    Default Unusual drill failure.

    SAM_0890.jpgSAM_0889.jpgSAM_0888.jpg
    Hello again.
    This caught me by surprise. I was rotating my drill index to select a 3/16" drill and a 14mm jobber that was lurking with the others did a suicide jump to the floor. Followed by a loud ping. The total drop being about 1mtr. In the first pic you just get the impact damage to the outer corner on the lip. Pic 2 has a small discoloured section on both pieces. The third pic I tried for a better angle. If the break had happened during use I could understand fully. Failure started at the end of a flat ground on the land behind the margin where the flute runs out into the body.
    During my working life I have tortured drills to death but never seen a tool shatter from a low drop.
    Regards to all.
    BC

  2. #2
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    I'd say there's a good chance the bit probably had developed a crack in it beforehand and the drop just finished it off.
    Sometimes all that is needed is a nick out of a flute for it to break.

Similar Threads

  1. Patternmaking failure!
    By nigelpearson in forum THE FOUNDRY
    Replies: 1
    Last Post: 8th Mar 2022, 02:53 PM
  2. Success & Failure
    By DSEL74 in forum THE SMITHY
    Replies: 10
    Last Post: 4th Nov 2016, 07:00 PM
  3. HELP! Lathe failure
    By Vernonv in forum METALWORK GENERAL
    Replies: 28
    Last Post: 10th Aug 2012, 01:51 PM
  4. Main HDD failure
    By ubeaut in forum FORUMS INFO, HELP, DISCUSSION & FEEDBACK
    Replies: 29
    Last Post: 29th Apr 2007, 11:31 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •