Press forming flat bar
Hi guys,
I needed to make 8 brackets to attach the mudguards to the trailer for the sawmill I'm building. My first thought was to mill up nice curvy brackets from HDPE similar to the way truck mudguards are attached to their cantilevered tubular supports, but then I thought of bending saddle brackets up from 25 x 3mm flat steel. After consulting some guys at work, it seemed that a simple press tool for the hydraulic press would work to form the brackets. I made up a very basic tool from mild steel rod turned to the inside diameter of the clamps and some blocks of 25x25 bright mild steel welded to a steel base.
IMG_0940.jpgIMG_0941.jpgIMG_0942.jpgIMG_0944.jpg
The tool is made dead square, and to the final shape I wanted. ie. with no allowance for spring back. There was some spring back after forming, but a quick squeeze in the vice fixed that. The items came out of the tool after pressing with no jamming. Forming all 8 brackets plus a few spares took less than 10 minutes.
IMG_0943.jpg
I marked and cut them to length and drilled the holes after forming. Then de-greased them thoroughly and put them in the zinc plating bath. The picture below is before plating, to show how they fit on the trailer.
IMG_0948.jpg
Here they are zinc plated with a blue passivate finish.
IMG_E0960.jpg
This was a fun project, and the brackets will do the job well. The cantilevered tubes are 1 inch ID gal water pipe, pushed into sockets welded to the trailer frame so that I can remove the mudguards when using the mill. It's turned out to be a neat and simple way of attaching the mudguards.
Graham.
-
7th Oct 2018, 08:22 PM #2Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,945
Hi Graham, They are very nice neat brackets for the trailer.
Presses like yours are very underated, and can pressed into all sorts of uses.
I have a 20 tonne unit plus a small arbor press that I use for similar projects.
Do you have a Zinc Plating set up at home, or is that your work????
KrynTo grow old is mandatory, growing up is optional.
-
7th Oct 2018, 08:24 PM #3Pink 10EE owner
- Join Date
- Aug 2008
- Location
- near Rockhampton
- Posts
- 6,216
Well I am impressed. I always thought forming brackets like that would require a much more complicated former.
Gold, the colour of choice for the discerning person.
-
7th Oct 2018, 09:31 PM #4Senior Member
- Join Date
- Dec 2013
- Location
- Sydney
- Posts
- 201
Kryn, I agree, this is a Hafco 20 tonne hydraulic press that I've had for 30 years, and I couldn't be without it. I used it and the top half of that form tool to put a dog leg bend into some tabs made from 50x5mm bar. It bent it like cheese.
IMG_0956.jpg
I got a Jane Kits zinc plating kit for fathers day this year. It's been in constant use since I got it, plating all the steel parts I'm making for the sawmill. The process is remarkably simple, and quick. I should put a thread up about it.
RC. Yes, I too thought I'd need way more force and a more complex tool to do this job, but to my surprise it worked first go and with surprisingly low force. The 3mm bar just slid into shape. I did oil the blanks first. I'd only tacked the blocks in place, but it worked straight away and I kept going and did all the brackets.
Graham.
-
8th Oct 2018, 08:00 PM #5Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,945
[QUOTE=Oldbikerider;194134I got a Jane Kits zinc plating kit for fathers day this year. It's been in constant use since I got it, plating all the steel parts I'm making for the sawmill. The process is remarkably simple, and quick. I should put a thread up about it. Graham.[/QUOTE]
YES PLEASETo grow old is mandatory, growing up is optional.
-
8th Oct 2018, 10:02 PM #6
Done my fair share of bending plate with the bearing press in the shop. Bit of thought and keeping an eye out so work or tooling doesn't shoot out the side.
Then you discover punch presses. Now that the one offs have become a couple of hundred at a time!!Frisky wife, happy life. Then I woke up. Oh well it was fun while it lasted.From an early age my father taught me to wear welding gloves . "Its not to protect your hands son, its to put out the fire when u set yourself alight".
-
9th Oct 2018, 12:58 PM #7Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
Nice work. I too am surprised at the results for such a simple system. I will put my hand up to say I'm interested in your zinc plating as well.
SimonGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
Similar Threads
-
Forming edge on brass piece
By aquaman1 in forum METALWORK GENERALReplies: 6Last Post: 9th Apr 2018, 07:06 PM -
Clues on forming this tray?
By neksmerj in forum METALWORK GENERALReplies: 7Last Post: 5th Jul 2013, 09:21 PM -
Flat top car trailer
By jex in forum TRAILERS & OTHER FABRICATED STUFFReplies: 15Last Post: 17th Aug 2012, 10:00 AM -
flat belting .... ?
By morrisman in forum METALWORK GENERALReplies: 24Last Post: 3rd Feb 2012, 09:53 PM -
General Purpose 90° Forming Punches and Dies
By RustyCan in forum METALWORK GENERALReplies: 5Last Post: 24th Nov 2010, 09:08 PM