    I bought a new Nicholson bastard file (made in Sth. America), I managed to dull it after a few hours of use on high carbon steel !

    I tried the white vinegar etch but that has not had any effect , no good. Maybe a stronger acid is needed. Maybe the prep wasn't good enough, cleaning the grooves, I used a copper scraper.

    Any suggestions ?

  2. #2
    Join Date
    Jul 2016
    Location
    Melbourne
    Age
    35
    Posts
    1,522

    Default

    If it lost its edge that quickly id sharpen it straight into the bin and replace it.

    Sent from my SM-G973F using Tapatalk

  3. #3
    Join Date
    Aug 2008
    Location
    Melbourne
    Age
    34
    Posts
    1,079

    Default

    Unfortunately, the new Nicholson stuff (along with many other well-known brands) it's kinda crap...

    This guy has a lot of new-old-stock files (and a ton of other stuff like taps, endmills, etc.) from back when they were made properly at very good prices https://www.ebay.com.au/sch/i.html?_...oc=2&_nkw=file Based in Australia as well so postage won't kill you
    No affiliation other than being a happy customer
    Gear cutting specialists and general engineers www.hardmanbros.com.au
    Fine pitch gear cutting from 0.1 Module www.rigear.com.au

  4. #4
    Join Date
    Sep 2008
    Location
    Riddells Creek, Vic.
    Posts
    837

    Default

    What was the hardness of the steel being filed?

  5. #5
    Join Date
    Jul 2008
    Location
    near Warragul, Victoria
    Posts
    3,723

    Default Spring

    Quote Originally Posted by Techo1 View Post
    What was the hardness of the steel being filed?
    I am beveling the lower edge , of old Land Rover leaf springs ( long story ) , I use a angle grinder to remove 90% then finish with a file. I don't have a linisher which would be handy for this type of job.

    Thanks for the replies, yes, a new Nicholson file is only 10 bucks from Bunnings , I guess I might have to buy a few to finish this job !

    elanjacobs thanks for the link

  6. #6
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    I wouldn't expect any file to last very long on leaf spring steel.
    Chris

Similar Threads

  1. Metal files 101
    By Grandad-5 in forum METALWORK GENERAL
    Replies: 205
    Last Post: 12th Sep 2018, 10:50 AM
  2. Storing files
    By ventureoverland in forum METALWORK GENERAL
    Replies: 20
    Last Post: 15th Jul 2017, 12:49 AM
  3. Ressurecting old files.
    By Schtoo in forum METALWORK GENERAL
    Replies: 30
    Last Post: 7th Jun 2007, 10:05 PM
  4. Music files?
    By gemi_babe in forum FORUMS INFO, HELP, DISCUSSION & FEEDBACK
    Replies: 9
    Last Post: 7th Sep 2004, 10:30 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •