Page 2 of 2 FirstFirst 12
Results 16 to 24 of 24
  1. #16
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,188

    Default


  2. #17
    Join Date
    Jul 2021
    Location
    ACT
    Posts
    12

    Default

    Thanks all!

    It turns out that I had made a mistake and the shaft is 1", not 1 1/8". It'll certainly be easier to find a 1" drill bit. Whether it'll be clean enough for to fit a shaft without reaming remains to be seen, but at least I won't need a hole saw.

  3. #18
    Join Date
    Feb 2014
    Location
    Werribee, Melbourne
    Posts
    178

    Default

    I agree with Michael - unless that handle is a nice snug fit it will be frustrating to fit and use.
    If you can get it to Melbourne easier than getting it to riverbuilder by some chance then I would be happy to bore that out for you as well so there is another option for you.
    I suspect that the NSW-VIC border won't be easing off for a while but the offer is there.

    Ray

  4. #19
    Join Date
    Jul 2021
    Location
    ACT
    Posts
    12

    Default

    Quote Originally Posted by Ray-s View Post
    unless that handle is a nice snug fit it will be frustrating to fit and use.
    it's designed to be used with a pin, so it doesn't have to be perfect. The shaft has a 1/4" pin hole

    Thanks so much for your offer

  5. #20
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,188

    Default

    It doesn't matter if it has a pin, if it's a little loose, the pin and pin hole will wear every time you move it and that will eventually put more pressure on the pin so that it may eventually break.

    What sort of a drill do you plan to drill the hole with?

  6. #21
    Join Date
    Sep 2008
    Location
    Riddells Creek, Vic.
    Posts
    837

    Default

    To be able to do this properly the person taking on the job will need to have the shaft as well.

  7. #22
    Join Date
    Oct 2001
    Location
    ACT
    Posts
    667

    Default

    I understand the Ueee is no longer in the ACT (has moved to bigger premises).

    However I am (in ACT), and can bore it out for you, but as Techo1 has said for best results I will need the shaft.

  8. #23
    Join Date
    Jul 2021
    Location
    ACT
    Posts
    12

    Default

    Thanks, everyone!

    I'm going to take Riverbuilder up on his offer, as he can supply the handwheels too

  9. #24
    Join Date
    Jul 2006
    Location
    Athelstone, SA 5076
    Posts
    4,258

    Default

    Quote Originally Posted by BobL View Post
    It doesn't matter if it has a pin, if it's a little loose, the pin and pin hole will wear every time you move it and that will eventually put more pressure on the pin so that it may eventually break.

    What sort of a drill do you plan to drill the hole with?
    and it will become a real pain in the ass

Page 2 of 2 FirstFirst 12

Similar Threads

  1. WTB-Cast Small Cast Iron Lapping Plate
    By Betnorm in forum WANTED TO BUY
    Replies: 4
    Last Post: 19th Nov 2019, 01:01 PM
  2. When does cast iron not machine like cas t iron?
    By simonl in forum METALWORK GENERAL
    Replies: 20
    Last Post: 31st Jul 2018, 08:57 PM
  3. Cast iron english wheel.
    By clear out in forum THE FOUNDRY
    Replies: 23
    Last Post: 29th Nov 2014, 06:28 AM
  4. Replies: 8
    Last Post: 19th Jun 2013, 06:32 PM
  5. Cast iron VS Cast steel lathe compound slide
    By Ueee in forum METALWORK GENERAL
    Replies: 10
    Last Post: 23rd Dec 2012, 11:40 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •