Needs Pictures: 0
Results 1 to 15 of 56
Thread: Rivnuts - or Similar
-
20th Nov 2021, 08:04 AM #1Golden Member
- Join Date
- Apr 2009
- Location
- Kingswood
- Posts
- 930
Rivnuts - or Similar
I am mounting electronic components onto the 1.5 mm back-plate of a new electrical enclosure for my CNC mill.
This includes DIN rail for PCB cards and relays, relatively heavy stepper driver modules and other components.
The stepper modules really need a couple of M5 full-strength fixings, doubtful in 1.5 mm.
Many years ago I used rivnuts in thin sheet metal, but they were impact rivetted from the back.
A version currently available inserts from one side, using a tool similar to a pop-rivet gun.
Is this the best solution ?
Any recommendations for a supplier ?
Keep well,
John.
-
20th Nov 2021, 08:08 AM #2Golden Member
- Join Date
- Sep 2009
- Location
- Sydney
- Posts
- 666
Rivnuts - or Similar
I did this (on a much smaller scale) by drilling the enclosure and having a small countersunk bolt through the hole from the back, with a threaded stand off on the inside. Would that work too?
-
20th Nov 2021, 08:22 AM #3Senior Member
- Join Date
- Apr 2007
- Location
- Newcastle
- Posts
- 229
I bought my setting tool from a specialty place years ago but I think I saw something similar in Sydney Tools the other day.
If the 1.5mm is not enough you could always do similar to the standoff idea above but use a thick mounting plate either on the backside or both sides. That way you're sandwiching the 1.5mm and spreading the load out over a much larger area.
-
20th Nov 2021, 08:41 AM #4Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
I discovered Rivnuts/Nutserts a couple of years ago, and give them a thumbs up.
Chinese make, Ebay sourced kits have tool and some rivets.
Rivet sets are available too, in MS, SS, Aluminium.
They take a bit of effort to install with the hand tool, and power tools are an option.
They can also be installed with simple bolt, nut, spacer. See google.
I used them to hold up shelf brackets in a shipping container, and are up to a pretty heavy load (in MS).
-
20th Nov 2021, 09:18 AM #5Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
6mm Rivnuts with oversize washers is how I installed cargo hold down rails inside my vans on just standard body thickness steel and I am constantly amazed at what load they can hold.
This is my old van - on the newer on there are rails all the way along the walls but up near there roof.
van.jpg
-
20th Nov 2021, 10:27 AM #6Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,673
Rivnuts are great, but another practical option is to pop rivet - either directly to the panel (in the case of din rails that never need to be removed, or rivet on a suitable mounting plate/bracket to the panel. Takes a decent amount of force to pull steel pop rivets though 1.5mm. Even aluminum rivets are fine in most cases.
For occasional use and particularly with smaller nuts the generic rivnut tools work fine. If you were putting in a lot of larger steel nuts it would be worth investing in a decent tool.
You can get generic mount brackets that clip onto din rail too.
Another possible option for mounting your driver modules is to use a sort of Z rail (imagine one side of a din rail) and have a matching bracket on the driver module. The brackets take all the weight of the module and you just need to restrain the bottom of the module so it can’t pull out or lift up.
Similar mounting method is used for metal household electrical switchboards - screw the Z bar onto the wall, hang the switchboard on it an put in a couple of screws at the bottom of the unit to stop it lifting up/out or moving sideways.
Steve
-
20th Nov 2021, 10:37 AM #7Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,673
Another method for getting more engagement in a panel is to punch the hole for the fastener rather drill it. The panel metal pushes out the back of the panel and can give you a lot more thread engagement.
Used a lot in production - I haven’t tried a DIY approach but thinking make the a hole with something like a nail then use the self tapping screws that have the fine threads and a small cutting notch at the end.
This 1.6mm panel just used old style pointed self tapping screws, and you can see the material deformed out the rear of the hole even from those.
Steve
-
20th Nov 2021, 10:54 AM #8Senior Member
- Join Date
- Oct 2008
- Location
- blackburn vic
- Posts
- 297
Rivnuts
One thing I found when fitting out a 4wd was Mic up the od of the rivnut and use that size drill bit for the hole. They like being tight in the mounting hole
Roger
-
20th Nov 2021, 11:40 AM #9Most Valued Member
- Join Date
- Mar 2011
- Location
- Southern Flinders Ranges
- Posts
- 1,555
I’d probably turn some plastic into stand-offs and bolt from both sides. Rivnuts are awesome until they start spinning in the panel.
Total tools have the Kincrome tool, set heads and 80 assorted nuts in a box for $79, seems reasonable to me.
https://www.totaltools.com.au/106444...RoCdZ0QAvD_BwE
-
20th Nov 2021, 01:01 PM #10
-
20th Nov 2021, 01:04 PM #11
-
20th Nov 2021, 01:07 PM #12
-
20th Nov 2021, 02:32 PM #13Senior Member
- Join Date
- May 2015
- Location
- Richmond
- Posts
- 214
I have plenty of m5 Rivnuts (Nutserts) and the tool here if you need them John.
DH
-
20th Nov 2021, 03:58 PM #14
Just about any fasteners vendor.
The fixing tool seems expensive for what it is. However a cheap work around tool can be cobbled up.
See examples on U Tube. I am sure our blokes have made the tool and posted threads about it here.
Specfast has the Rivnuts by the metric size starting at 3mm .
Have not purchased imperial from them , so unaware of that aspect .
Grahame
-
20th Nov 2021, 04:48 PM #15Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Similar Threads
-
Rivnuts?
By wm460 in forum METALWORK GENERALReplies: 18Last Post: 14th May 2017, 08:16 PM -
Need a 300mm caliper or similar
By Michael G in forum WANTED TO BUYReplies: 0Last Post: 24th Jan 2016, 07:49 PM -
any one know which lathe this is ? look similar to the Lorch
By thorens in forum METALWORK GENERALReplies: 11Last Post: 27th Oct 2013, 08:44 AM -
Lathes similar to AL320G
By 19brendan81 in forum METALWORK GENERALReplies: 18Last Post: 25th Nov 2011, 08:25 PM -
9x20 and similar lathes
By Big Shed in forum METALWORK GENERALReplies: 1Last Post: 8th Sep 2011, 09:45 AM