I figured that with the arrival of a new machine, I shouldn't start yet another thread ill fail to update and instead keep all the progress or otherwise in here.
CVA Lathe - Pretty much finished with its solid compound but i dont think aluminium was a great choice it seems to have more harmonic issues than before, ill devise a more rigorous test before i go making it again.
DSG Lathe - Need to make a new fastlock backplate, I got drawings off a nice guy on PM so now i just have to spring for a 12" slug of 4140. Once a fresher chuck is mounted it'll need to make a couple of bushes for itself.
About two months ago some nice guys from Hella came over the road and asked if wanted to do a walk through before everything started being shut down. I am very sad to see such an advanced manufacturer going, especially when it was still profitable even without automotive. While there i asked if I could buy the Aciera F5 they had in the tool/maint room, they gave a fair price and i agreed.
Well after a lot of waiting it finally came over the road on their big forklift while i was away on holiday. It had been tagged out as broken in 2014 and not used since. It seems as though the X axis has a feed issue that i have yet to diagnose. the controls all seem free and i am yet to find any really egregious abuse. Due to space reasons ( I also got some other things like a set of rolls and a cold saw) My Bridgeport is going to have to be sold so PM me if interested.
If anyone here knows more about the smaller F mills powers feed i would be very keen to know more.
it didnt have any of the really fancy accessories but i did get its dividing head, geartrain, normal vertical head and a random rotary table. I was very concerned things would go missing as it had to sit there while all the greys purchases went out but all good.
IMG_20181108_101317.jpgIMG_20181108_101322.jpgIMG_20181108_101337.jpg
The quill only has a short 60mm of travel, and the handle being at the front pointed sideways is a bit odd, i also havent found any kind of stops or fine feed, the knob on the right seems to do nothing? I imagine something is broken in there
IMG_20181108_101352.jpg
The coolant sump and pump are at the bottom there, and thankfully have straight oil in them (its very gross but at least no corrosion)
IMG_20181108_101425.jpg
Phaser should like this, absolutely no labels on the controls at all. wooo
IMG_20181108_101401.jpgIMG_20181108_101404.jpg
I cant find a date or serial on the machine except the dro is dated 1976, cutting edge! I dont know if its factory (although all the mounting hardware is blackened so im guessing it is, also the machine has no gauge block or trav-a-dial mounts)
IMG_20181108_101418.jpg
Feed motor gearbox is in the foot with a tiny set of expanding pulleys like the main drive. that knob is feed speed adjustment, not exactly convenient, although you can turn rapids on at the side of the machine with a big handle.
IMG_20181108_113540.jpg
Part of the inbuilt arm to swing the vertical head away is missing, ill have to fabricate a new one. pretty heavy duty as the head only weighs 65kgs. I also cant find any lube points for the head so i think it has to be fully broken down to lubricate, wonder when that was last done? guessing I was in breeches still.
IMG_20181108_114905.jpg
Those lube lines in the apron are 1/8 OD, i sure bloody hope they aren't blocked!! They almost definitely will be though.
IMG_20181108_115535.jpg
Main drive setup, the expanding pulleys feel pretty good but the upper final drive sheaves are a bit worn.
And this it where im up to, trying to split away the x axis feeds clutch, im having huge trouble getting the two close fit dowels to budge, any tips on splitting flat cases like this without damage?
IMG_20181108_113516.jpgIMG_20181108_113521.jpg
In that photo you can also see the vee that provides location for the removable table, im sure in a dumpster somewhere its universal table is looking forlorn.
Thanks for reading
-
8th Nov 2018, 06:06 PM #2
Don't know about your machine, but congratulations on the buy.
Using Tapatalk
-
9th Nov 2018, 08:31 AM #3Senior Member
- Join Date
- Nov 2012
- Location
- Mid North Coast NSW
- Posts
- 423
Looks like a beauty
I found this : Aciera F5
-
10th Nov 2018, 11:54 AM #4Senior Member
- Join Date
- Nov 2012
- Location
- Mid North Coast NSW
- Posts
- 423
-
10th Nov 2018, 12:31 PM #5Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
That funny angled handle is actually the Y axis, the ram the vertical head is on is Y, the Z is in two places the front of the table and another handle about 20" down from that y handle beneath the table.
It's odd but the machine is laid out so you can operate it from the front or the right hand side. I'm not really sure why the RHS is a good idea, maybe to keep you away from the chips?
-
10th Nov 2018, 09:03 PM #6Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
I am a fool, I'm not missing a piece of the vertical head removal bracket, I just had to wind the Y axis back.
I also got into the X axis feed, I think something is bad down inside the apron as the feed rod won't make a full revolution and binds badly. I suspect the bevel gears that take drive from the base into the apron are missing some teeth.
Anyone got any good articles on making 90 degree bevels?
IMG_20181110_160524.jpg
IMG_20181110_160529.jpg
IMG_20181110_160507.jpg
I can't currently work out how to undo the horizontal drawbar, it's holding in a spindle protector and I don't think the vertical head has been off in many many years
-
10th Nov 2018, 09:11 PM #7Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,563
If it has not been off in many many years, it could be gummed up with old oil so stuck in place. Try a bit of penetrating oil and after that has had time to get in, treat it like you would any drawbar/ tool combination - loosen off a turn or two and a good wack with a (soft faced) hammer or mallet to break the adhesion.
The dual controls are probably because most of the time you will operate from the front, but sometimes there is better visibility of a job from the rear or the side, especially if you were using the horizontal spindle with a milling cutter mounted directly in it.
Michael
-
12th Nov 2018, 09:46 AM #8.
- Join Date
- Nov 2008
- Location
- Perth WA
- Age
- 71
- Posts
- 6,459
Ralph,
I imagine you have already visited David Samway's Anglo Swiss Tools site where he has a substantial collection of manuals and catalogues available for free download. There is no F5 literature but the F4 manual may provide suggestions as to how Aciera addressed things - https://drive.google.com/file/d/0B_D...BXakNGZ2c/edit
Another possible source of information is the Yahoo group Aciera - Old Swiss Machine Tools for Metalwork - https://groups.yahoo.com/neo/groups/Aciera/info
Bob.
-
13th Nov 2018, 10:09 AM #9Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
Thanks for that Bob, I had read that f4 manual and it was very helpful, also I had not found the yahoo group so I'll dig though that now. Thanks again!
Got the table off today, just the rest of the apron to go. Had to Garry a chain fall to the roof beam as I couldn't get the forklift in.
IMG_20181112_115142.jpg
-
13th Nov 2018, 10:32 AM #10.
- Join Date
- Nov 2008
- Location
- Perth WA
- Age
- 71
- Posts
- 6,459
IMG_20181112_115142.jpg
I'm getting old and it was hurting my neck!
Another possible source of F5 info might be the French forum Passion Usinages - Fraiseuses. Google Translate helps but there are numerous humorous translations. I have found a lot of useful information relating to my little mill amongst the posts.
BT
-
18th Nov 2018, 05:52 PM #11Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
Well i've found the problem, and its bad. The worm wheel in the feed gearbox has lost all of its teeth, right down to the root.
I have some enquries out in Switzerland, but im not sure if anything will come out of that, so im going to need to get this thing made. In order to do that im going to need to know what it used to look like, hoping they used something off the shelf-ish but i need some advice, ive been poring through stock gear catalogs and I am yet to find what i need. Maybe someone here can help.
Here is what i know about the worm and wheel
Being that its european im assuming its metric/module
Worm:
- Two start
- Left handed
- pitch of 12.25mm
- OD is 31.75mm
- Root diameter is 23.50mm
EDIT Just realised the worm pitch comes out to bang on .5", makes me very suspicious
Wheel
- 24 Teeth
- OD of blank is 55.88mm
- Root diameter could be about 44mm, very hard to measure in current state.
- ID is 17mm, 5mm keyway
From what i can read in the catalogs there are axial module worm wheel sets and pitch module sets, how do i tell what i have?
What other information am i going to need to reverse engineer this thing? Im assuming i need the center to center distance but that is going to be hard, ill have to reassemble the gearbox without the wheel and slip gauge blocks in.
Help.
IMG_20181117_085959.jpgIMG_20181116_194428.jpg
-
18th Nov 2018, 06:26 PM #12Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,563
A module 4 gear also has a pitch of 12.57, so it may not be as suspicious as you think. If it is a 2 start worm then the 'real' tooth size is module 2, with an ID of 43.37 and OD of 52mm. Should not be difficult to get one made.
Michael
-
18th Nov 2018, 06:36 PM #13
-
18th Nov 2018, 06:42 PM #14Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,563
I could lend the gears to Ralph too - as he has the same lathe, he could make a cutter and have all the fun of hobbing a gear. (see //metalworkforums.com/f65/t1708...78#post1661078)
Michael
-
18th Nov 2018, 07:36 PM #15Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
Thanks everyone, are you talking a self feeding type hobbing, making a matching worm, cutting flutes in it and then somehow doing the relieving? I just dont know how i would put any flank relief on the cutter?
would there be a way to plunge hob this considering the helix angle?
Similar Threads
-
Thread for Workshop Jacks
By electrosteam in forum METALWORK GENERALReplies: 13Last Post: 3rd Jan 2014, 08:44 PM -
My workshop
By Jan Nieuwenhuis in forum METALWORK GENERALReplies: 32Last Post: 16th Jun 2013, 08:01 AM -
Possible new workshop
By Sterob in forum METALWORK GENERALReplies: 12Last Post: 8th Jun 2008, 12:33 PM -
New Workshop
By Paulxsteel in forum METALWORK GENERALReplies: 7Last Post: 25th Feb 2008, 11:09 AM