    Would you accept a proper nipple? That nut arrangement doesn't look too convincing.
    Just give a diameter, from the holes on the caliper.

  2. #32
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    18

    Default

    Quote Originally Posted by nadroj View Post
    Would you accept a proper nipple? That nut arrangement doesn't look too convincing.
    Just give a diameter, from the holes on the caliper.
    Yes, if this arrangement doesn't work. It's not soldered yet - I'm hoping that when it's flooded with silver solder the nut will be held firmly in place.

  3. #33
    Join Date
    Jun 2007
    Location
    Vic
    Age
    48
    Posts
    544

    Default

    Quote Originally Posted by nadroj View Post
    Would you accept a proper nipple? That nut arrangement doesn't look too convincing.
    Just give a diameter, from the holes on the caliper.
    Yes, just make the "nipple" out of stainless steel with a hole to fit though then TIG the end to the nipple.

    https://metalworkforums.com/f316/t20...-cable-cutting

  4. #34
    Join Date
    Oct 2004
    Location
    Southern Highlands NSW
    Posts
    1,898

    Default

    Quote Originally Posted by jackaroo View Post
    Yes, just make the "nipple" out of stainless steel with a hole to fit though then TIG the end to the nipple.
    That would be welding to the cable wire?
    I'd be concerned that the very high temperature could detrimentally change features of the wire metal.
    Mind you, I don't know a thing about working with stainless steel Bowden cable inners.

  5. #35
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    18

    Default

    Hi All,

    Another quick update. I took the cable to a jeweler on Friday. At first she seemed a bit perplexed by what I wanted, but after explaining it a bit more she said she'd have a go at soldering it. Should be done later this week so fingers crossed.

    Cheers!

  6. #36
    Join Date
    Oct 2020
    Location
    Greendale Vic. Australia
    Posts
    64

    Default

    Don't really understand what the fuss is about. For a century we've been using brass nipples, soft soldered to the cable.
    Excess heat will quite likely cause the cable to become brittle -just what you don't need at that point. The jeweller will no doubt use silver-solder, hopefully the lowest temp she has in stock. Just ensure the strands are spread out within the nipple countersink - that's what really provides the strength. (and maybe heatsink the cable too)

  7. #37
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    18

    Default

    Quote Originally Posted by joolstacho View Post
    Don't really understand what the fuss is about. For a century we've been using brass nipples, soft soldered to the cable.
    Excess heat will quite likely cause the cable to become brittle -just what you don't need at that point. The jeweller will no doubt use silver-solder, hopefully the lowest temp she has in stock. Just ensure the strands are spread out within the nipple countersink - that's what really provides the strength. (and maybe heatsink the cable too)
    What you're suggesting will be Plan B! The reason I went with Plan A was because (according to what I've read online) it will be difficult to solder to stainless steel.

  8. #38
    Join Date
    Jun 2007
    Location
    Vic
    Age
    48
    Posts
    544

    Default

    Quote Originally Posted by cpsmusic View Post
    What you're suggesting will be Plan B! The reason I went with Plan A was because (according to what I've read online) it will be difficult to solder to stainless steel.
    If it failed. PM me your address and more details .ie the cable length +diameter of the hole as in previous post...

Page 3 of 3 FirstFirst 123

Similar Threads

  1. Cable disc brakes routing of cable.
    By gros21 in forum TRAILERS & OTHER FABRICATED STUFF
    Replies: 3
    Last Post: 14th May 2017, 06:41 PM
  2. Bike trailer plans help
    By BLKWDW in forum TRAILERS & OTHER FABRICATED STUFF
    Replies: 8
    Last Post: 28th Dec 2013, 11:52 PM
  3. QUEENSLAND Bike trailer
    By neyund in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 0
    Last Post: 10th Apr 2013, 11:27 AM
  4. Making a Pan Brake "Folder with fingers" for home
    By simso in forum METALWORK GENERAL
    Replies: 147
    Last Post: 27th Mar 2012, 08:49 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •