Hello Grahame.
For difficult steel definitely reduce the rpm, use a stub drill to increase rigidity and if necessary reduce the rake angle so the drill is not so aggressive. Good brand drills are a must.
Regards
BC
-
27th Jun 2022, 07:11 PM #17
Hi BC
I went back today and did all that bar using the stub drill.
I had previously written I had set the slowest speed. That was not correct due to my poor eyesight incorrectly reading the chart on the DP. I am waiting on new prescription glasses.
I had to take my linisher outside to see well enough for grinding the drill to a shallower included angle.
It was tough to get through but not as bad as it has been. The difference being, it got hard immediately just before breaking through.
I am assembling a set of stub drills by means of breaking the longer ones.
Only two more holes to drill, now. Thank goodness!
Thanks
Grahame
-
1st Jul 2022, 01:19 PM #18Senior Member
- Join Date
- Nov 2019
- Location
- Brisbane
- Age
- 69
- Posts
- 452
drill grinding.
Hello again.
Changing the edge included angle may help but I was referring to grinding the flute to decrease the edge rake angle. The rake is the spiral angle of the flute. By reducing that the edge is stronger and less prone to burst thru surge. I did a video on using bench grinders and showed how to change drill rake angle. Also good for brass and some plastics. Making stub drills is OK but those made recently don't have a web thinning process. They are fat to the tip and point split to compensate.
The best with your project. BC
Similar Threads
-
Drilling square holes
By Groggy in forum METALWORK GENERALReplies: 11Last Post: 22nd May 2012, 01:12 AM -
Drilling holes
By brinesharks in forum METALWORK GENERALReplies: 9Last Post: 29th Nov 2009, 03:33 PM -
Drilling Holes with Rag
By Kody in forum METALWORK GENERALReplies: 1Last Post: 8th Jul 2009, 11:25 PM -
Drilling holes in steel
By henlan77 in forum METALWORK GENERALReplies: 17Last Post: 22nd Apr 2009, 10:24 PM -
Drilling big holes
By Vernonv in forum METALWORK GENERALReplies: 34Last Post: 28th Aug 2007, 10:07 PM