30th Sep 2009, 01:02 PM
Thread: Contact Welding Rods
by echnidna- Replies
- 8
- Views
- 8,086
Apparently there are 2 different types of spot...
Apparently there are 2 different types of spot guns
one uses carbon rods
the other uses conventional rods so it could be used to stitch weld as well as spot weld.
I suppose I need to bite the... -
28th Sep 2009, 09:39 PM
Thread: Generator for Arc Welder help
by echnidna- Replies
- 6
- Views
- 10,740
ditto
ditto
-
28th Sep 2009, 01:02 PM
Thread: Contact Welding Rods
by echnidna- Replies
- 8
- Views
- 8,086
When I first started welding 47 years ago with my...
When I first started welding 47 years ago with my homemade welder I got a packet of Lincoln "Self Weld" rods. They were great , just lay them on the weld line at an angle and they'd strike and run a...
-
28th Sep 2009, 10:10 AM
Thread: Contact Welding Rods
by echnidna- Replies
- 8
- Views
- 8,086
Hi Grahame, I found this link for a Spot Welding...
Hi Grahame,
I found this link for a Spot Welding Gun Plan
it runs off an arc welder and is similar to the spot weld guns on ebay (international).
... -
26th Sep 2009, 10:34 PM
Thread: Contact Welding Rods
by echnidna- Replies
- 8
- Views
- 8,086
Contact Welding Rods
Hi,
Does anyone know if Contact Welding Rods are available in oz? -
19th Sep 2009, 07:45 PM
Thread: TIG welding helmets
by echnidna- Replies
- 91
- Views
- 54,857
try some new batteries
try some new batteries
-
10th Sep 2009, 09:26 AM
Thread: Is it possible to ignore forums?
by echnidna- Replies
- 27
- Views
- 12,669
It'd be more fun & possibly very entertaining for...
It'd be more fun & possibly very entertaining for the rest of us if WW had to read the penturners posts before he could look at the other forums. :p
-
1st Sep 2009, 04:52 PM
Thread: freehand turning??
by echnidna- Replies
- 19
- Views
- 13,725
I've made shaped stuff on metal lathes by filing...
I've made shaped stuff on metal lathes by filing across the spinning metal.
-
10th Aug 2009, 10:06 PM
Thread: 6 stud toyota stub axles for trailer
by echnidna- Replies
- 35
- Views
- 29,958
Well if I want advice about trailers I'll ask...
Well if I want advice about trailers I'll ask Yonnee coz he is a professional trailer builder.
Why on earth would I want to consult a hi-fi man about building a trailer?
btw if soundman has a... -
30th Jul 2009, 11:10 PM
Thread: Standard stabila/lufkin level
by echnidna- Replies
- 7
- Views
- 6,897
The large aluminium companies (Alcoa etc) will...
The large aluminium companies (Alcoa etc) will extrude the exact profile you want, given their minimum quantities.
They may have changed but it used to be that the larger the volume you bought... -
30th Jul 2009, 09:22 PM
Thread: Joint Effort
by echnidna- Replies
- 11
- Views
- 5,850
what about a model lucas sawmill
what about a model lucas sawmill
-
28th Jul 2009, 12:04 AM
Thread: One little big job
by echnidna- Replies
- 59
- Views
- 31,445
You need to get this right first time. As it's on...
You need to get this right first time. As it's on an existing building hire a Boilermaker to do the job and avoid many hassles.
-
27th Jul 2009, 01:09 PM
Thread: Safety tip
by echnidna- Replies
- 2
- Views
- 3,673
nasty
nasty
-
25th Jul 2009, 08:31 PM
Thread: Brazing aluminium to metal
by echnidna- Replies
- 11
- Views
- 7,657
Nuts & Bolts
Nuts & Bolts
-
24th Jul 2009, 12:05 AM
Thread: 6 stud toyota stub axles for trailer
by echnidna- Replies
- 35
- Views
- 29,958
can you explin that soundman?
can you explin that soundman?
-
18th Jul 2009, 11:05 AM
- Replies
- 3
- Views
- 5,532
I have knocked them into thickwall tube...
I have knocked them into thickwall tube successfully,
You may need to file them down a bit if the tube is very thick -
The ball out of a tierod end would be easy to...
The ball out of a tierod end would be easy to work with
-
1st Jul 2009, 06:06 PM
Thread: Need to make large holes in steel
by echnidna- Replies
- 30
- Views
- 16,373
Cheap holesaws are useless on steel, you need a...
Cheap holesaws are useless on steel, you need a hss blade
-
1st Jul 2009, 10:54 AM
Thread: Need to make large holes in steel
by echnidna- Replies
- 30
- Views
- 16,373
That's what I do now, one day I'll get a metal...
That's what I do now, one day I'll get a metal cutting holesaw.
p.s. big drill bits in a normal 16mm drill press are a pita -
24th Jun 2009, 09:42 PM
Thread: The Charcoal Foundry
by echnidna- Replies
- 63
- Views
- 40,320
have cast ally many years ago My forge was a...
have cast ally many years ago
My forge was a 13"' holden whhel on the ground and loose sand packed around the perimeter. I used the blower side of an old vac cleaner for the air.
Despite... -
22nd Jun 2009, 10:59 PM
Thread: Worn thread on a saw spindle
by echnidna- Replies
- 21
- Views
- 12,702
I'd be inclined to run a thread file over the...
I'd be inclined to run a thread file over the start of the damaged thread then run a die nut along the whole lot.
-
4th Jun 2009, 11:36 PM
Thread: Trailer Build... mission possible
by echnidna- Replies
- 22
- Views
- 16,573
2 wheeler or tandem?
2 wheeler or tandem?
-
4th Jun 2009, 11:21 PM
Thread: Trailer Build... mission possible
by echnidna- Replies
- 22
- Views
- 16,573
have a look at big boat trailers
have a look at big boat trailers
-
28th May 2009, 10:46 AM
Thread: Cutting Aluminium Plate
by echnidna- Replies
- 12
- Views
- 6,802
I've cut a lot of ally on my bench saw, there is...
I've cut a lot of ally on my bench saw, there is no way I'd try cutting 35mm thick ally on it.
Use a bandsaw - that's the safe way. -
23rd May 2009, 06:34 PM
Thread: Library opening, when?
by echnidna- Replies
- 4
- Views
- 4,412
Have a feeling there was an unforseen health...
Have a feeling there was an unforseen health problem cropped up.
-
22nd May 2009, 09:41 PM
- Replies
- 2
- Views
- 6,601
shouldn't be any problems but unplug the saw
shouldn't be any problems but unplug the saw
-
21st May 2009, 09:23 PM
Thread: Measuring flatness of plate
by echnidna- Replies
- 9
- Views
- 8,086
You can align a saw table very accurately without...
You can align a saw table very accurately without messing around making a plate
-
18th May 2009, 11:10 AM
Thread: Painting black metal
by echnidna- Replies
- 21
- Views
- 14,702
no
no
-
18th May 2009, 09:35 AM
- Replies
- 26
- Views
- 15,083
If I wanted to sell something I would list it...
If I wanted to sell something I would list it here and on ebay, so that the interested parties determine the final purchaser and price.
-
7th May 2009, 03:19 PM
Thread: Welding strength?
by echnidna- Replies
- 64
- Views
- 38,470
ncrease the current or use a smaller rod.
ncrease the current or use a smaller rod.
-
6th May 2009, 10:45 PM
Thread: Bandsaw or Power Hacksaw
by echnidna- Replies
- 9
- Views
- 7,220
I'd love to use steel straight off the saw but a...
I'd love to use steel straight off the saw but a rub on the linisher isn't hard work
-
6th May 2009, 06:48 PM
Thread: Bandsaw or Power Hacksaw
by echnidna- Replies
- 9
- Views
- 7,220
Bandsaw or Power Hacksaw
I don't do much metalwork but I'd like a band saw or Power Hacksaw.
I feel the band saw might be a better tool finish wise but power hacksaws are cheaper at times on ebay.
And there is the... -
3rd May 2009, 01:19 PM
Thread: Free Metal and Wood Work Plans For Tools
by echnidna- Replies
- 0
- Views
- 3,572
Free Metal and Wood Work Plans For Tools
http://www.sawmill.ausmade.com.au/building.html
-
3rd May 2009, 01:17 PM
Thread: home Made Power Hacksaw
by echnidna- Replies
- 25
- Views
- 31,590
Follow this link for 3 different sets of plans...
Follow this link for 3 different sets of plans for power hacksaws.
http://www.sawmill.ausmade.com.au/building.html
There are some other free metal (and wood) working plans on the same webpage -
28th Apr 2009, 03:59 PM
Thread: Including audio files in posts.
by echnidna- Replies
- 3
- Views
- 4,351
if you do put audio in Neil, please make it so...
if you do put audio in Neil, please make it so those of us who don't want it can turn it off.
-
26th Apr 2009, 04:09 PM
Thread: Metal Working For Woodworkers
by echnidna- Replies
- 0
- Views
- 4,635
Metal Working For Woodworkers
I just uploaded these pdf's onto my website for free download
Marking Metal
Hand Tapping Machine
Electric Hacksaw
Better Metal Drilling
How To Cut Sheetmetal
How To Use Metal Punches
Swing... -
25th Apr 2009, 08:57 PM
Thread: Bitza has bitz the dust
by echnidna- Replies
- 6
- Views
- 7,406
Best wishes Derek, hope it all works out well.
Best wishes Derek, hope it all works out well.
-
24th Apr 2009, 05:01 PM
Thread: What size angle grinder ??
by echnidna- Replies
- 24
- Views
- 21,996
Thanks Bob I just found a good use for my old...
Thanks Bob I just found a good use for my old table saw :)
I might forget about getting a horizontal bandsaw -
23rd Apr 2009, 08:42 AM
Thread: Knife shaping
by echnidna- Replies
- 7
- Views
- 5,721
Reckon a 100mm angle grinder with a 1mm(app)...
Reckon a 100mm angle grinder with a 1mm(app) thick Inox (stainless steel) cutting disk would do it. With these discs you can cut to the edge of a pencil line just like cutting a bit of timber with a...
-
15th Apr 2009, 09:34 PM
Thread: What happened to my post?
by echnidna- Replies
- 28
- Views
- 12,787
Sounds like its been nicked to hang a gate on :D
Sounds like its been nicked to hang a gate on :D
-
12th Apr 2009, 01:11 PM
Thread: What happened to my post?
by echnidna- Replies
- 28
- Views
- 12,787
Are you in the habit of losing things John? :D
Are you in the habit of losing things John? :D
-
9th Apr 2009, 08:34 PM
Thread: New forum ideas
by echnidna- Replies
- 4
- Views
- 3,918
There have been so mamy different woodie things...
There have been so mamy different woodie things discussed over the years that most info is already here. Maybe we need a newby/novice woodies section
-
8th Apr 2009, 10:17 PM
Thread: New forum ideas
by echnidna- Replies
- 4
- Views
- 3,918
Theres a nothing to do with woodwork forum already
Theres a nothing to do with woodwork forum already
-
7th Apr 2009, 09:41 PM
Thread: Tool Steel
by echnidna- Replies
- 5
- Views
- 5,796
I think silver steel is a type of tool steel
I think silver steel is a type of tool steel
-
6th Apr 2009, 07:47 PM
Thread: Photo posting whinge.
by echnidna- Replies
- 31
- Views
- 21,681
Not everyone has or can get fast internet. ...
Not everyone has or can get fast internet.
Last time I looked nearly 30% of people were still stuck on dialup -
28th Mar 2009, 09:35 PM
Thread: sashless sliding windows
by echnidna- Replies
- 5
- Views
- 6,535
An alternative is rollup crystal clear plastic...
An alternative is rollup crystal clear plastic blinds. (bunnies sell some)
-
22nd Mar 2009, 07:28 AM
Thread: Brass on Brass
by echnidna- Replies
- 10
- Views
- 5,392
Teflon or hdpe or a metal like steel, stainless,...
Teflon or hdpe or a metal like steel, stainless, cast iron etc.
-
21st Mar 2009, 06:26 PM
Thread: Brass on Brass
by echnidna- Replies
- 10
- Views
- 5,392
brass doesn't like rubbing against brass,
brass doesn't like rubbing against brass,
-
20th Mar 2009, 10:32 AM
Thread: I'm Taking the Plunge
by echnidna- Replies
- 9
- Views
- 5,560
So FC, now you can make all your own machines &...
So FC, now you can make all your own machines & tools.
Start with CNC and see where that takes you. -
19th Mar 2009, 03:17 PM
Thread: Quench metal by oxygen torch
by echnidna- Replies
- 17
- Views
- 11,061
You shouldn't need to harden an axle that size