    I bought this nutsert kit for both my son and I.
    The kit is great, but you really need the longer tool or the drill adaptor for M8 and up, as I have pretty strong hands and this tool Max's out at M6.
    The drill tool is expensive at around $100, from memory the longer tool is around $40

    https://www.ebay.com.au/itm/1606PCS-...154756-20017-0

    Sent from my 5007U using Tapatalk
    Using Tapatalk

  2. #17
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    https://www.ebay.com.au/itm/430Pcs-R...154756-20017-0

    Sent from my 5007U using Tapatalk
    Using Tapatalk

  3. #18
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    They have gone up in price, the next inline is $149, so you would need to using it often to justify the price

    https://www.ebay.com.au/itm/Professi...154756-20017-0

    Sent from my 5007U using Tapatalk
    Using Tapatalk

  4. #19
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    Just when you all think that oils are oils and rivnuts are rivnuts consider the following :

    https://www.rivetnutusa.com/rivnut-rivet-nut/

    Probably not readily available locally.

    Grahame

  5. #20
    Join Date
    Apr 2009
    Location
    Kingswood
    Posts
    930

    Default

    Thanks guys, you all have combined to answer just about every aspect on this subject.
    Fantastic response, I think we all love to tinker with fixings.

    I was looking at Rivnuts as they seemed a good general-purpose tool to have in the shop.

    DaveJ,
    Yes, I dream about 3 mm backplates in electrical boxes, but such boxes are just too expensive now.
    I also am reusing the original control box supplied with the mill, at 2.2 mm it is Ok.
    We should compare our boxes at some time.
    The friction drilling is really interesting, I will research this further.

    DH,
    I will contact you to discuss a possible loan of the tool to get some experience.

    Keep well all,
    John.

  6. #21
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Quote Originally Posted by electrosteam View Post
    Thanks guys, you all have combined to answer just about every aspect on this subject.
    Fantastic response, I think we all love to tinker with fixings.

    I was looking at Rivnuts as they seemed a good general-purpose tool to have in the shop.

    DaveJ,
    Yes, I dream about 3 mm backplates in electrical boxes, but such boxes are just too expensive now.
    I also am reusing the original control box supplied with the mill, at 2.2 mm it is Ok.
    We should compare our boxes at some time.
    The friction drilling is really interesting, I will research this further.

    DH,
    I will contact you to discuss a possible loan of the tool to get some experience.

    Keep well all,
    John.
    I've just mounted my 600x400x200mm cabinet with DRO scale cables routed behind with 20x3mm flat bar it to make it all neat and out of harm's way.
    Just working out a nice looking arm to go to the control panel I'm going to build.

    The mill is fully functional, but there are cables and wires everywhere since I've added so many home built accessories, like electric power drawbars X2, power, power quill feed etc.

    It's still only a manual mill, but with 2 vfds, one for the vertical and horizontal which will be a blessing and all the other stuff I have here to go in to make it like factory install is a lot of work.

    X,Y,Z cable routing for knee movement

    Sent from my 5007U using Tapatalk
    Using Tapatalk

  7. #22
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Quill and ram scale wire storage for when the ram is turned 180 degrees to use.

    Sent from my 5007U using Tapatalk
    Using Tapatalk

  8. #23
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,959

    Default

    John, I think I've a set here you can have, I'll even throw in some 5mm Rivnuts, if you want it.
    I upgrade to a heavier duty set
    Kryn
    To grow old is mandatory, growing up is optional.

  9. #24
    Join Date
    May 2015
    Location
    Richmond
    Posts
    214

    Default

    Quote Originally Posted by jack620 View Post
    Completely off topic, but I’m just curious. Richmond Vic, NSW or Tas?
    Nsw. Only 25 minutes from John Electrosteam.

    D

  10. #25
    Join Date
    Apr 2018
    Location
    Perth
    Posts
    168

    Default

    For one offs where not worth expense of buying, tool you can use a bolt, washer and a nut to set the rivnuts.

    Ive used a similar method when I had to install a heap of M12 steel ones in a conveyor frame.

    https://www.youtube.com/watch?v=heLMQYwE1_o

  11. #26
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Quote Originally Posted by electrosteam View Post
    Thanks guys, you all have combined to answer just about every aspect on this subject.
    Fantastic response, I think we all love to tinker with fixings.

    I was looking at Rivnuts as they seemed a good general-purpose tool to have in the shop.

    DaveJ,
    Yes, I dream about 3 mm backplates in electrical boxes, but such boxes are just too expensive now.
    I also am reusing the original control box supplied with the mill, at 2.2 mm it is Ok.
    We should compare our boxes at some time.
    The friction drilling is really interesting, I will research this further.

    DH,
    I will contact you to discuss a possible loan of the tool to get some experience.

    Keep well all,
    John.
    I bought the last cheap slotted cable ducting from electrotraders.
    40x80mm and 25x80mm.
    It was only $13 for 2x 1m lengths and $10 postage.
    I looked around and it easily went up to $85 for a 1m piece, it was runout stock.
    It's a pity they where not at the same time to save on postage.
    It will make the install look neat and tidy, just like the factory boxes on mills.

    Sent from my 5007U using Tapatalk
    Using Tapatalk

  12. #27
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Thanks for the heads up.
    Seems the $149 are the way to go, or just go back to the long handled manual tool

    Sent from my 5007U using Tapatalk
    Using Tapatalk

  13. #28
    Join Date
    Nov 2008
    Location
    North Brisbane. Qld. Australia
    Age
    70
    Posts
    1,514

    Default

    Don't buy this type of Nutsert tool. They deform and split at the plastic nose section with 6mm nutserts. I've destroyed a couple of them. Cheap eBay ones are probably worse.
    Attached Images Attached Images
    Nev.

  14. #29
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,480

    Default

    Hi Guys,

    Wouldn't it be better to turn up some mandrels to fit into a pop rivet tool, threaded to suit what ever nutsets/rivnuts used.

    I made several mandrels to suit 2, 4, & 6Ba and 3, 4, 5mm press serts ! Though if you don't have the room to press them in, a mandrel in a pair of lazy tongs works well.
    Best Regards:
    Baron J.

  15. #30
    Join Date
    Nov 2008
    Location
    North Brisbane. Qld. Australia
    Age
    70
    Posts
    1,514

    Default

    Quote Originally Posted by BaronJ View Post
    Hi Guys,


    I made several mandrels to suit 2, 4, & 6Ba and 3, 4, 5mm press serts ! Though if you don't have the room to press them in, a mandrel in a pair of lazy tongs works well.
    Is this the type you use?

    https://www.youtube.com/watch?v=tQiamU5QUn0

    Wondering if they would work in timber.
    Nev.

Page 2 of 4 FirstFirst 1234 LastLast

Similar Threads

  1. Rivnuts?
    By wm460 in forum METALWORK GENERAL
    Replies: 18
    Last Post: 14th May 2017, 08:16 PM
  2. Need a 300mm caliper or similar
    By Michael G in forum WANTED TO BUY
    Replies: 0
    Last Post: 24th Jan 2016, 07:49 PM
  3. any one know which lathe this is ? look similar to the Lorch
    By thorens in forum METALWORK GENERAL
    Replies: 11
    Last Post: 27th Oct 2013, 08:44 AM
  4. Lathes similar to AL320G
    By 19brendan81 in forum METALWORK GENERAL
    Replies: 18
    Last Post: 25th Nov 2011, 08:25 PM
  5. 9x20 and similar lathes
    By Big Shed in forum METALWORK GENERAL
    Replies: 1
    Last Post: 8th Sep 2011, 09:45 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •