Hi Morrisman, Guys,
I use a "Shear tool" for fine finishing particularly if I'm going to run a ball race on it !
shear.jpg
The only problem with this kind of tool is that you can only remove a thou or so ! But you do get an extremely smooth finish. The cutting edge slopes back about 30 degrees with a few degrees of rake on the front face, and its not sensitive to height. If you wear the cutting edge you just move the tool up or down a few thou. I hone the edges to get it really sharp.Best Regards:
Baron J.
-
19th Dec 2021, 08:03 AM #3Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
Morrisman's tool has the shear edge nearly horizontal.
Baron J's is nearly vertical.
I wonder if there's an advantage either way?
-
19th Dec 2021, 09:07 AM #4Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
The Hercus Textbook of Turning recommends the same grind for truing up a faceplate.
Chris
-
19th Dec 2021, 09:27 AM #5Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
-
19th Dec 2021, 10:05 AM #6Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,671
-
19th Dec 2021, 10:24 AM #7Senior Member
- Join Date
- Oct 2009
- Location
- Upwey VIC
- Posts
- 187
-
19th Dec 2021, 11:36 AM #8Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
-
19th Dec 2021, 09:00 PM #9
Hi Guys,
I have occasionally unintentionally used my shear tool as a normal lathe tool ! However the swarf that you get from the Shear tool used properly is like a very very fine wool, "Fairy Hair" is a good expression to describe it.
You can get a similar cut on an internal surface using a round tool ground with a flat on the end ground at an at an angle ! Really good for through holes but you cannot get right to a flat bottomed hole. The way I've dealt with that issue is to take the bottom edge of a bore off for a mm or so.Best Regards:
Baron J.
Similar Threads
-
Re-registration of tool bit for a finishing pass?
By topari in forum METALWORK GENERALReplies: 11Last Post: 14th Apr 2018, 09:33 PM -
Lathe Knife Tool and Boring Tool Sharpening
By metaler in forum METALWORK GENERALReplies: 30Last Post: 3rd Mar 2017, 08:38 PM -
Stanley Knife Blade as Finishing Tool ?
By steamingbill in forum METALWORK GENERALReplies: 4Last Post: 13th Aug 2016, 12:10 AM -
Shaper shear tool for finishing
By .RC. in forum METALWORK GENERALReplies: 3Last Post: 26th Dec 2011, 10:06 PM -
Poor finish with my finishing tool.
By simonl in forum METALWORK GENERALReplies: 87Last Post: 23rd Dec 2011, 11:25 PM