    I bought A Short length of 4140 which I think is what they call " pre-hard" the seller says it's hardness is RK 32 or therabouts, the surface finish is very smooth and shiny .

    There are various terms used to describe the state of 4140 - annealed or tempered and cold rolled and hardened

    So if the the shiny smooth finish is achieved by cold rolling . Do they roll it after it has been tempered and quenched or before the tempering has been done ?

    The cold rolling process does surface harden it to some degree I think .

  2. #2
    Join Date
    Jan 2012
    Location
    Melbourne
    Posts
    149

    Default

    You may have material that is hardened then "peeled and polished" and sold under that description. I have bought it from Bohler, don't know what their finishing process is.

  3. #3
    Join Date
    Nov 2008
    Location
    North Brisbane. Qld. Australia
    Age
    70
    Posts
    1,514

    Default

    Probably peeled and polished as stated. I have some here in 65mm for a special project. Bought from Bohler as well.
    Nev.

  4. #4
    Join Date
    Jul 2008
    Location
    near Warragul, Victoria
    Posts
    3,726

    Default Thanks

    Quote Originally Posted by SurfinNev View Post
    Probably peeled and polished as stated. I have some here in 65mm for a special project. Bought from Bohler as well.
    OK. I found this info useful as a general guide http://www.atlassteels.com.au/docume...Oct%202011.pdf

  5. #5
    Join Date
    Mar 2014
    Location
    South of Adelaide
    Posts
    1,229

    Default

    Pretty much all 4140 barstock sold here in Aus is pre hardened. i have only encountered annealed 4140 in a forging i had to proof machine, and it was gummy and horrible to machine. The smooth finish is from the burnishing effect when they cold roll the bar.

Similar Threads

  1. single to 3 phase vsd confusion.
    By lather in forum METALWORK GENERAL
    Replies: 117
    Last Post: 9th May 2020, 07:38 PM
  2. Tumble Reverse Confusion
    By pench in forum METALWORK GENERAL
    Replies: 3
    Last Post: 12th Feb 2014, 09:08 PM
  3. MIG wire confusion
    By twebb01 in forum WELDING
    Replies: 19
    Last Post: 9th Jun 2012, 12:46 PM
  4. Helical gear confusion
    By Ueee in forum METALWORK GENERAL
    Replies: 4
    Last Post: 10th Apr 2012, 01:10 PM
  5. CONFUSION - Doorstops missing
    By DanP in forum FORUMS INFO, HELP, DISCUSSION & FEEDBACK
    Replies: 17
    Last Post: 12th Dec 2003, 12:34 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •