    I am working on a 48 Indian and they have exposed kick start gears. It got me thinking. Is there a practical way to stop the gear corroding, give it a nice black colour and help with reduced friction.

    Something like metal blacking comes to mind if the right finishing oil was used. I am keen to do this at home. Even if I decide not to go this way on this gear I would be interested in options. I am always keen to learn. Please share your anti friction recipes and experiences.

    Thanks Steve

  2. #2
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Quote Originally Posted by Reidy41 View Post
    Hello all

    I am working on a 48 Indian and they have exposed kick start gears. It got me thinking. Is there a practical way to stop the gear corroding, give it a nice black colour and help with reduced friction.

    Something like metal blacking comes to mind if the right finishing oil was used. I am keen to do this at home. Even if I decide not to go this way on this gear I would be interested in options. I am always keen to learn. Please share your anti friction recipes and experiences.
    Even the very best commercial metal blackening/bluing will not resist metal on metal contact and it will eventually rub away. About the best you can do is keep a thin layer of oil on it.

    Heres my DIY metal bluing thread that might give you some ideas.
    https://metalworkforums.com/f65/t197115-metal-bluing?

  3. #3
    Join Date
    Aug 2010
    Location
    Near Bendigo, Victoria, AUS
    Age
    72
    Posts
    3,105

    Default

    Quote Originally Posted by Reidy41 View Post
    Hello all

    I am working on a 48 Indian and they have exposed kick start gears. It got me thinking. Is there a practical way to stop the gear corroding, give it a nice black colour and help with reduced friction.

    Something like metal blacking comes to mind if the right finishing oil was used. I am keen to do this at home. Even if I decide not to go this way on this gear I would be interested in options. I am always keen to learn. Please share your anti friction recipes and experiences.

    Thanks Steve
    Hi Steve,
    from memory, the '48 Chief had a silver coloured kick start lever and gear. I would get it nickel plated to prevent rust or corrosion. It won't help much with friction reduction, but drylube will. The kind used on off-road bike chains. That will also prevent corrosion as long as it is there - so regular squirts are in order....
    oh, just noticed your question of doing it at home: Janekit in Sydney sell "electroless nickel" plating kits. I use them quite a bit and they work very well.
    Cheers, Joe
    retired - less energy, more time to contemplate projects and more shed time....

  4. #4
    Join Date
    Aug 2008
    Location
    Melbourne
    Age
    34
    Posts
    1,080

    Default

    Chromium nitride would probably work a treat (excellent corrosion and wear resistance, as well as reducing friction), but it's not the kind of thing you can DIY

Similar Threads

  1. Noise Reduction
    By Satwinder Singh in forum METALWORK GENERAL
    Replies: 25
    Last Post: 17th May 2020, 10:27 PM
  2. GMC 2200W friction cut off saw SWITCH help?
    By Grahame Collins in forum METALWORK GENERAL
    Replies: 8
    Last Post: 6th Sep 2017, 11:35 AM
  3. Speed reduction vs. Stalling a motor vs. Horsepower
    By steamingbill in forum METALWORK GENERAL
    Replies: 8
    Last Post: 26th Feb 2017, 03:27 PM
  4. More on lube and anti corrosion /reclaimation
    By Grahame Collins in forum METALWORK GENERAL
    Replies: 3
    Last Post: 16th Apr 2012, 12:07 AM
  5. VSD Hp reduction
    By Stustoys in forum METALWORK GENERAL
    Replies: 31
    Last Post: 12th Jan 2011, 02:04 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •