milling aluminium with woodwork router bits
I want to make a couple of hawse fairleads, like this
https://www.amazon.com/WARN-94244-Ha.../dp/B018AIHO5W
Planning on casting in aluminium. I've been looking at corner-rounding endmills and the price for one with around 1" radius is way over the top. I'm wondering if it is worth trying a woodwork rounding-over bit like this
https://www.ebay.com.au/itm/264169233241?
and what are the pitfalls of doing so?
-
12th May 2021, 03:18 PM #2Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
BIL is an Al boilermaker on shipbuilding duties at Naval base here in WA. His toolkit includes a bunch of ww tools including hand held WW circulars,, jigsaws, and routers. He regularly slightly over fills TIG & MIG welds and rounds over with round over router bits. He welds lots of curved surfaces and by the time he’s finished they look seamless.
-
12th May 2021, 03:47 PM #3Golden Member
- Join Date
- Jun 2007
- Location
- Vic
- Age
- 48
- Posts
- 544
I used the wood router to cut this dovetail. It worked with mild steel and aluminium is softer.
20160721_230016.jpg
-
12th May 2021, 04:07 PM #4Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
Wax or meths can be used as a lube for Al.
-
12th May 2021, 05:09 PM #5Most Valued Member
- Join Date
- Mar 2011
- Location
- Southern Flinders Ranges
- Posts
- 1,553
The V groove in these was cut with a router bit
-
12th May 2021, 05:40 PM #6Golden Member
- Join Date
- Apr 2018
- Location
- Drouin Vic
- Posts
- 634
Well that's very good to know, I'll have to get a suitable rounding-over bit and give it a try. Around one-tenth of the price for a router bit as for a milling cutter. Might be a bit of a challenge for a collet to hold onto a cutter with a 3" o.d. and a 1/2" shank, I guess I'll just take it gently.
-
12th May 2021, 06:23 PM #7Most Valued Member
- Join Date
- Mar 2011
- Location
- Southern Flinders Ranges
- Posts
- 1,553
Cast ally is easier to route than some hardwood.
Having said that, I’d consider machining them over casting them if you want them to last.
-
12th May 2021, 06:33 PM #8Best Regards:
Baron J.
-
12th May 2021, 07:11 PM #9Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
-
12th May 2021, 09:05 PM #10Most Valued Member
- Join Date
- Mar 2011
- Location
- Southern Flinders Ranges
- Posts
- 1,553
The inside radius where the rope comes out only needs to be around 10ish mm.
Out side radius for aesthetics can be whatever you want, I commonly use an R3 for stuff like that.
Both are significantly smaller than 3"
-
12th May 2021, 09:36 PM #11Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Pete,
that bit has an 8mm radius. I think this is the one you want (maybe): https://unitedtoolsmckinnon.com.au/p...ver-router-bitChris
-
12th May 2021, 09:53 PM #12Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
To ask the obvious, why? Unless you are planning on making lots of them by the time you have made a pattern, well, you have already made one. What's one or two extra...
Carbide wood bits work fine on Al. The bigger the radius, the slower the rpm though. As others have suggested, for cosmetics any radius will do so chose something manageable.
Michael
-
12th May 2021, 10:16 PM #13Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,079
No problem holding it, I've run plenty of 2.5" diameter bits in wood, both by hand and in a CNC, and they don't go anywhere. Just go easy on the feed, use lube as mentioned above and don't try to cut too deep in one pass; once you start approaching full profile, I'd be doing no more than 1mm depth per pass
-
12th May 2021, 11:31 PM #14Golden Member
- Join Date
- Apr 2018
- Location
- Drouin Vic
- Posts
- 634
A router cutter with a radius of about 3/4" appears to have an outside diameter somewhere in the vicinity of 3 inches, just from looking at photos at present (edit- I was guesstimating based on 1/2" shank but the one I was looking at is probably 1/4" shank. So much smaller OD than I thought.)...I'm talking here about milling the inside of the slot to give a radius for the rope to run on, not the outside of the body of the thing. which I think is what you mean in the suggestion above about using the lathe? I can't see any way to machine the inside of the slot in a lathe rather than a mill.
I'm actually going a bit cold on the casting idea, I was originally thinking of casting them with lettering or some other design but I've decided that's a waste of time so I'm now thinking just mill them from a billet. The better quality bought ones appear to be about 1.5" thick with a 3/4" radius on both the back and front inside the slot for the rope to run over. So I'm looking at a router bit with about that radius.
Another thought- if I'm going to mill them from stock, what about steel stock? I know with this sort of thing, the harder the material the better, as it is damaged surfaces that damage the rope. I have some leftover offcuts of forklift tine (almost certainly 4140) in ideal dimensions; would I have any hope of radiusing that with a router bit?
-
13th May 2021, 12:17 AM #15Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,079
Similar Threads
-
Router Bits
By bwal74 in forum METALWORK GENERALReplies: 6Last Post: 18th Apr 2021, 10:42 PM -
Opinions on Sharpening Router Bits?
By NGrimberg in forum CNC ForumReplies: 3Last Post: 16th Jul 2020, 09:25 AM -
Small HS Router Bits
By electrosteam in forum CNC ForumReplies: 6Last Post: 23rd Nov 2017, 11:54 AM -
Router bits
By phaser in forum METALWORK GENERALReplies: 11Last Post: 1st Mar 2017, 11:14 PM -
router bits in lathe to mill aluminium - youtube video
By steamingbill in forum METALWORK GENERALReplies: 3Last Post: 29th Oct 2013, 06:55 PM