Needs Pictures: 0
Results 1 to 15 of 18
Thread: Confusion regarding tap sizes
-
1st Nov 2021, 06:50 AM #1New Member
- Join Date
- Nov 2021
- Location
- Oshawa
- Posts
- 3
Confusion regarding tap sizes
I'm just getting into metalworking, and tap sizing seems very complicated to me. If I wanted to tap a 1.5 mm hole in hardened steel (58-60 HRC), what size / kind of tap should I use? Does thread size affect the anything along the process other than the screw I would have to use? Thanks!
-
1st Nov 2021, 08:07 AM #2
Welcome to the MetalWork Forums.
In this case the thread diameter 1.5mm is very small, indeed.
I would suggest that drilling a tap size hole- smaller than the thread OD is going to be a very difficult exercise for a beginner.
As drill diameter sizes decrease , the rpm required to run them efficiently,increases.
Without practice and understanding of the procedure, I predict you will snap the drill bit, let alone the tap.
You will need something like a Dremel tool to provide the drill bit RPMs, required. I would be using a Dremel drill press to fix the Dremel tool to enable square to job drilling. Revolutions around around 10,000rpm are required.
Drilling hardened steel is another problem. You do not mention the thickness that is to be drilled.
To my mind,the hole could only be drilled and tapped when the steel is in a soft annealed state and then hardened after the drill and tap operation.
If you have never drilled a hole and run a tap I would try some larger size ,say 6mm before moving ahead and do this on mild steel,first up.
I have 50 years of drill and tap experience behind me and yet when I drilled a 1.5mm in 16 mm mild steel and it took several drill bits and new holes before I was successful.
A light sense of touch and clearing the drill bit often is essential.
As far a tapping a hole that small I have not tried that,so you are on your own there.
welcome to the forums
Grahame
-
1st Nov 2021, 08:32 AM #3Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,080
Gear cutting specialists and general engineers www.hardmanbros.com.au
Fine pitch gear cutting from 0.1 Module www.rigear.com.au
-
1st Nov 2021, 08:36 AM #4Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
I agree with Grahame, I wouldn't even attempt to tap a 1.5mm diameter in anything harder than mild steel .
Would it be possible to anneal the steel and regarded it after drilling and tapping the hole?
More info about the material and task you are trying to achieve might assist us in helping you.
-
1st Nov 2021, 05:38 PM #5Diamond Member
- Join Date
- Mar 2014
- Location
- South of Adelaide
- Posts
- 1,227
only way to thread steel that hard is to threadmill in a very good cnc mill, or 4 axis EDM. tapping will not work
-
1st Nov 2021, 06:39 PM #6Senior Member
- Join Date
- Apr 2007
- Location
- Newcastle
- Posts
- 229
I'm with the others. Things can turn south really quick with small taps. I generally wouldn't even try at less than 4-5mm and 1.5mm sounds impossible.
-
1st Nov 2021, 07:20 PM #7
Hi Guys,
You could machine a hole in your steel and then use a softer threaded insert ! I've seen Japanese stuff done that way. I agree with the others, there is no way you could thread a hole in a HRC50 hard steel with a tap !Best Regards:
Baron J.
-
1st Nov 2021, 07:27 PM #8Most Valued Member
- Join Date
- Nov 2008
- Location
- North Brisbane. Qld. Australia
- Age
- 70
- Posts
- 1,514
-
1st Nov 2021, 11:51 PM #9Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
Yeah, using a special oversize tap and tapping before hardening is possible but still sucks as your tolerance is wholly dependant on repeatability of material and treatment. I think your only hope for tapping 60rc would be EDM, 50 would tap okay with a carbide tap but as stated not happening at 1.5mm
Sent from my SM-G973F using Tapatalk
-
2nd Nov 2021, 02:12 PM #10
Is it just me ,or have others noticed that 1.5 mm does not appear in the commonly available drill tap charts online or in books.
ISO Metric Course charts that I saw list 1, 1.1, 1.2,1.4,1.6 and so on. No 1.5mm thread size.
I googled and did find an available 1.5mm taps sold as a single for what is obviously aimed at veterinary surgical implants.
StevensonCh, just curious, is the 1.5mm tap spec a part of something specified in a plan or drawing design, or is it a number you have settled on as being the correct diameter ?
Grahame
-
2nd Nov 2021, 03:17 PM #11Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,080
TBH, I just saw "tap 1.5mm in HRC 58-60" and didn't bother thinking if 1.5mm was even a thing because it can't be done
Gear cutting specialists and general engineers www.hardmanbros.com.au
Fine pitch gear cutting from 0.1 Module www.rigear.com.au
-
2nd Nov 2021, 04:54 PM #12Senior Member
- Join Date
- Apr 2007
- Location
- Newcastle
- Posts
- 229
It crossed my mind that the 1.5mm is a mix up with reading the threadform and is actually pitch.
-
2nd Nov 2021, 08:13 PM #13Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
The hardest thing I have put threads into was the 10mm thick Bisalloy plate which forms the lower half of the base of my tri-grinder lazy susan
I went through 3 taps cutting the threads for the 12, 3/16" machine screws
One tap broke (luckily enough was poking out to be able to grab it with a multigrips) and two other taps were stuffed by the time I finished.
Mind you they were cheap carbon steel taps - I still don't know why I just didn't use through screws with nuts underneath.
IMG_2911.jpg
-
2nd Nov 2021, 08:53 PM #14
Hi Guys,
Metric coarse 1.5 X 0.3 mm and metric fine 1.5 X 0.2 mm are common in HDD assemblies. I've also seen much finer screws used as well, probably around 0.5 mm. All in aluminium components. I think some of the very small ones may be self threading since the screw seems to be tapered, with a coarse thread a bit like a wood screw. I believe that they are stainless steel since you cannot pick them up with a magnet.Best Regards:
Baron J.
-
2nd Nov 2021, 09:30 PM #15Senior Member
- Join Date
- Feb 2012
- Location
- Tamworth, NSW
- Posts
- 205
Making folding knives common sizes are 2-56, 1-72 or sometimes 0-80 so these are down around the 1-2.5mm size. I regularly tap 2-56 in titanium which can end in tears pretty easily but I would never try hardened steel.
Similar Threads
-
Confusion
By NedsHead in forum AUTO RESTORATIONReplies: 8Last Post: 29th Oct 2021, 03:25 PM -
4140 confusion
By morrisman in forum METALWORK GENERALReplies: 4Last Post: 23rd Apr 2021, 09:55 PM -
40 taper tooling confusion
By OxxAndBert in forum METALWORK GENERALReplies: 10Last Post: 20th Feb 2019, 12:38 PM -
Tumble Reverse Confusion
By pench in forum METALWORK GENERALReplies: 3Last Post: 12th Feb 2014, 09:08 PM -
MIG wire confusion
By twebb01 in forum WELDINGReplies: 19Last Post: 9th Jun 2012, 12:46 PM