  1. Aah yes, that would be a good way to fix it. not...

    Aah yes, that would be a good way to fix it. not thought about that. Actually I hope i will not have to fix my muffler anytime I have my current motorcycle. It is the only good transportation I...
  2. Hello, It is an rust converter paint (Brunox...

    Hello,

    It is an rust converter paint (Brunox primer) on the spot, then I paint it over. But the rust inside cannot be reached completely. It is showing a bit of rust through the paint a bit.
    ...
  3. Today I asked a motorcycle sales person /...

    Today I asked a motorcycle sales person / "mechanic"?. He said it will take ages to rust through. On the internet I read when metal becomes warmed / heated it will rust faster. So, I decided to buy a...
  4. Many thanks for the replies! Previous owner...

    Many thanks for the replies!

    Previous owner did a engine revision: new clutch plates, clutch springs, oil,new spark plugs. new light as it was damaged. Enough thread on tyres. Just a slide damage...
  5. Damaged chrome plating and bare metal spot motorcycle exhaust

    Hello all,

    I have a question how i might be able to fix a bare scraped motorcycle exhaust end. The spot has scraped against the pavement and is about 2 cm by 7 cm big. The chrome is gone and the...