Search:

Type: Posts; User: mattm82

Page 1 of 2 1 2

Search: Search took 0.00 seconds.

  1. Replies
    3
    Views
    2,353

    Eclipse 244 and/or 245 tapping wrench

    Hi all, as above I’m keen to get a hold of the 244 and 245 Eclipse tapping wrench.

    I don’t really need them but I just really want them.

    Cheers,

    Matt
  2. Replies
    30
    Views
    6,455

    Thanks Tony, I’ve since deleted a bunch of older...

    Thanks Tony, I’ve since deleted a bunch of older messages.
    Cheers
  3. Replies
    30
    Views
    6,455

    Hi Steve, The M8 course and both M10’s are gone....

    Hi Steve,
    The M8 course and both M10’s are gone. Happy to discuss the remainder if you’re interested.
  4. Replies
    30
    Views
    6,455

    Hi Steve, just waiting to here back from...

    Hi Steve, just waiting to here back from Silversprings. He’s interested in 3. If he doesn’t take them you’re next in line and I’m sure we can work something out.
    Cheers
  5. Replies
    30
    Views
    6,455

    Gents, I have the following complete, boxed...

    Gents,

    I have the following complete, boxed Sutton in excellent condition

    M8x1.25
    M10x1.0
    M10x1.5
    M12x1.75

    5/16x22 in good condition but no box AH England brand?
  6. Replies
    30
    Views
    6,455

    Hi Tony, another member has also asked for...

    Hi Tony, another member has also asked for details so I’ll add them to this thread this afternoon so you can also see what’s available.

    Cheers
  7. Replies
    30
    Views
    6,455

    Can’t help with the die head gents, but have a...

    Can’t help with the die head gents, but have a number of complete chaser sets I’d be willing to part with if there is any interest. All Sutton brand. Happy to provide further details if anyone is...
  8. Replies
    38
    Views
    22,953

    Any chance you’ve still got the Toyo drill? I’d...

    Any chance you’ve still got the Toyo drill? I’d love to see a picture, I have a Toyo lathe that is an awesome piece of equipment!
    Cheers
    Matt
  9. Replies
    6
    Views
    5,847

    Hi Gavin, Heading over to SA for Christmas, if...

    Hi Gavin,

    Heading over to SA for Christmas, if this hasn’t sold by then I’ll take it.
    Cheers
  10. Replies
    23
    Views
    5,895

    Unless you’re planning to harden the 4140 I would...

    Unless you’re planning to harden the 4140 I would use mild. Cheaper, and will do the same job as unhardened 4140.
  11. Replies
    23
    Views
    5,895

    But the same place will happily sell you a bulb...

    But the same place will happily sell you a bulb specific to the light you just bought. I haven’t found a single Australian supplier selling a hold down specific to the vice.
  12. Replies
    23
    Views
    5,895

    It’s a fair point, guess I’m just surprised....

    It’s a fair point, guess I’m just surprised. Looks like I’ll be making some. I should be pleased for a new project but I had plans that now need to go on hold until I do.
    The only square stock I...
  13. Replies
    23
    Views
    5,895

    Thanks for the info. I’m sure I can work from the...

    Thanks for the info. I’m sure I can work from the pic you provided if I go that way.

    Cheers

    Matt
  14. Replies
    23
    Views
    5,895

    Thanks Dave, Figured I cast a wide net and see...

    Thanks Dave,

    Figured I cast a wide net and see what I catch!

    I have the tools to make some hold downs, it just seems bizarre they don’t come with some. Even if they just had a pilot hole that...
  15. Replies
    23
    Views
    5,895

    I can do that, just don’t really want to. Seems...

    I can do that, just don’t really want to. Seems crazy that such a common item doesn’t have holddowns available, despite being made to be used in conjunction with them! Live and learn...
  16. Replies
    23
    Views
    5,895

    Where to get toolmaker vice holddowns?

    I bought a toolmaker vice from Hare and Forbes... had a voucher, wanted one! I stupidly assumed a vice would come with hold downs, but it has not. Now looking it seems they're not a straight forward...
  17. Replies
    10
    Views
    5,150

    Hi Aaron, You’re correct. I have both of those....

    Hi Aaron, You’re correct. I have both of those. Appreciate the thought however. Hope you didn’t invest too much time.
    Cheers
  18. Replies
    24
    Views
    5,793

    The same site I linked you too sells belts for...

    The same site I linked you too sells belts for linishers in a variety of sizes, and a variety of specific uses. Ceramic belts are the business when it comes to steel.

    Keep in mind the smaller...
  19. Replies
    24
    Views
    5,793

    What is your planned use for it mate? That may...

    What is your planned use for it mate? That may play a big part in what type of machine you use.
    I use belt linishers every day for work so happy to help out if I can
  20. Replies
    5
    Views
    3,719

    Build a frame from heavy angle iron that the blue...

    Build a frame from heavy angle iron that the blue base can fit snuggly into. Add some lockable wheels and you’re done
  21. That’s an excellent point, but I love my Waldowns...

    That’s an excellent point, but I love my Waldowns for their rigidity, accuracy and ease of refurbishment.
    Fitting a 3 phase motor and a VFD works really well on these machines and that will solve...
  22. Replies
    24
    Views
    5,793

    Just go here. Not cheap but absolute work horses....

    Just go here. Not cheap but absolute work horses.
    ...
  23. Replies
    10
    Views
    5,150

    I don’t, as I said, just got the mill with the...

    I don’t, as I said, just got the mill with the Clarkson Autolock and I mostly use 2-3mm end mills. I was hoping to find some collets.

    I have since spoken to Ueee and confirmed the smaller sizes...
  24. Replies
    10
    Views
    5,150

    Not 100% but I think it’s a small. Just bought a...

    Not 100% but I think it’s a small. Just bought a mill they came with one, lots of collets, lots of end mills, just no collets that small
  25. Replies
    10
    Views
    5,150

    I haven’t seen any but I’ve read they exist. Yet...

    I haven’t seen any but I’ve read they exist. Yet to find out but I’m hoping!
  26. Replies
    10
    Views
    5,150

    Chasing Clarkson Autolock collets

    Hi all, I’m after 2 and 3mm collets for an Clarkson Autolock. I use 3mm endmills the most, closely followed by 2mm.
    Any help greatly appreciated.
  27. Replies
    3
    Views
    4,875

    For anyone that is on the fence there has been a...

    For anyone that is on the fence there has been a great response and the order is going to be placed this week. Let me know ASAP, or check out the FB thread, if you want some.
  28. Replies
    3
    Views
    4,875

    A full set of machine files in one grit is...

    A full set of machine files in one grit is $246.31 USD plus some shipping. They are available in 80, 120 and 180g.

    Individually the files range from $22 to $65 USD.

    The diamond wires are $15USD...
  29. Replies
    3
    Views
    4,875

    Diamond Machine files for Die filers

    I am in the process of having a some diamond coated machine files for Die filers brought in.

    The company is
    MF Files & Handles

    If this is of interest to you please PM me or go to the FB group...
  30. Thread: Just a box

    by mattm82
    Replies
    2
    Views
    5,908

    That is a beautiful piece of work and very nicely...

    That is a beautiful piece of work and very nicely done. Great job
  31. Thread: Deckel KF 12

    by mattm82
    Replies
    4
    Views
    5,424

    PM sent

    PM sent
  32. Thread: Knife handles

    by mattm82
    Replies
    10
    Views
    34,300

    As a full time maker best answer I can give is,...

    As a full time maker best answer I can give is, it depends on the knife.
    Stabilizing has opened up a huge variety of timbers that were previously ignored due to durability or stability.
    I usually...
  33. Replies
    4
    Views
    3,567

    Thanks for the link. I did see it but the price...

    Thanks for the link. I did see it but the price was pretty up there!
  34. Replies
    4
    Views
    3,567

    File machine is what I’m after.

    File machine is what I’m after.
  35. Replies
    4
    Views
    3,567

    Wanting a Die Filer

    As above, keen to lay my hands on a working die filer. I’m in ACT but can travel/arrange freight for the right machine.

    Cheers,

    Matt
  36. Replies
    12
    Views
    3,477

    Ray, Thank you for your reply. I do have the...

    Ray,

    Thank you for your reply. I do have the higher speed machine, so I’ll have to look at your your calculations, along with how it matches up to my machine.

    I have a single phase model and...
  37. Replies
    12
    Views
    3,477

    Sure can

    Sure can
  38. Replies
    12
    Views
    3,477

    Greatly appreciated Ray, Thank you.

    Greatly appreciated Ray,

    Thank you.
  39. Translated perfectly and it makes total sense. A...

    Translated perfectly and it makes total sense. A good piece of info for when I get around to having a go, thank you
  40. Thread: Hammer Time

    by mattm82
    Replies
    25
    Views
    31,849

    More beautiful work! My old man has just done a...

    More beautiful work! My old man has just done a hand engraving course and has asked for some hammers to add to the one he already has. You’ve set the benchmark!!
  41. That is some lovely smithing, very accurate!! I’m...

    That is some lovely smithing, very accurate!! I’m impressed. I’ve been wanting to try some of these techniques for a while but there is never enough time for play when I have knife orders to work on!...
  42. Replies
    2
    Views
    2,137

    I’ll take the 0-25 micrometer. Will need postage...

    I’ll take the 0-25 micrometer. Will need postage to Canberra please.
  43. Replies
    12
    Views
    3,477

    Greatly appreciated, thankyou. I’ll send him a PM...

    Greatly appreciated, thankyou. I’ll send him a PM now [emoji106]
  44. Replies
    9
    Views
    7,516

    0 - 25mm

    Fair enough, thanks for letting me know.

    Matt
  45. Replies
    12
    Views
    3,477

    Waldown NH

    Fair enough, I've never come across anyone with one! I'd love to find one to measure so I could fabricate one. I've had two NH drills and neither had a b set but both were labeled for them.

    Cheers
  46. Replies
    12
    Views
    3,477

    Wanted B pully for Waldown BH drill

    Please note:

    The following posts have been moved from METALWORK - Machinery, Equipment, MARKET thread Waldown NH and are from Post #8 on.....

    You don't happen to have a 'b' set pulley on your...
  47. Replies
    9
    Views
    7,516

    0-25mm micrometer

    If you can post I'll take the 0-25mm micrometer if still available.

    Cheers,

    Matt
  48. Replies
    20
    Views
    5,748

    Artisan supplies has a large variety of high...

    Artisan supplies has a large variety of high carbon/tool steels and postage is quite reasonable.
  49. Replies
    2
    Views
    1,478

    Thanks, I'll check them out. It is frustrating...

    Thanks, I'll check them out. It is frustrating trying to get anything a little uncommon in Aus!!


    Sent from my iPhone using Tapatalk
  50. Replies
    2
    Views
    1,478

    410 or 420 stainless tube or RHS supplier?

    Hi all,

    Trying to find a supplier of small quantities of 2-3" tube or similar size rhs in 410 or 420 stainless.

    I live in Australia and can't find it anywhere so I'm going to g to have to ship...
Results 1 to 50 of 54