Needs Pictures: 0
Picture(s) thanks: 0
Results 1 to 5 of 5
Thread: 4140 confusion
-
23rd Apr 2021, 07:10 PM #1
4140 confusion
I bought A Short length of 4140 which I think is what they call " pre-hard" the seller says it's hardness is RK 32 or therabouts, the surface finish is very smooth and shiny .
There are various terms used to describe the state of 4140 - annealed or tempered and cold rolled and hardened
So if the the shiny smooth finish is achieved by cold rolling . Do they roll it after it has been tempered and quenched or before the tempering has been done ?
The cold rolling process does surface harden it to some degree I think .
-
23rd Apr 2021, 07:45 PM #2Senior Member
- Join Date
- Jan 2012
- Location
- Melbourne
- Posts
- 149
You may have material that is hardened then "peeled and polished" and sold under that description. I have bought it from Bohler, don't know what their finishing process is.
-
23rd Apr 2021, 08:17 PM #3Most Valued Member
- Join Date
- Nov 2008
- Location
- North Brisbane. Qld. Australia
- Age
- 70
- Posts
- 1,514
Probably peeled and polished as stated. I have some here in 65mm for a special project. Bought from Bohler as well.
Nev.
-
23rd Apr 2021, 09:52 PM #4
Thanks
OK. I found this info useful as a general guide http://www.atlassteels.com.au/docume...Oct%202011.pdf
-
23rd Apr 2021, 09:55 PM #5Diamond Member
- Join Date
- Mar 2014
- Location
- South of Adelaide
- Posts
- 1,229
Pretty much all 4140 barstock sold here in Aus is pre hardened. i have only encountered annealed 4140 in a forging i had to proof machine, and it was gummy and horrible to machine. The smooth finish is from the burnishing effect when they cold roll the bar.
Similar Threads
-
single to 3 phase vsd confusion.
By lather in forum METALWORK GENERALReplies: 117Last Post: 9th May 2020, 07:38 PM -
Tumble Reverse Confusion
By pench in forum METALWORK GENERALReplies: 3Last Post: 12th Feb 2014, 09:08 PM -
MIG wire confusion
By twebb01 in forum WELDINGReplies: 19Last Post: 9th Jun 2012, 12:46 PM -
Helical gear confusion
By Ueee in forum METALWORK GENERALReplies: 4Last Post: 10th Apr 2012, 01:10 PM -
CONFUSION - Doorstops missing
By DanP in forum FORUMS INFO, HELP, DISCUSSION & FEEDBACKReplies: 17Last Post: 12th Dec 2003, 12:34 PM