    10,110

    Thank you for the picters. Any suggestions where...

    Thank you for the picters. Any suggestions where I can buy new springs.
    Mine functions oke, but is damaged. I'm afraid it'll break in the near future.
  2. Thread: HyLo vice

    by Spieker
    Replies
    20
    Views
    10,110

    385622 This is what I mend. This is where one...

    385622 This is what I mend. This is where one end of the spring will fit in.? Right.?
  3. Thread: HyLo vice

    by Spieker
    Replies
    20
    Views
    10,110

    Hello Thread, thanks for your reply. I have the...

    Hello Thread, thanks for your reply. I have the spring, but I wasn't clear. I mean, what is more clear at picture 2, sort of cap that can be screwed on the messing knob.?!
    greetings John
  4. Thread: HyLo vice

    by Spieker
    Replies
    20
    Views
    10,110

    What's missing here

    Hello people,

    My nam's John, I introduced myself in the GDay Yall.
    I bought this nice Hylo 2 speed vice, but there is somthing missing.
    My question:
    can you tell me what it is that's missing....
  5. Replies
    4
    Views
    2,376

    Some examples of things I forged

    385592385593
  6. Replies
    4
    Views
    2,376

    Always learning and curious.

    Hello to yall,

    My name is John, age 61 and I'm living in a small town called Elburg in the Netherlands.

    After working for more than 30 years as a woodworker, I started 8 years ago as a metal...