    Default milling aluminium with woodwork router bits

    I want to make a couple of hawse fairleads, like this
    https://www.amazon.com/WARN-94244-Ha.../dp/B018AIHO5W

    Planning on casting in aluminium. I've been looking at corner-rounding endmills and the price for one with around 1" radius is way over the top. I'm wondering if it is worth trying a woodwork rounding-over bit like this
    https://www.ebay.com.au/itm/264169233241?
    and what are the pitfalls of doing so?

  2. #2
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    BIL is an Al boilermaker on shipbuilding duties at Naval base here in WA. His toolkit includes a bunch of ww tools including hand held WW circulars,, jigsaws, and routers. He regularly slightly over fills TIG & MIG welds and rounds over with round over router bits. He welds lots of curved surfaces and by the time he’s finished they look seamless.

  3. #3
    Join Date
    Jun 2007
    Location
    Vic
    Age
    48
    Posts
    544

    Default

    I used the wood router to cut this dovetail. It worked with mild steel and aluminium is softer.

    20160721_230016.jpg

  4. #4
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Wax or meths can be used as a lube for Al.

  5. #5
    Join Date
    Mar 2011
    Location
    Southern Flinders Ranges
    Posts
    1,555

    Default

    The V groove in these was cut with a router bit
    Attached Images Attached Images

  6. #6
    Join Date
    Apr 2018
    Location
    Drouin Vic
    Posts
    634

    Default

    Well that's very good to know, I'll have to get a suitable rounding-over bit and give it a try. Around one-tenth of the price for a router bit as for a milling cutter. Might be a bit of a challenge for a collet to hold onto a cutter with a 3" o.d. and a 1/2" shank, I guess I'll just take it gently.

  7. #7
    Join Date
    Mar 2011
    Location
    Southern Flinders Ranges
    Posts
    1,555

    Default

    Cast ally is easier to route than some hardwood.
    Having said that, I’d consider machining them over casting them if you want them to last.

  8. #8
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,480

    Default

    Quote Originally Posted by Pete O View Post
    Well that's very good to know, I'll have to get a suitable rounding-over bit and give it a try. Around one-tenth of the price for a router bit as for a milling cutter. Might be a bit of a challenge for a collet to hold onto a cutter with a 3" o.d. and a 1/2" shank, I guess I'll just take it gently.
    Hi Pete, Guys,

    3 inch diameter is a very big and expensive cutter even for a router toolbit ! I very much doubt that you will need one that big. If you are doing the ends in one operation, I would go for a form tool in the lathe and use a four jaw to hold the work.
    Best Regards:
    Baron J.

  9. #9
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Quote Originally Posted by Pete O View Post
    Well that's very good to know, I'll have to get a suitable rounding-over bit and give it a try. Around one-tenth of the price for a router bit as for a milling cutter. Might be a bit of a challenge for a collet to hold onto a cutter with a 3" o.d. and a 1/2" shank, I guess I'll just take it gently.
    The largest round-over bit I have seen BIL use is a 25mm OD cutter.

  10. #10
    Join Date
    Mar 2011
    Location
    Southern Flinders Ranges
    Posts
    1,555

    Default

    The inside radius where the rope comes out only needs to be around 10ish mm.
    Out side radius for aesthetics can be whatever you want, I commonly use an R3 for stuff like that.
    Both are significantly smaller than 3"

  11. #11
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    Quote Originally Posted by Pete O View Post
    I'm wondering if it is worth trying a woodwork rounding-over bit like this
    https://www.ebay.com.au/itm/264169233241?
    Pete,
    that bit has an 8mm radius. I think this is the one you want (maybe): https://unitedtoolsmckinnon.com.au/p...ver-router-bit
    Chris

  12. #12
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,561

    Default

    Quote Originally Posted by Pete O View Post
    ...Planning on casting in aluminium...
    To ask the obvious, why? Unless you are planning on making lots of them by the time you have made a pattern, well, you have already made one. What's one or two extra...

    Quote Originally Posted by Pete O View Post
    I'm wondering if it is worth trying a woodwork rounding-over bit ...and what are the pitfalls of doing so?
    Carbide wood bits work fine on Al. The bigger the radius, the slower the rpm though. As others have suggested, for cosmetics any radius will do so chose something manageable.

    Michael

  13. #13
    Join Date
    Aug 2008
    Location
    Melbourne
    Age
    34
    Posts
    1,080

    Default

    Quote Originally Posted by Pete O View Post
    Well that's very good to know, I'll have to get a suitable rounding-over bit and give it a try. Around one-tenth of the price for a router bit as for a milling cutter. Might be a bit of a challenge for a collet to hold onto a cutter with a 3" o.d. and a 1/2" shank, I guess I'll just take it gently.
    No problem holding it, I've run plenty of 2.5" diameter bits in wood, both by hand and in a CNC, and they don't go anywhere. Just go easy on the feed, use lube as mentioned above and don't try to cut too deep in one pass; once you start approaching full profile, I'd be doing no more than 1mm depth per pass

  14. #14
    Join Date
    Apr 2018
    Location
    Drouin Vic
    Posts
    634

    Default

    Quote Originally Posted by BaronJ View Post
    Hi Pete, Guys,

    3 inch diameter is a very big and expensive cutter even for a router toolbit ! I very much doubt that you will need one that big. If you are doing the ends in one operation, I would go for a form tool in the lathe and use a four jaw to hold the work.

    A router cutter with a radius of about 3/4" appears to have an outside diameter somewhere in the vicinity of 3 inches, just from looking at photos at present (edit- I was guesstimating based on 1/2" shank but the one I was looking at is probably 1/4" shank. So much smaller OD than I thought.)...I'm talking here about milling the inside of the slot to give a radius for the rope to run on, not the outside of the body of the thing. which I think is what you mean in the suggestion above about using the lathe? I can't see any way to machine the inside of the slot in a lathe rather than a mill.

    I'm actually going a bit cold on the casting idea, I was originally thinking of casting them with lettering or some other design but I've decided that's a waste of time so I'm now thinking just mill them from a billet. The better quality bought ones appear to be about 1.5" thick with a 3/4" radius on both the back and front inside the slot for the rope to run over. So I'm looking at a router bit with about that radius.

    Another thought- if I'm going to mill them from stock, what about steel stock? I know with this sort of thing, the harder the material the better, as it is damaged surfaces that damage the rope. I have some leftover offcuts of forklift tine (almost certainly 4140) in ideal dimensions; would I have any hope of radiusing that with a router bit?

  15. #15
    Join Date
    Aug 2008
    Location
    Melbourne
    Age
    34
    Posts
    1,080

    Default

    Quote Originally Posted by Pete O View Post
    I have some leftover offcuts of forklift tine (almost certainly 4140) in ideal dimensions; would I have any hope of radiusing that with a router bit?
    The carbide grades used for woodworking tools are relatively brittle, I'm not so sure they would cope with something that tough. You might actually be better with HSS

Page 1 of 2 12 LastLast

Similar Threads

  1. Router Bits
    By bwal74 in forum METALWORK GENERAL
    Replies: 6
    Last Post: 18th Apr 2021, 10:42 PM
  2. Opinions on Sharpening Router Bits?
    By NGrimberg in forum CNC Forum
    Replies: 3
    Last Post: 16th Jul 2020, 09:25 AM
  3. Small HS Router Bits
    By electrosteam in forum CNC Forum
    Replies: 6
    Last Post: 23rd Nov 2017, 11:54 AM
  4. Router bits
    By phaser in forum METALWORK GENERAL
    Replies: 11
    Last Post: 1st Mar 2017, 11:14 PM
  5. router bits in lathe to mill aluminium - youtube video
    By steamingbill in forum METALWORK GENERAL
    Replies: 3
    Last Post: 29th Oct 2013, 06:55 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •