . I hope you do have a few and can...
Thanks Steve .
I hope you do have a few and can part with one .
Rob