Results 1 to 13 of 13
  1. #1
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default Pneumatic chamfering tool

    I don't think I have a use for one of these, but maybe some of you do?

    https://www.youtube.com/watch?v=Ak747RzFUa8
    Chris

  2. #2
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,188

    Default

    My Al ship builder BIL uses a small hand held router and standard WW carbide rounding bits to round over some of his corner TIG welds. He's typically welding 12 -16 mm plate and by the time he's finished it looks like a solid curved piece.

  3. #3
    Join Date
    Aug 2011
    Location
    Perth, Western Australia
    Age
    67
    Posts
    362

    Default

    Nice tool if you have one but I`ll stick with my DIY one.
    WW bits for ally and die grinder bits for steel. Good enough for me.

    DSC06564 e.jpg

    Tony

  4. #4
    Join Date
    Mar 2014
    Location
    South of Adelaide
    Posts
    1,227

    Default

    We have one based on a straight die grinder at work. has been very handy, but it cost more like $1000

  5. #5
    Join Date
    Apr 2012
    Location
    Healesville
    Posts
    2,129

    Default

    Quote Originally Posted by jack620 View Post
    I don't think I have a use for one of these, but some of you do?

    https://www.youtube.com/watch?v=Ak747RzFUa8
    G/day Chris, hey thanks for that m8..... I dont need one either but it looks like a handy thingo so i grabbed one from here https://www.aliexpress.com/item/1005...2c884c4dP9L3rg

  6. #6
    Join Date
    Aug 2011
    Location
    Perth, Western Australia
    Age
    67
    Posts
    362

    Default

    Quote Originally Posted by shedhappens View Post
    G/day Chris, hey thanks for that m8..... I dont need one either but it looks like a handy thingo so i grabbed one from here https://www.aliexpress.com/item/1005...2c884c4dP9L3rg

    Do these come with the changeable carbide tips like the one in the OP or they a tool steel insert?

    Tony

  7. #7
    Join Date
    Apr 2012
    Location
    Healesville
    Posts
    2,129

    Default

    Quote Originally Posted by bts View Post
    Do these come with the changeable carbide tips like the one in the OP or they a tool steel insert?

    Tony
    G/day Tony, here is a close up from one of the pics on the web page link above, looks like carbide inserts to me.
    Attached Images Attached Images

  8. #8
    Join Date
    Oct 2004
    Location
    Southern Highlands NSW
    Posts
    1,898

    Default

    Any plastic parts on these tools?

  9. #9
    Join Date
    Mar 2011
    Location
    Southern Flinders Ranges
    Posts
    1,552

    Default

    They use a triangular carbide insert.
    If you’re doing a lot of heavy structural section that requires bevelling to weld, they are the ducks.. They are also very handy for a thousand other things that you don’t think of when you buy it. There was a thread on here about 18 months or so ago when they were first starting to appear more widely, someone bought one and did a bit of a show and tell on it.
    The weak point is the guide bearing, as the youtube video suggests, the one it comes with will flog out relatively quickly, put a decent quality replacement on it, and keep a couple as spares.

  10. #10
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    Quote Originally Posted by racingtadpole View Post
    They are also very handy for a thousand other things that you don’t think of when you buy it.
    Looks like I do need one after all.
    Chris

  11. #11
    Join Date
    Sep 2008
    Location
    Riddells Creek, Vic.
    Posts
    837

    Default

    [QUOTE=racingtadpole;1983963]They use a triangular carbide insert.
    If you’re doing a lot of heavy structural section that requires bevelling to weld, they are the ducks..

    This is a very small unit with a maximum chamfer of about 1mm so not really suitable for pre - weld preparation. The 45 degree angle is also not ideal.

  12. #12
    Join Date
    Apr 2012
    Location
    Healesville
    Posts
    2,129

    Default

    Quote Originally Posted by jack620 View Post
    Looks like I do need one after all.
    You could wrap it nicely and give it to the missus for mothers day, i'm sure she will let you use it

  13. #13
    Join Date
    Mar 2011
    Location
    Southern Flinders Ranges
    Posts
    1,552

    Default

    This is a very small unit with a maximum chamfer of about 1mm so not really suitable for pre - weld preparation. The 45 degree angle is also not ideal.
    The one I bought would do 3.5ish mm if you did it in several passes, worked really well for 5-10mm material before I dropped it and fractured the body of it.

Similar Threads

  1. NSW. Pneumatic curiosity
    By Metalman in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 2
    Last Post: 17th Jul 2020, 12:00 AM
  2. What is your favourite lathe chamfering/deburring tool?
    By OxxAndBert in forum METALWORK GENERAL
    Replies: 6
    Last Post: 9th May 2020, 12:52 AM
  3. pneumatic cylinders uses
    By joez in forum METALWORK GENERAL
    Replies: 9
    Last Post: 15th Feb 2018, 03:42 PM
  4. Deburring and chamfering machine
    By jhovel in forum METALWORK PROJECTS
    Replies: 11
    Last Post: 30th Apr 2016, 10:41 PM
  5. QUEENSLAND SMC CNC Pneumatic Ram (New)
    By SurfinNev in forum METALWORK - Machinery, Equipment, MARKET