22nd Nov 2021, 08:04 PM #31
-
22nd Nov 2021, 08:28 PM #32Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
Not so sure. All the riv-nuts I've used have been in steel or Al. The two things that I have noticed are that the holes need to be pretty good diameter wise, and that those nuts really clinch up hard. I suspect that the clinching action would just push the wood out the way and it would be a sloppy fit. Could be wrong though.
Michael
-
22nd Nov 2021, 08:33 PM #33Most Valued Member
- Join Date
- Nov 2008
- Location
- North Brisbane. Qld. Australia
- Age
- 70
- Posts
- 1,514
These are different to nutserts or rivnuts. Designed for plastic apparently. They just get pressed into a hole and the fastener expands them so they grip. See this link -
https://metalworkforums.com/redirect...%3DtQiamU5QUn0Nev.
-
22nd Nov 2021, 08:36 PM #34Most Valued Member
- Join Date
- Nov 2008
- Location
- North Brisbane. Qld. Australia
- Age
- 70
- Posts
- 1,514
I'd love that little press they have in that video.
Nev.
-
23rd Nov 2021, 12:30 AM #35
Hi Nev, Guys,
Yes those are nice in plastics, and would probably work in hardwood’s. The others are similar but are intended to put a thread into relatively thin and soft materials, like alloy and mild steel sheet. There are two forms, one has a thin hexagonal flange on the top and a splined serrated body. The other just cuts a spline into the metal as its pressed in place, it also pulls out quite easily, usually when you don't want it to !
If you have the room underneath I prefer the pop rivet type where the part above the thread bulges out locking it in place.
EDIT: Just to add that TR Fastenings will send you samples if you ask them.Best Regards:
Baron J.
-
24th Nov 2021, 08:52 AM #36Member
- Join Date
- May 2012
- Location
- Dandenong
- Posts
- 76
Rivnuts are fantastic! I go nuts using them wherever they'e useful, which is pretty much everywhere! Amazing sheer strength, easy to fix, just can't be beat for convenience and ease. And way stronger than most rivets as the bolt screwed into applies holding force keeping it rigid.
This trolley/stand for my ~500kg fly press was put together with rivnuts of varying sizes. That's a ~18mm thick steel sheet on top rivnutted on. Solid as a rock with the fly press in use on top!
stand 02.jpg
-
24th Nov 2021, 11:11 AM #37Most Valued Member
- Join Date
- Mar 2011
- Location
- Southern Flinders Ranges
- Posts
- 1,555
Rivnuts/Nutserts will not work in timber, screw threaded inserts or T nuts depending on application are the go to for timber.
-
24th Nov 2021, 02:52 PM #38Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
-
24th Nov 2021, 11:39 PM #39Senior Member
- Join Date
- May 2019
- Location
- Picnic Point, Sydney
- Age
- 77
- Posts
- 314
I bought a hand tool and hundreds of different size nutserts from Avdel about 40 years ago and unlike what I see offered today they are flush fitting. Todays Rivnuts all seem to have a flange which sometimes isn't desirable and was wondering if anyone makes a flush fit option as my stock has dwindled?
-
25th Nov 2021, 09:05 AM #40Most Valued Member
- Join Date
- Mar 2011
- Location
- Southern Flinders Ranges
- Posts
- 1,555
You’re looking for the thin sheet series.
United fasteners keep them
https://www.unitedfasteners.com.au/p...s#product-list
-
25th Nov 2021, 05:15 PM #41Golden Member
- Join Date
- Apr 2009
- Location
- Kingswood
- Posts
- 930
Got a nutsert/rivnut kit off a local friend - no name and no instructions.
It contains a selection of inserts, the set tool, and appropriate set arbors.
Keen to give one a go tomorrow.
But, the reference to countersunk head nutserts got me thinking that that would be a superior solution.
Checked ebay, but no joy there.
Then checked Bolt and Nut Australia - loads of listings of all sizes in all materials for countersunk nutserts.
They have a walk-in 10 minutes drive from me, so tomorrow morning .....
Two warnings from friends:
- don't overdo the pressure, you can break the arbor,
- don't underdo the pressure, the insert can turn in the hole.
The borrowed tool has a travel limit adjuster, how does one set the adjuster ?
Will keep you posted on developments.
Keep well,
John.
-
25th Nov 2021, 06:19 PM #42Most Valued Member
- Join Date
- Mar 2011
- Location
- Southern Flinders Ranges
- Posts
- 1,555
Get a couple of extras to practice with and allow you to set the stop.
Basically you want to set the stop to pull the tool up on full disruption of the fastener, not a big if it’s not correct on the flange head ones but somewhat important for the thin sheet ones because they will pull through. Also very important with the thin sheet fasteners to get the hole size spot on. I bought the correct size drills for the ones I’ve used regularly and leave them in the case with the tool.
Check the nose pieces of your tool against the pictures on the Avdel website, if the noses don’t have the radius in them like the Avdel ones it will be an exercise in frustration trying to get them to work on the thin sheet inserts. The radius forces the top edge of the fastener beyond the limits of the hole while it’s being set, without it the fastener pulls through. Some of the cheaper tools don’t have it, they’ll set flanged inserts ok but not thin sheet.
-
25th Nov 2021, 09:08 PM #43
Just in case this isn't well-known: I discovered you can get rivnuts which are closed on the 'far' side. I used these to mount the solar panels on the roof of our camper. I didn't like the idea of through-holes in the roof....
Cheers, Joe
retired - less energy, more time to contemplate projects and more shed time....
-
25th Nov 2021, 10:27 PM #44Member
- Join Date
- May 2012
- Location
- Dandenong
- Posts
- 76
It's a pretty big beastie! The guy I bought it from said it was around 500kgs (might be less though), and it seems to be roughly similar to at least a size 10.
That's why I dramatically over engineered the base with close to a couple hundred rivnuts (including some beefy 20mm dia x 38mm long ones) to really keep things rigid.
-
25th Nov 2021, 11:54 PM #45Most Valued Member
- Join Date
- Mar 2011
- Location
- Southern Flinders Ranges
- Posts
- 1,555
I’m curious, do the inserts in the cabinet have any bolts in them? There are none in the photos, kind of looks like you’ve use them to rivet the panels together.
Similar Threads
-
Rivnuts?
By wm460 in forum METALWORK GENERALReplies: 18Last Post: 14th May 2017, 08:16 PM -
Need a 300mm caliper or similar
By Michael G in forum WANTED TO BUYReplies: 0Last Post: 24th Jan 2016, 07:49 PM -
any one know which lathe this is ? look similar to the Lorch
By thorens in forum METALWORK GENERALReplies: 11Last Post: 27th Oct 2013, 08:44 AM -
Lathes similar to AL320G
By 19brendan81 in forum METALWORK GENERALReplies: 18Last Post: 25th Nov 2011, 08:25 PM -
9x20 and similar lathes
By Big Shed in forum METALWORK GENERALReplies: 1Last Post: 8th Sep 2011, 09:45 AM