27th Jun 2020, 01:15 PM #1Senior Member
- Join Date
- Nov 2012
- Location
- Mid North Coast NSW
- Posts
- 423
Triangles for machining
Just finished making these for milling setups. 45deg and 60/30deg.
I made them on the CNC from 1/4" perspex and they are both 100mm on the hypotenuse.
There's no way for me to check them for accuracy but they should be aweful close since they are mathematically produced.
If anyone is interested in having the G-code just let me know and I'll post it.
triangles.jpg
-
27th Jun 2020, 05:31 PM #2Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,672
Nice!
A reasonable way to check them would be to cut another two of the 30/60 and then you could put 30+60 and check for square.
Use the third one for 30 +30+30 to make sure you haven’t got 28 + 62 deg etc.
The 45deg one you should be able to just check against a second one.
Steve
-
27th Jun 2020, 09:06 PM #3Senior Member
- Join Date
- Nov 2012
- Location
- Mid North Coast NSW
- Posts
- 423
-
27th Jun 2020, 09:53 PM #4
Hi Phaser, Guys,
Making another one would be a test of how accurate your CNC is !Best Regards:
Baron J.
-
27th Jun 2020, 10:34 PM #5Senior Member
- Join Date
- Nov 2012
- Location
- Mid North Coast NSW
- Posts
- 423
-
28th Jun 2020, 11:12 AM #6Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,258
-
30th Jun 2020, 10:41 AM #7Senior Member
- Join Date
- Nov 2012
- Location
- Mid North Coast NSW
- Posts
- 423
Making these triangles has made me realize something that could be significant to some people.
If you have a lathe where the dials read direct, and you take a 10 thou cut, you will actually take 20 thou off the diameter of the part , right ?
With a 30/60 triangle the opposite side is exactly half the length of the hypotenuse.
So just swivel the compound to 30deg and whatever you set that dial to will come off the diameter.
I don't have any trouble remembering to double the figure but it can be confusing so this might useful to someone.
-
30th Jun 2020, 09:58 PM #8Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,080
Further tip similar to that, setting your compound to 3 degrees off horizontal will give you a (near enough to) 10:1 diameter ratio (1 thou on the compound = one tenth on diameter) if you need really fine control.
Similar Threads
-
HSS Machining
By Auskart in forum METALWORK GENERALReplies: 11Last Post: 28th Oct 2016, 09:10 AM -
Looking for someone in Melbourne to do some machining for me
By doug3030 in forum METALWORK GENERALReplies: 15Last Post: 16th Dec 2013, 10:40 AM -
SOLD: Machining book"tabletop machining"
By woodsurfer in forum METALWORK - Machinery, Equipment, MARKETReplies: 4Last Post: 7th Feb 2012, 06:52 PM -
machining stainless
By Gavin Newman in forum METALWORK GENERALReplies: 3Last Post: 17th Apr 2010, 01:12 PM -
Machining oil
By Bodgy in forum METALWORK GENERALReplies: 3Last Post: 23rd Apr 2008, 10:57 PM