Thought the Smithy sub forum had been a bit quiet lately so thought I'd post a few images of some recent projects.
I have been making a few axes lately. two out of the three below are folded construction, forge welded, with steel bit inserted and again forge welded in. The third is from the solid bar/Model T ford axle.
These sizes mainly aimed at craft work/bowl or spoon carving type work or whatever.
small one, pictured left without the bit welded in yet; didn't fully grind as wanted the forged finish around the eye/poll. measures 4.5inches long x 2-1/4 edge
IMG_0303.jpg IMG_0305.jpg
Progress shots of the larger one, finished shot below
IMG_1621.jpg IMG_1625.jpg
model T axle punching the eye in the fly press, started this one a while ago but recently thought Id better finish it.
IMG_2376.jpgIMG_2405.jpg
Model T axle top 4-3/4 x 3-3/4 edge; larger one 5-3/4 x 3-1/2 edge
IMG_1671.jpg
Cheers
-
17th Oct 2022, 05:58 AM #2Senior Member
- Join Date
- Feb 2012
- Location
- Tamworth, NSW
- Posts
- 205
They look great. What is the plan for handles, do you make own or but handles and fit them?
-
18th Oct 2022, 07:05 PM #3Golden Member
- Join Date
- Oct 2001
- Location
- ACT
- Posts
- 667
Hi Danger Mouse,
Normally make my handles, depends on what size handle and timber i have,but possibly will make from ash or elm or maybe black locust.
Have made one now for the small axe out of some split blanks of spotted gum.
cheers
-
14th Mar 2023, 08:41 PM #4New Member
- Join Date
- Feb 2023
- Location
- Amsterdam
- Age
- 29
- Posts
- 5
It looks more than great. Do you have a picture of the completed project?
Similar Threads
-
Your latest project
By .RC. in forum METALWORK GENERALReplies: 3019Last Post: 9th Apr 2024, 12:57 PM -
latest aquisitions
By eskimo in forum METALWORK GENERALReplies: 14Last Post: 28th Sep 2013, 01:06 AM -
Latest Arno pic
By 4-6-4 in forum METALWORK GENERALReplies: 0Last Post: 11th Jun 2012, 11:43 PM -
Projects Blogs FAQ .. Projects Blogs FAQ .. It's deja-vu all over again
By Ron Dunn in forum FORUMS INFO, HELP, DISCUSSION & FEEDBACKReplies: 0Last Post: 24th May 2008, 10:18 AM