Needs Pictures: 0
Results 31 to 32 of 32
Thread: Fume bluing two planes
-
7th September 2020, 07:49 PM #31.
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 27,790
Finally finished the bluing of all the home made steel parts.
FInished.jpg
O are the parts from the original 78 that my uncle left me in 1967.
B is the resurrected one from the bits in the plane parts box.
B1 - B4 are he home made parts.
Close up of the blued screws.
Only the most right hand has proper knurling.
The left hand side ones were (accidentally) done with different knurling tool.
Screws.jpg
This is the set my friend gets for his dad's 78
Brasset.jpg
and one more for fun.
Finisged2.jpeg
-
7th September 2020 07:49 PM # ADSGoogle Adsense Advertisement
- Join Date
- Always
- Location
- Advertising world
- Posts
- Many
-
14th September 2020, 02:23 PM #32.
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 27,790
I finally made a replacement lever cap screw from a dodgy bit of 16mm steel rod for the 78 I have been reconstructing out of "parts in a box"
9/32" 19 TPI, no die for this so cut the thread on the lathe.
First time I've used the Hercus to cut a thread and the last time I cut a thread would be 10+ years ago on the Nuttall at work.
I don't have a thread chaser for the Hercus so had to reverse the bit back and forth to keep the thread regsitration.
I wouldn't call it my best thread but it works and holds OK.
Capscrew.jpg
Here it is alongside the screw from my other rebate plane.
Capscrew2.jpg
Note my knurling is not as crisp as Anorak Bob's.
Similar Threads
-
Welding fume extraction
By MWF FEED in forum METALWORK FORUMReplies: 0Last Post: 29th June 2020, 01:50 PM -
Fume extraction
By Lappa in forum CNC MachinesReplies: 10Last Post: 21st September 2019, 12:32 PM -
Solder fume extraction.
By BobL in forum DUST EXTRACTIONReplies: 11Last Post: 18th August 2017, 10:41 PM -
Welding bay fume hood
By BobL in forum METALWORK FORUMReplies: 19Last Post: 4th June 2012, 11:58 AM -
Where to buy fume extractor fans?
By gvz in forum SAFETYReplies: 4Last Post: 17th October 2005, 11:00 PM