Thought this might be of interest to some people..

It is a pdf document on how to prepare chemicals for case hardening and the process itself...I have not tried it yet, but I have found one of the more exotic chemicals required, Barium Carbonate available on ebay.

It is 2.7MB in size---->>> http://users.beagle.com.au/lathefan/...0hardening.pdf