4 Attachment(s)
How to extend these axles
Hey guys more progress on the boat trailer finally got my spring hangers hung i dry test fit my velox deep dish disc hubs and they came up with no clearance
What is the best way to extend the axles? Its mostly untill i can buy the proper length axles which may be a few months however need to get the trailer as a roller for now
Have looked at shs 50x50x5mm sleeve but unsure if it will be enough strength
A guy on the boat forum where im building the trailer suggested a weld pad than machine it on the lathe as a sleeve
What would be the proper way? Need to extend it maybe 100mm