    Anybody know where I can get small lengths( 300mm or so) of s/s metric hex in Australia? I think the sizes I need are 16 mm and 19 mm.
    Tried Ebay and Google.
    I want to make some filler/ drain plugs for one of my m/bikes and they should fit metric spanners, etc.
    Stephen

  2. #2
    Join Date
    Jun 2007
    Location
    sydney ( st marys )
    Age
    64
    Posts
    4,890

    Default

    Hello Stephen if you have too much trouble finding what your after in W.A,I would more than likely be able to source material and get it posted to you.
    Short of that can you get hold of some round stock and mill the flats,or use imperial 5/8" is only .004" smaller than 16mm and 3/4" is only .002" smaller ,shouldnt be a great deal of slop for a ring,openender or socket.
    Is your main problem material sizes or getting it cut to length.

  3. #3
    Join Date
    May 2003
    Location
    Perth WA
    Posts
    526

    Default

    Hi Steve,
    BÖHLER-UDDEHOLM are the most likely source in Perth.

    cheers,
    Rod
    Cheers,
    Rod

  4. #4
    Join Date
    Feb 2006
    Location
    Lindfield N.S.W.
    Age
    62
    Posts
    2,383

    Default

    Offcuts Galore sells offcuts of sheet, rod, tube and bar in various metals including stainless. He tends to list stainless steel using the abbreviation SS and this may explain why you didn't find him on an eBay search.

    There is no hex listed at the moment, but the listing tends to be updated once or twice a week, so it pays to keep an eye out. When I buy from him, I tend to buy several pieces of metal of different kinds at once - George (the owner) is happy to combine the postage and the saving becomes quite significant if you have 4 or 5 pieces to buy
    Cheers

    Jeremy
    If it were done when 'tis done, then 'twere well it were done quickly

  5. #5
    Join Date
    Sep 2006
    Location
    Australind , WA
    Age
    58
    Posts
    1,281

    Default

    Quote Originally Posted by pipeclay View Post
    imperial 5/8" is only .004" smaller than 16mm and 3/4" is only .002" smaller ,
    Thanks guys,
    I guess I was too quick to ignore the imperial sizes. Those errors seem quite insignificant.
    I will check the other options as well.
    Thanks
    Stephen

  6. #6
    Join Date
    Feb 2007
    Location
    brisbane
    Posts
    245

    Default

    I will second Bohler (www.buau.com.au) as a good source. They are a pretty large outfit.
    I was at their Brisbane branch today picking up some 90 & 70mm 1045.

    I see a golf ball launcher on my horizon.

    Be aware they have minimum sale price of $50 so you will probably need to work out what else you need to get the order value up.

    Since you have a lathe there is no doubt there would be other steel you need.

    Haven't used Global Metals but they are also in WA
    51 Charles Street, Bentley - WA 6102
    PO Box 1046, East Victoria Park - WA 6101
    T: +61 8 9451 4733
    F: +61 8 9451 4755
    E: [email protected]
    Cheers

    Craig
    Brisbane

  7. #7
    Join Date
    Sep 2006
    Location
    Australind , WA
    Age
    58
    Posts
    1,281

    Default

    Thanks Hux, I will check them out.

  8. #8
    Join Date
    Jul 2007
    Location
    Perth
    Posts
    332

    Default

    Sterob, Another place to try is Prime Steel, Townsend St, Malaga, 92482666 they deal in off cuts of many metals. Not cheap but they will cut to length if req. No connection but do get some stuff from there. Alan.

Similar Threads

  1. Stainless Steel or 4140
    By Dusty Wheels in forum METALWORK GENERAL
    Replies: 9
    Last Post: 27th May 2007, 11:23 AM
  2. Stainless Steel welding
    By Clinton1 in forum WELDING
    Replies: 15
    Last Post: 6th Apr 2007, 01:58 AM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •