Search:
Type: Posts; User: Jacarver18
Search: Search took 0.00 seconds.
-
13th May 2019, 10:35 AM
Thread: Bismuth dangers
by Jacarver18- Replies
- 7
- Views
- 9,951
I went to the emergency room and they said I had...
I went to the emergency room and they said I had become dangerously dehydrated and low on potassium as well as there is the presence of protein in urine. They don't know if there will be further...
-
11th May 2019, 10:32 AM
Thread: Bismuth help!!!
by Jacarver18- Replies
- 8
- Views
- 22,930
Bismuth help!!!
I was exposed to bismuth as a part of melting it to make shot.i feel very sick now and I feel like I'm out of it. I have shivers and I can't stop shaking. My breathing feels shallow and my stomach...
-
11th May 2019, 10:24 AM
Thread: Bismuth dangers
by Jacarver18- Replies
- 7
- Views
- 9,951
Bismuth dangers
I was making bismuth crystals and thought I had enough ventilation but I was wrong. I seemed to have been exposed as now I feel very Ill. I have shivers and feel very sick. I can't concentrate and...